IP Library Granted Patent US 8,920,697
Granted Patent B2
US 8,920,697 · App. 13/419,669 · Granted Dec 30, 2014

Method for building three-dimensional objects in extrusion-based additive manufacturing systems using core-shell consumable filaments

Inventors: James K. Mikulak (Austin, TX); Carl R. Deckard (Austin, TX); Robert L. Zinniel (Plymouth, MN)
Assignee: Stratasys, Inc.
B29C67/0055B29C47/025B29C47/04D01F8/04B29C47/0019B29C47/0064B29C47/065B32B3/26D01F8/12B29C47/92B29C2947/92704
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,920,697
App. No.
13/419,669
Granted
Dec 30, 2014
Kind
B2
Abstract

A consumable filament for use in an extrusion-based additive manufacturing system, where the consumable filament comprises a core portion of a first thermoplastic material, and a shell portion of a second thermoplastic material that is compositionally different from the first thermoplastic material, where the consumable filament is configured to be melted and extruded to form roads of a plurality of solidified layers of a three-dimensional object, and where the roads at least partially retain cross-sectional profiles corresponding to the core portion and the shell portion of the consumable filament.

Claims (34)

1. A method for building a three-dimensional object with an additive manufacturing system having an extrusion head, the method comprising:

feeding a consumable filament to the extrusion head, the consumable filament comprising a longitudinal length, a core portion extending along the longitudinal length, and a shell portion extending along the longitudinal length and substantially encasing the core portion, wherein the core portion compositionally comprises a first thermoplastic material, and wherein the shell portion compositionally comprises a second thermoplastic material that is different from the first thermoplastic material;

melting the fed consumable filament in the extrusion head to form molten material;

depositing the molten material as an extruded road that defines at least a portion of a layer of the three-dimensional object, wherein the extruded road comprises a core region of the first thermoplastic material, and a shell region of the second thermoplastic polymeric material; and

solidifying the extruded road.

2. The method of claim 1 , wherein the first thermoplastic material is a first semi-crystalline polymeric material having a first peak crystallization temperature, and wherein the second thermoplastic material is a second semi-crystalline polymeric material having a second peak crystallization temperature that is greater than the first peak crystallization temperature.

3. The method of claim 2 , wherein the additive manufacturing system includes a heated build chamber, and wherein the method further comprises maintaining an environment within the heated build chamber at one or more temperatures that are about equal to, or are within a range of about 10° C. above or below, the peak crystallization temperature of the second semi-crystalline polymeric material.

4. The method of claim 1 , wherein the consumable filament is a support material consumable filament and the three-dimensional object is a support structure for a three-dimensional model, and wherein the method further comprises:

building a layer of the three-dimensional model with the additive manufacturing system, wherein the layer of the three-dimensional model is supported by the solidified layer of the support structure; and

removing the support structure from the three-dimensional model.

5. The method of claim 4 , wherein the second thermoplastic material is at least partially soluble in an aqueous solution, and wherein removing the support structure from the three-dimensional model comprises at least partially dissolving the second thermoplastic material in the aqueous solution.

6. The method of claim 4 , wherein the second thermoplastic material of the shell portion comprises a colorant, and wherein the shell of the extruded road also includes the colorant.

7. The method of claim 1 , wherein the consumable filament comprises a cylindrical geometry along the longitudinal length.

8. The method of claim 1 , wherein the consumable filament has an average cross-sectional area ranging from about 0.5 square millimeters to about 8 square millimeters.

9. A method for building a three-dimensional model and associated support structure with an additive manufacturing system retaining an extrusion head, the method comprising:

feeding a consumable filament to the extrusion head, the consumable filament comprising:

a longitudinal length;

a core portion extending along the longitudinal length, wherein the core portion compositionally comprises a first thermoplastic material; and

a shell portion extending along the longitudinal length and substantially encasing the core portion, wherein the shell portion compositionally comprises a second thermoplastic material that is different from the first thermoplastic material, and wherein the second thermoplastic material is soluble in an aqueous liquid;

melting the fed consumable filament in the extrusion head to form a molten material;

depositing the molten material in the heated build chamber to form a series of extruded roads for a layer of the support structure, wherein at least a portion of the extruded roads each comprise a core region of the first thermoplastic material and a shell region of the second thermoplastic material;

at least partially solidifying the layer; and

building a layer of the three-dimensional model from a modeling material with the additive manufacturing system, wherein the layer of the three-dimensional model is supported by the at least partially solidified layer of the support structure.

10. The method of claim 9 , wherein the first thermoplastic material of the core portion has a creep relaxation temperature that is within about 20° C. of a creep relaxation temperature of the modeling material.

11. The method of claim 10 , wherein the creep relaxation temperature of the first thermoplastic material is within about 10° C. of the creep relaxation temperature of the modeling material.

12. The method of claim 11 , wherein the creep relaxation temperature of the first thermoplastic material is within about 5° C. of the creep relaxation temperature of the modeling material.

13. The method of claim 9 , wherein the aqueous liquid that the second thermoplastic material is soluble in comprises an alkaline aqueous solution.

14. The method of claim 9 , wherein the first thermoplastic material of the core portion has a tensile strength that is higher than a tensile strength of the second thermoplastic material of the shell portion.

15. The method of claim 9 , wherein the first thermoplastic material of the core portion is substantially the same as the modeling material.

16. The method of claim 9 , wherein the additive manufacturing system includes a heated build chamber, and wherein the method further comprises maintaining an environment within the heated build chamber at one or more temperatures that are between about a solidification temperature of the modeling material and a creep relaxation temperature of the modeling material.

17. The method of claim 9 , wherein the core portion of the consumable filament has an average cross-sectional area that is greater than an average cross-sectional area of the shell portion.

18. The method of claim 9 , wherein the consumable filament comprises a cylindrical geometry along the longitudinal length.

19. The method of claim 9 , wherein the first thermoplastic material of the core portion is not soluble in the aqueous liquid.

20. The method of claim 9 , and further comprising exposing the support structure to the aqueous liquid to remove the support structure from the three-dimensional model.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 30, 2012
From: MIKULAK, JAMES K.; DECKARD, CARL R.; ZINNIEL, ROBERT L.
To: STRATASYS, INC.
Reel/Frame 028286/0379 →
Continuity (3)
Continuation In Part 13233280 · Sep 15, 2011
Provisional Application 61383844 · Sep 17, 2010
Related Publication 20120231225A1 · Sep 13, 2012