IP Library Granted Patent US 9,932,446
Granted Patent B2
US 9,932,446 · App. 13/395,390 · Granted Apr 3, 2018

Method of manufacturing a purified product of alkyl-modified polydimethylsiloxane, a cosmetic raw material, and cosmetics

Inventors: Yasuo Nomura (Yokohama, JP); Keisuke Nishino (Hakusan, JP); Yasue Kanzaki (Chiba, JP)
Assignee: DOW CORNING TORAY CO., LTD.
C08G77/34A61K8/064A61K8/585A61K8/891A61Q17/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,932,446
App. No.
13/395,390
Granted
Apr 3, 2018
Kind
B2
Abstract

To provide a method for manufacturing a purified product of an alkyl-modified polydimethylsiloxane that is practically odorless and compatible with other cosmetic raw materials. The manufacturing method comprises the steps of: [A] synthesizing an alkyl-modified polydimethylsiloxane by subjecting a hydrosilyl-containing polydimethylsiloxane and an C2-C30 α-olefin to a hydrosilation reaction, and [B] subjecting the crude alkyl-modified polydimethylsiloxane obtained in Step [A] to a treatment of rendering it odorless by a hydrogenation reaction in the presence of a hydrogenation catalyst in an organic solvent (c) that is essentially free of active hydrogen atoms and has a boiling point equal to or greater than 70° C.

Claims (30)

1. A method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane having the following general formula (1):

where R 1 is an alkyl group of formula —C 2 H 4 —C p H 2p+1 that contains 2 to 30 carbon atoms, where “p” is a number ranging from 0 to 28, R 2 is a methyl group or a group defined earlier for R 1 ; “m” is a number ranging from 0 to 300; and “n” is a number ranging from 0 to 50; however, when “n” is 0, at least one R 2 is a group indicated by R 1 , the method comprising the steps of:

[A] synthesizing an alkyl-modified polydimethylsiloxane of general formula (1) by subjecting

a hydrosilyl-containing polydimethylsiloxane (a) having the following formula (2):

where R 3 is a methyl group or a hydrogen atom; and “m” and “n” are each individually numbers in the same ranges as defined above; however, when “n” is 0, at least one R 3 is a hydrogen atom, and

an α-olefin of general formula CH 2 ═CH—C p H 2p+1 (b) that contains 2 to 30 carbon atoms where “p” is a number ranging from 0 to 28, to a hydrosilation reaction, and

[B] subjecting the crude alkyl-modified polydimethylsiloxane obtained in Step [A] to a treatment of rendering it odorless by a hydrogenation reaction that is carried out at a temperature of 25° C. in the presence of a hydrogenation catalyst in methylcyclohexane and/or ethylcyclohexane, wherein the methylcyclohexane and/or ethylcyclohexane have a boiling point equal to or greater than 70° C. under a pressure of 1 atmosphere.

2. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 1 , wherein the hydrogenation catalyst used in Step [B] is a Raney nickel.

3. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 1 , wherein step [A] comprises a step [A1] of synthesizing an alkyl-modified polydimethylsiloxane of formula (3) given below:

where R 1 is the same as defined earlier,

by subjecting 1,1,1,3,5,5,5-heptamethyltrisiloxane (a1) and an α-olefin of general formula CH 2 ═CH—C p H 2p+1 that contains 2 to 30 carbon atoms where “p” is a number ranging from 0 to 28, to a hydrosilation reaction, and wherein step [B] comprises a step [B1] of subjecting the crude alkyl-modified polydimethylsiloxane obtained in Step [A1] in the presence of a hydrogenation catalyst to a treatment of rendering it odorless by a hydrogenation reaction in methylcyclohexane or ethylcyclohexane.

4. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 1 , comprising a step of stripping of light fractions by distillation from the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof, prior to or after Step [B], wherein the stripping is carried out by bringing the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof into contact with gaseous nitrogen under a reduced pressure.

5. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 2 , wherein step [A] comprises a step [A1] of synthesizing an alkyl-modified polydimethylsiloxane of formula (3) given below:

where R 1 is the same as defined earlier,

by subjecting 1,1,1,3,5,5,5-heptamethyltrisiloxane (a1) and an α-olefin of general formula CH 2 ═CH—C p H 2p+1 that contains 2 to 30 carbon atoms where “p” is a number ranging from 0 to 28, to a hydrosilation reaction, and wherein step [B] comprises a step [B1] of subjecting the crude alkyl-modified polydimethylsiloxane obtained in Step [A1] in the presence of a hydrogenation catalyst to a treatment of rendering it odorless by a hydrogenation reaction in methylcyclohexane and/or ethylcyclohexane.

6. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 2 , comprising a step of stripping of light fractions by distillation from the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof, prior to or after Step [B], wherein the stripping is carried out by bringing the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof into contact with gaseous nitrogen under a reduced pressure.

7. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 3 , comprising a step of stripping of light fractions by distillation from the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof, prior to or after Step [B], wherein the stripping is carried out by bringing the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof into contact with gaseous nitrogen under a reduced pressure.

8. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 5 , comprising a step of stripping of light fractions by distillation from the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof, prior to or after Step [B], wherein the stripping is carried out by bringing the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof into contact with gaseous nitrogen under a reduced pressure.

9. A method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane having the following general formula (1):

where R 1 is an alkyl group of formula —C 2 H 4 —C p H 2p+1 that contains 2 to 30 carbon atoms, where “p” is a number ranging from 0 to 28, R 2 is a methyl group or a group defined earlier for R 1 ; “m” is a number ranging from 0 to 300; and “n” is a number ranging from 0 to 50; however, when “n” is 0, at least one R 2 is a group indicated by R 1 , the method comprising the steps of:

[A] synthesizing an alkyl-modified polydimethylsiloxane of general formula (1) by subjecting:

a hydrosilyl-containing polydimethylsiloxane (a) having the following formula (2):

where R 3 is a methyl group or a hydrogen atom; and “m” and “n” are each individually numbers in the same ranges as defined above; however, when “n” is 0, at least one R 3 is a hydrogen atom, and

an α-olefin of general formula CH 2 ═CH—C p H 2p+1 (b) that contains 2 to 30 carbon atoms where “p” is a number ranging from 0 to 28, to a hydrosilation reaction;

[B] subjecting the crude alkyl-modified polydimethylsiloxane obtained in Step [A] to a treatment of rendering it odorless by a hydrogenation reaction that is carried out at a temperature of 25° C. in the presence of a hydrogenation catalyst in methylcyclohexane and/or ethylcyclohexane;

[C] stripping of light fractions by distillation from the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof, prior to or after Step [B], wherein the stripping is carried out by bringing the crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof into contact with gaseous nitrogen under a reduced pressure; and

[D] mixing the stripped crude alkyl-modified polydimethylsiloxane or a product of hydrogenation thereof of step [C] with a lipophilic material which has a degree of solubility of less than 1 wt. % per 100 g of water at room temperature.

10. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 9 , wherein said lipophilic material is selected from the group consisting of UV absorbers, silicones that are in a gum state at room temperature, silicone resins, powdered silicone elastomers, physiologically active ingredients, fragrances, and pigments.

11. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 9 , wherein said lipophilic material is an organic UV absorber.

12. The method of manufacturing a purified product of an alkyl-modified polydimethylsiloxane according to claim 11 , wherein said lipophilic material comprises ethylhexyl methoxycinnamate.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 17, 2019
From: DOW CORNING TORAY CO., LTD.
To: DOW TORAY CO., LTD.
Reel/Frame 051322/0925 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 30, 2012
From: NOMURA, YASUO; NISHINO, KEISUKE; KANZAKI, YASUE
To: DOW CORNING TORAY CO., LTD.
Reel/Frame 028126/0767 →
Priority Claims (1)
JP 2009-208768 · Sep 10, 2009 · national
Continuity (1)
Related Publication 20120202893A1 · Aug 9, 2012