Drug releasing coatings for medical devices
The invention relates to a medical device for delivering a therapeutic agent to a tissue. The medical device has a layer overlying the exterior surface of the medical device. The layer contains a therapeutic agent and an additive. The additive has a hydrophilic part and a hydrophobic part and the therapeutic agent is not enclosed in micelles or encapsulated in particles or controlled release carriers.
1. A method for preparing a drug coated balloon catheter, the method comprising:
(a) preparing a solution comprising:
an organic solvent selected from the group consisting of hexane, octane, cyclohexane, heptane, benzene, toluene, xylene, methanol, ethanol, propanol, isopropanol, diethylamide, ethylene glycol monoethyl ether, Trascutol, benzyl alcohol, dioxane, dimethyl ether, tetrahydrofuran, ethyl acetate, isobutyl acetate, acetone, acetonitrile, diethyl ketone, methyl ethyl ketone, dimethylformamide, dimethylsulfoxide, mixtures of water and ethanol, mixtures of water and acetone, mixtures of water and methanol, mixtures of water and tetrahydrofuran, and combinations thereof;
a therapeutic agent selected from the group consisting of paclitaxel, rapamycin, and mixtures thereof;
at least one first additive selected from the group consisting of PEG sorbitan monolaurates, PEG sorbitan monooleates, and mixtures thereof; and
at least one additional additive selected from the group consisting of sorbitol, sorbitan, gluconolactone, and mixtures thereof;
(b) forming a coating layer containing the therapeutic agent and the at least one additive on an exterior surface of a balloon of a balloon catheter to form the drug coated balloon catheter by:
(i) applying the solution to the balloon in an inflated or partially inflated state; and
(ii) drying the balloon to evaporate the organic solvent from the coating solution after the solution is applied; and
(c) deflating and folding the balloon,
wherein the ratio by weight of the additives to the therapeutic agent in the coating layer is from 0.05 to 100.
2. The method according to claim 1 , wherein the thickness of the coating layer is from about 0.1 μm to 200 μm.
3. The method according to claim 1 , wherein the ratio by weight of the additives to the therapeutic agent in the coating layer is from 0.1 to 5.
4. The method according to claim 1 , wherein the ratio by weight of the additives to the therapeutic agent in the coating layer is from 0.8 to 1.2.
5. The method according to claim 1 , wherein the at least one additional additive is selected from the group consisting of sorbitol, sorbitan, and mixtures thereof.
6. The method according to claim 1 , wherein the at least one first additive is selected from the group consisting of PEG-20 sorbitan monolaurate and PEG-20 sorbitan monooleate.
7. The method according to claim 1 , wherein:
the at least one first additive is selected from the group consisting of PEG-20 sorbitan monolaurate and PEG-20 sorbitan monooleate; and
the at least one additional additive is selected from the group consisting of sorbitol, gluconolactone, and mixtures thereof.
8. The method according to claim 7 , wherein the solution consists essentially of the organic solvent, the therapeutic agent, the at least one first additive, and the at least one additional additive.
9. The method according to claim 7 , wherein the solution consists essentially of:
the organic solvent;
from 1% to 15% total by weight, based on the total weight of the solution, of the at least one first additive and the at least one additional additive; and
from 2% to 20% total by weight, based on the total weight of the solution, of the therapeutic agent, the at least first one additive, and the at least one additional additive.
10. The method according to claim 9 , wherein the organic solvent is selected from the group consisting of ethanol; mixtures of water and ethanol; acetone; mixtures of water and acetone; mixtures of acetone and ethanol; and mixtures of water, acetone, and ethanol.
11. The method according to claim 1 , wherein (b)(i) and (b)(ii) are repeated until a therapeutically effective amount of the therapeutic agent in the coating layer is deposited on the exterior surface of the balloon.
12. The method according to claim 1 , wherein (b)(i) and (b)(ii) are repeated until the exterior surface of the balloon has thereon a concentration density of therapeutic agent of from 1 μg/mm 2 to 20 μg/mm 2 .
13. The method according to claim 1 , wherein the solution comprises:
from 0.5% to 50% by weight, based on the total weight of the solution, of the therapeutic agent; and
from 1% to 45% by weight, based on the total weight of the solution, of the additives.
14. The method according to claim 1 , wherein the solution comprises a total of from 2% to 20% by weight, based on the total weight of the solution, of the therapeutic agent and additives in the organic solvent.
15. The method according to claim 1 , wherein the organic solvent is selected from the group consisting of methanol, ethanol, propanol, isopropanol, acetone, dioxane, tetrahydrofuran, dimethylformamide, acetonitrile, dimethylsulfoxide, and combinations thereof.
16. The method according to claim 1 , wherein the organic solvent is selected from the group consisting of ethanol; mixtures of water and ethanol; acetone; mixtures of water and acetone; mixtures of acetone and ethanol; and mixtures of water, acetone, and ethanol.