System and method including multi-circuit solution extraction for recovery of metal values from metal-bearing materials

Inventors: Jason M Morgan (Morenci, AZ); Barbara J Savage (Silver City, NM); David G Meadows (Phoenix, AZ); Wayne W Hazen (Lakewood, CO)
Assignee: FREEPORT MINERALS CORPORATION
C22B3/0005B01D11/028B01D11/0488
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,169,533
App. No.
13/331,717
Granted
Oct 27, 2015
Kind
B2
Abstract

The present disclosure relates to a metal recovery process comprising a solvent extraction process. In an exemplary embodiment, the solution extraction system comprises a plant with a first and second circuit. A high-grade pregnant leach solution (“HGPLS”) is provided to the first and second circuit, and a low-grade pregnant leach solution (“LGPLS”) is provided to the second circuit. The first circuit produces a rich electrolyte, which can be forwarded to a primary metal recovery, and a low-grade raffinate, which can be forwarded to a secondary metal recovery process. The second circuit produces a rich electrolyte, which can also be forwarded to the primary metal recovery process. The first and second circuits are in fluid communication with each other.

Claims (20)

1. A method of extracting a metal value comprising:

providing a first portion of a first metal-bearing solution to a first circuit of a solution extraction plant comprising a first barren organic stream;

providing a second portion of the first metal-bearing solution to a second circuit of the solution extraction plant comprising a second barren organic stream, wherein the first circuit of the solution extraction plant and the second circuit of the solution extraction plant are in fluid communication;

providing a second metal-bearing solution to the second circuit of the solution extraction plant;

extracting a first circuit raffinate, wherein the first circuit raffinate is a low-grade raffinate produced by contacting the second metal-bearing solution with the first barren organic stream and the second barren organic stream;

extracting a first circuit electrolyte; and

extracting a second circuit electrolyte.

2. The method of claim 1 , wherein the first metal-bearing solution is a high-grade pregnant leach solution.

3. The method of claim 1 , wherein the second metal-bearing solution is a low-grade pregnant leach solution.

4. The method of claim 1 , wherein the first circuit electrolyte is a rich electrolyte.

5. The method of claim 1 , wherein the second circuit electrolyte is a rich electrolyte.

6. The method of claim 1 , wherein the first metal-bearing solution and second metal-bearing solution comprise copper.

7. The method of claim 1 , wherein the low-grade raffinate comprises a secondary metal value.

8. The method of claim 1 further comprising extracting a second second circuit raffinate, and supplying the second second circuit raffinate to the first circuit of the solution extraction plant.

9. A method for extracting metal value comprising:

preparing a metal-bearing material;

performing a reactive process on the metal-bearing material to produce a metal-bearing solution;

performing a solution extraction process comprising providing a portion of a first metal-bearing solution comprising a high grade pregnant leach solution to a first circuit of a solution extraction plant comprising a first barren organic solution, providing a portion of the first metal-bearing solution to a second circuit of the solution extraction plant comprising a second barren organic solution, wherein the first circuit of the solution extraction plant and the second circuit of the solution extraction plant are in fluid communication with each other, providing a second metal-bearing solution to the second circuit of the solution extraction plant, extracting a first circuit low-grade raffinate by contacting the second metal-bearing solution with the first barren organic solution and the second barren organic solution, extracting a first circuit electrolyte, and extracting a second circuit electrolyte;

performing a primary metal recovery process on the first circuit electrolyte and second circuit electrolyte; and

performing a secondary metal recovery process on the first circuit raffinate.

Assignments (3)
CHANGE OF NAME Recorded Jul 23, 2014
From: FREEPORT-MCMORAN CORPORATION
To: FREEPORT MINERALS CORPORATION
Reel/Frame 033389/0300 →
MERGER Recorded Jul 17, 2014
From: FREEPORT-MCMORAN CORPORATION
To: FREEPORT-MCMORAN CORPORATION
Reel/Frame 033357/0849 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 8, 2012
From: MORGAN, JASON M; SAVAGE, BARBARA J; MEADOWS, DAVID G; HAZEN, WAYNE W
To: FREEPORT-MCMORAN CORPORATION
Reel/Frame 027826/0429 →
Continuity (1)
Related Publication 20130152741A1 · Jun 20, 2013