Method of producing calcite capable of controlling a grain size thereof

Inventors: Young Nam Jang (Daejeon, KR); Kyoung Won Ryu (Daejeon, KR); Myung Gyu Lee (Daejeon, KR); Seung Woo Lee (Daejeon, KR); Kyung Sun Song (Daejeon, KR); Jun Hwan Bang (Daejeon, KR); Soo Chun Chae (Seoul, KR)
Assignee: Korea Institute of Geoscience and Mineral Resources
C01F11/181C01P2004/41C01P2004/39C01P2004/40C01P2004/38C01P2002/72C01P2002/77C01P2002/88C01P2004/03C01P2004/30C01P2004/61C01P2004/62
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,056,781
App. No.
13/450,058
Granted
Jun 16, 2015
Kind
B2
Abstract

Provided is a method of synthesizing high-purity calcite capable of controlling a grain size thereof, by reacting an aqueous calcium chloride solution with CO 2 gas under strong alkaline condition, to crystallize into white and ultra-fine grain calcite. The method of synthesizing fine-grain calcite according to the present disclosure can decrease super-saturation by producing calcite under the strong alkaline conditions, thereby suppressing generation and growth of grain, resulting in controlling the grain size. Therefore, the above method is useful in producing high-purity ultra-fine grain calcite and can control the grain size of calcite from several hundreds of nanometers to several tens of nanometers by regulating the concentration of an aqueous caustic soda solution.

Claims (10)

1. A method of producing calcite comprising:

mixing an aqueous calcium chloride solution and an aqueous caustic soda solution to form a mixture; and

simultaneously reacting the mixture while CO 2 gas is flown thereinto, under room temperature and room pressure, to crystallize into high-purity single-phase calcite,

wherein the molar ratio of the caustic soda of the aqueous caustic soda solution to the calcium chloride of the aqueous calcium chloride solution is from (2/3):1 to (150/41):1 to produce calcite, and a grain size of the calcite is controlled to less than 200 nm by using an aqueous caustic soda solution of 5N or more.

2. The method of claim 1 , further comprising:

a) preparing source materials by preparing an aqueous caustic soda solution and an aqueous calcium chloride solution;

b) performing crystallization by slowly adding the aqueous calcium chloride solution to the aqueous caustic soda solution under room temperature and room pressure and at the same time blowing CO 2 gas thereinto, to crystallize into calcite; and

c) obtaining high-purity single-phase calcite by separating solid and liquid from each other in a slurry crystallized in Step b), and drying the solid.

3. The method of claim 2 , wherein an input amount of CO 2 gas is 0.3 to 5 L/min.

4. The method of claim 1 , wherein an input amount of CO 2 gas is 0.3 to 5 L/min.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 22, 2024
From: KOREA INSTITUTE OF GEOSCIENCE AND MINERAL RESOURCES
To: UNIHUB INC.
Reel/Frame 066191/0186 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 12, 2015
From: JANG, YOUNG NAM; RYU, KYOUNG WON; LEE, MYUNG GYU; LEE, SEUNG WOO; SONG, KYUNG SUN; BANG, JUN HWAN; CHAE, SOO CHUN
To: KOREA INSTITUTE OF GEOSCIENCE AND MINERAL RESOURCES
Reel/Frame 035613/0644 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 18, 2012
From: JANG, YOUNG NAM; RYU, KYOUNG WON; LEE, MYUNG GYU; LEE, SEUNG-WOO; SONG, KYUNG SUN; BANG, JUN HWAN; CHAE, SOO CHUN
To: KOREA INSTITUTE OF GEOSCIENCE AND MINERAL RESOURCES
Reel/Frame 028067/0788 →
Priority Claims (1)
KR 10-2011-0036630 · Apr 20, 2011 · national
Continuity (1)
Related Publication 20120269714A1 · Oct 25, 2012