IP Library Granted Patent US 8,183,301
Granted Patent B2
US 8,183,301 · App. 13/121,111 · Granted May 22, 2012

Preparation methods for liquid hydrocarbons by Fischer-Tropsch synthesis through slurry reaction

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,183,301
App. No.
13/121,111
Granted
May 22, 2012
Kind
B2
Abstract

The present invention relates to a method for preparing liquid hydrocarbons via a slurry phase Fischer-Tropsch (F-T) synthesis. In particular, the present invention relates to a method for preparing liquid hydrocarbons from syngas via slurry phase F-T synthesis using a catalyst, which can prevent the decrease in catalyst activity and filter clogging due to catalyst aggregation, simultaneously with improving selectivity for C 5 or higher hydrocarbons by using C 7 -C 12 alcohols having a high boiling point as an additive for a slurry reaction solvent or recycling the same alcohol separated from by-products that are generated during the F-T reaction. Since the method of the present invention is more carbon-effective and shows improved long-term stability of a reactor, it can be effectively used in the preparation of liquid hydrocarbons.

Claims (5)

1. A method for preparing liquid hydrocarbons from syngas via slurry phase Fischer-Tropsch synthesis using a catalyst, wherein said slurry phase Fischer-Tropsch synthesis is carried out in the presence of a C 7 -C 12 alcohol having a high boiling point.

2. The method according to claim 1 , wherein the alcohol having a high boiling point is separated from a by-product generated during the slurry phase Fischer-Tropsch synthesis reaction and then recycled.

3. The method according to claim 1 , wherein the alcohol having a high boiling point has a boiling point of 150° C. or higher under atmospheric pressure at a concentration of 5,000 to 50,000 ppm.

4. The method according to claim 1 , wherein the catalyst is a cobalt-based catalyst having a specific surface area of 50 to 500 m 2 /g in which the content of cobalt is in the range of from 5 to 40 wt %.

5. The method according to claim 2 , wherein the alcohol having a high boiling point has a boiling point of 150° C. or higher under atmospheric pressure at a concentration of 5,000 to 50,000 ppm.

Assignments (2)
CHANGE OF ADDRESS Recorded Apr 22, 2015
From: KOREA NATIONAL OIL CORPORATION
To: KOREA NATIONAL OIL CORPORATION
Reel/Frame 035476/0964 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 25, 2011
From: OH, JONG HYEOK; BAE, JONG WOOK; PARK, SUN JU; LEE, YUN JO; JUN, KI WON
To: KOREA RESEARCH INSTITUTE OF CHEMICAL TECHNOLOGY; DAELIM INDUSTRIAL CO., LTD.; KOREA GAS CORPORATION; KOREA NATIONAL OIL CORPORATION; HYUNDAI ENGINEERING CO., LTD.; SK INNOVATION CO., LTD.
Reel/Frame 026024/0838 →