IP Library Granted Patent US 8,420,564
Granted Patent B2
US 8,420,564 · App. 13/236,326 · Granted Apr 16, 2013

Sulfur-tolerant catalyst prepared through high pressure decomposition

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,420,564
App. No.
13/236,326
Granted
Apr 16, 2013
Kind
B2
Abstract

A method of producing a MoS 2 catalyst. The method begins by the decomposition of ammonium tetrathiomolybdate in an organic solvent. This decomposition is done in the presence of a solution comprising: a solvent and a promoter, and done under gaseous pressure.

Claims (17)

1. A method comprising:

decomposition of ammonium tetrathiomolybdate in an organic solvent in the presence of a solution comprising:

a solvent; and

a promoter comprising zirconium and elemental sulfur,

wherein the decomposition produces a MoS 2 catalyst and the decomposition occurs under gaseous pressure.

2. The method of claim 1 , wherein the solvent is H 2 O.

3. The method of claim 1 , wherein the temperature of the decomposition is from 275° C. to 475° C.

4. The method of claim 1 , wherein the gaseous pressure of the decomposition is greater than 2000 psig.

5. The method of claim 1 , wherein the gaseous pressure of the decomposition is from 2000 psig to 3000 psig.

6. The method of claim 1 , wherein the decomposition occurs under the gaseous pressure of H 2 .

7. The method of claim 1 , wherein the MoS 2 catalyst has a total CO conversion in synthesis gas methanation greater than 75%.

8. A method comprising:

decomposition of ammonium tetrathiomolybdate in an organic solvent in the presence of a solution comprising:

a solvent of water; and

a promoter comprising zirconium and elemental sulfur,

wherein the temperature of the decomposition is from 275° C. to 475° C. and the pressure the decomposition occurs under a H 2 gaseous pressure from 2000 psig to 3000 psig,

to produce a MoS 2 catalyst having a total CO conversion in synthesis gas methanation greater than 75%.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 15, 2012
From: CONOCOPHILLIPS COMPANY
To: PHILLIPS 66 COMPANY
Reel/Frame 028213/0824 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 19, 2011
From: ANAND, MADHU; ALLISON, JOE D.
To: CONOCOPHILLIPS COMPANY
Reel/Frame 026929/0336 →