IP Library Granted Patent US 9,158,044
Granted Patent B2
US 9,158,044 · App. 13/501,216 · Granted Oct 13, 2015

Optical film and display panel

Inventors: Kentaro Akiyama (Tokyo-to, JP); Seiji Shinohara (Tokyo-to, JP); Emi Shimano (Tokyo-to, JP); Hiroshi Nakamura (Tokyo-to, JP); Mayu Yoki (Tokyo-to, JP)
Assignee: DAI NIPPON PRINTING CO., LTD.
G02B5/0247G02B5/0242G02B5/0278G02F1/133502G02F2201/50
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,158,044
App. No.
13/501,216
Granted
Oct 13, 2015
Kind
B2
Abstract

An optical film having an optically-transparent substrate, and a low refractive index layer having a thickness d on one side of the optically-transparent substrate, a polarizing plate and a display panel provided with the same, and a display provided with the same.

Claims (10)

1. An optical film comprising an optically-transparent substrate, and a low refractive index layer having a thickness d on one side of the optically-transparent substrate,

wherein the low refractive index layer comprises hollow particles having a refractive index from 1.20 to 1.40 and having an average primary particle diameter of 10 to 100 nm, and solid particles having a refractive index from 1.42 to 1.46 and having a dispersion average particle diameter of a value which is in the range from 1 to 20 nm and a half or less of the thickness d,

wherein a ratio of the average primary particle diameter of the hollow particles and the dispersion average particle diameter of the solid particles (average primary particle diameter/dispersion average particle diameter) is 2.0 or more; and

in an area of a cross-sectional surface of the low refractive index layer in a thickness direction with a width of 500 nm in a plane direction of the low refractive index layer, at least one of the hollow particles is covered with a cured resin of the low refractive index layer and allowed to contact with an interface on a side opposite to an optically-transparent substrate side of the low refractive index layer, and

the solid particles occupy 50% or more of the interface excluding a part in which the hollow particles are in contact with and are eccentrically located from the interlace to the depth which is twice the dispersion average particle diameter of the solid particles in the thickness direction, and

a maximum height (Ry) defined by JIS B 0601-1998 of the interface is 0.050 μm or less.

2. The optical film according to claim 1 , wherein a ratio of the eccentrically located solid particles is from 40 to 100% with respect to the total amount of the solid particles present in the area.

3. A polarizer comprising the optical film defined by claim 1 .

4. A display comprising a back-side member and the polarizer defined by claim 3 arranged on a viewer side of the back-side member.

5. A display comprising a back-side member and the optical film defined by claim 1 arranged on a viewer side of the back-side member.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 10, 2012
From: AKIYAMA, KENTARO; SHINOHARA, SEIJI; SHIMANO, EMI; NAKAMURA, HIROSHI; YOKI, MAYU
To: DAI NIPPON PRINTING CO., LTD.
Reel/Frame 028021/0920 →
Priority Claims (1)
JP 2009-239685 · Oct 16, 2009 · national
Continuity (1)
Related Publication 20120200933A1 · Aug 9, 2012