IP Library Granted Patent US 8,765,842
Granted Patent B2
US 8,765,842 · App. 13/256,820 · Granted Jul 1, 2014

Method for producing polymeric solids

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,765,842
App. No.
13/256,820
Granted
Jul 1, 2014
Kind
B2
Abstract

The invention relates to a method for producing polymeric solids free of auxiliary emulators starting from polymer latices (dispersion), wherein a polymer dispersion with a starting ph-value greater than 9 is set to a ph-value of 6 to 9 by adding gaseous carbon dioxide and the polymer dispersion is subsequently coagulated by shearing and/or freezing.

Claims (9)

1. A method for producing polymeric solids free of auxiliary emulsifiers starting from polymer latices, comprising;

providing a polymer dispersion having a starting pH value greater than 9,

adjusting the starting pH value to an adjusted pH value of from 6 to 9 by addition of gaseous carbon dioxide and where the polymer dispersion is subsequently coagulated by shear and/or freezing out.

2. The method according to claim 1 , wherein the adjusted pH value is between 7 and 8.

3. The method according to claim 2 , wherein the polymer dispersion is an anionically stabilized polychloroprene dispersion in which the proportion of polymerized chloroprene in the solid matter of the dispersion as a whole is greater than 50%.

4. The method according to claim 2 , wherein the polymer dispersion is prepared by means of a continuous polymerization of chloroprene without the addition of auxiliary emulsifiers.

5. The method according to claim 4 , wherein the introduction of gaseous carbon dioxide is carried out continuously.

6. The method according to claim 5 , wherein the introduction of gaseous carbon dioxide is controlled so that a yield of carbon dioxide from the adjusting step is greater than 20%.

7. The method according to claim 6 , wherein the introduction of gaseous carbon dioxide is carried out at local pressures at the point of introduction of <80 bar.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 19, 2016
From: LANXESS DEUTSCHLAND GMBH
To: ARLANXEO DEUTSCHLAND GMBH
Reel/Frame 039753/0760 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 22, 2011
From: ACHTEN, DIRK; KUEKER, PETER; KEMPKES, JURGEN; LORENZ, BIANKA; OBRECHT, WERNER; STOBRAWE, ANNIKA
To: LANXESS DEUTSCHLAND GMBH
Reel/Frame 027435/0540 →