Microporous membranes, methods for making such membranes, and the use of such membranes as battery separator film

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,295,950
App. No.
13/260,658
Granted
Mar 29, 2016
Kind
B2
Abstract

The invention relates to microporous membranes comprising polymer and having well-balanced permeability, shutdown temperature, and pin puncture strength. The invention also relates to methods for making such membranes, and the use of such membranes as battery separator film in, e.g., lithium ion secondary batteries.

Claims (12)

1. A microporous membrane comprising a mixture of polyolefin, the mixture of polyolefin consisting essentially of a first polyethylene, a second polyethylene having a Tm ≧131.0° C. and an Mw of 5.6×10 5 to 7.5×10 5 , a third polyethylene having an Mw >1.0×10 6 , and polypropylene, wherein 1) the first polyethylene is a copolymer of ethylene and a comonomer which is selected from the group consisting of butene-1, pentene-1, hexane-1, 4-methyl-pentene-1, octane-1, vinyl acetate, methyl methacrylate and styrene, 2) the first polyethylene has a Mw of 3.8×10 4 to 2.6×10 5 , a molecular weight distribution of from 1.8 to 3.5 and a Tm of 123.0° C. to 126.0° C., 3) the second polyethylene and the third polyethylene are ethylene homopolymer, 4) an amount of the polypropylene is <5.0 wt. %, based on the weight of the polymer used to produce the microporous membrane and 5) the microporous membrane has a normalized air permeability of 1.0×10 2 seconds/100 cm 3 /20 μm to 3.58×10 2 seconds/100 cm 3 /20 μm.

2. The microporous membrane according to claim 1 , wherein the membrane has a shutdown temperature ≦130.5° C.

3. The microporous membrane according to claim 1 , wherein the first polyethylene is present in an amount of 4.0 wt. % to 20.0 wt. %, based on the total weight of polymer in the polymer-diluent mixture.

4. The microporous membrane according to claim 1 , wherein the second polyethylene is present in an amount of 50.0 wt. % to 95.0 wt. %, based on the total weight of polymer in the polymer-diluent mixture, and the third polyethylene is present in an amount of 1.0 wt. % to 46.0 wt. %, based on the total weight of polymer in the polymer-diluent mixture.

5. A battery separator film comprising the microporous membrane of claim 1 .

6. A battery comprising an electrolyte, an anode, a cathode, and a separator situated between the anode and the cathode, wherein the separator comprises the microporous membrane of claim 1 .

7. A method of producing a microporous membrane, comprising:

(1) extruding a mixture of diluent and polymer, the polymer consisting essentially of a first polyethylene, a second polyethylene having a Tm ≧131.0° C. and an Mw of 5.6×10 5 to 7.5×10 5 , a third polyethylene having an Mw >1.0×10 6 , and polypropylene, wherein 1) the first polyethylene is a copolymer of ethylene and a commoner which is selected from the group consisting of butene-1, pentene-1, hexane-1, 4-methyl-pentene-1, octane-1, vinyl acetate, methyl methacrylate and styrene, 2) the first polyethylene has a Mw of 3.8×10 4 to 2.6×10 5 , a molecular weight distribution of from 1.8 to 3.5 and a Tm of 123.0° C. to 126.0° C., 3) the second polyethylene and the third polyethylene are ethylene homopolymer, and 4) an amount of the polypropylene is <5.0 wt. %, based on the weight of the polymer used to produce the microporous membrane;

(2) stretching the extrudate in at least one planar direction; and

(3) removing at least a portion of the diluent from the stretched extrudate to form the microporous membrane which has a normalized air permeability of 1.0×10 2 seconds/100 cm 3 /20 μm to 3.58×10 2 seconds/100 cm 3 /20 μm and a shutdown temperature ≦130.5° C.

8. The method of claim 7 , wherein the first polyethylene is present in an amount of 4.0 wt. % to 17.0 wt. %, based on the weight of the polymer in the polymer-diluent mixture, the second polyethylene is present in an amount of 50.0 wt. % to 95.0 wt. % , based on the weight of the polymer in the polymer-diluent mixture, and the third polyethylene is present in an amount of 1.0 wt. % to 46.0 wt. %, based on the weight of the polymer in the polymer-diluent mixture.

9. A membrane product of the method of claim 7 .

Assignments (5)
MERGER Recorded Sep 15, 2017
From: TORAY BATTERY SEPARATOR FILM CO., LTD.
To: TORAY INDUSTRIES, INC.
Reel/Frame 043968/0447 →
MERGER Recorded Jul 21, 2017
From: TORAY BATTERY SEPARATOR FILM CO., LTD.
To: TORAY INDUSTRIES, INC.
Reel/Frame 043453/0721 →
CHANGE OF NAME Recorded Sep 6, 2012
From: TORAY BATTERY SEPARATOR FILM GODO KAISHA
To: TORAY BATTERY SEPARATOR FILM CO., LTD.
Reel/Frame 028905/0220 →
CHANGE OF NAME Recorded Aug 29, 2012
From: TORAY TONEN SPECIALTY SEPARATOR GODO KAISHA
To: TORAY BATTERY SEPARATOR FILM GODO KAISHA
Reel/Frame 028867/0647 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 27, 2011
From: ISHIHARA, TAKESHI; MIYAOKA, SATOSHI; KONO, KOICHI; CROWTHER, DONNA J.; BRANT, PATRICK
To: TORAY TONEN SPECIALTY SEPARATOR GODO KAISHA
Reel/Frame 026975/0985 →