Production method of deodorized polyoxyalkylene-modified polysiloxane composition

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,877,886
App. No.
13/513,741
Granted
Nov 4, 2014
Kind
B2
Abstract

To provide a method of producing a polyoxyalkylene-modified polysiloxane composition that is free of acid-mediated carbon-oxygen bond and silicon-oxygen bond cleavage, that is substantially deodorized and also does not generate odor with elapsed time, and that is therefore well suited for use in cosmetic applications, e.g., for hair cosmetics, skin cosmetics, and so forth. A production method of this invention is characterized by removing the odor-causing substance from a polyoxyalkylene-modified polysiloxane composition that has been synthesized by a hydrosilylation reaction, by subjecting the polyoxyalkylene-modified polysiloxane composition to a hydrolysis treatment in the presence of an acidic inorganic salt that is a solid at 25° C. and gives a specific pH at 25° C. in aqueous solution; for example, potassium hydrogensulfate.

Claims (23)

1. A production method of a polyoxyalkylene-modified polysiloxane composition, the production method comprising:

a step [A] of synthesizing a polyoxyalkylene-modified polysiloxane composition by carrying out a hydrosilylation reaction between

(a) a polyoxyalkylene compound that has a carbon-carbon double bond in molecular chain terminal position, and

(b) an organohydrogenpolysiloxane; and

a step [B] of removing an odor-causing substance by treating the polyoxyalkylene-modified polysiloxane composition in the presence of

(c) at least one acidic inorganic salt that is a solid at 25° C., is soluble in water, and gives a pH at 25° C. of not more than 4 for the aqueous solution prepared by dissolving 50 g of component (c) in 1 liter of ion-exchanged water, wherein component (c) is at least one acidic inorganic salt comprising a hydrogensulfate ion HSO 4 − and a monovalent cation M.

2. The production method according to claim 1 , wherein component (c) is at least one acidic inorganic salt selected from the group consisting of sodium hydrogensulfate, potassium hydrogensulfate, and ammonium hydrogensulfate.

3. The production method according to claim 1 further comprising:

a step [C] of carrying out a deodorization treatment by subjecting the polyoxyalkylene-modified polysiloxane composition to a hydrogenation reaction in the presence of a hydrogenation catalyst.

4. The production method according to claim 3 , wherein step [C] is carried out subsequent to step [B].

5. The production method according to claim 3 , wherein step [B] is carried out subsequent to step [C].

6. The production method according to claim 1 , wherein component (a) in step [A] is a straight-chain polyoxyalkylene compound given by the following structural formula (1)

CH 2 ═CH—C p H 2p O—(C 2 H 4 O) p1 (C 3 H 6 O) p2 R  (1)

wherein p is a number in the range from 1 to 10, p1 and p2 are numbers in the range from 0 to 30, (p1+p2) is a number in the range from 4 to 50, and R is the hydrogen atom or a C 1-10 alkyl group,

and component (b) in step [A] is an organohydrogenpolysiloxane given by the following structural formula (2)

wherein R 2 is a substituted or unsubstituted monovalent hydrocarbyl group, R is the hydrogen atom or a group selected from R 2 , m is a number in the range from 0 to 1000, and n is a number in the range from 0 to 200, wherein when n =0, at least one of R is the hydrogen atom.

7. The production method according to claim 1 further comprising, as a step preceding step [B] or a step following step [B],

a stripping step of distillatively removing a low-boiling component from the polyoxyalkylene-modified polysiloxane composition under reduced pressure while in contact with nitrogen gas.

8. The production method according to claim 1 , wherein component (a) in step [A] is a straight-chain polyoxyalkylene compound given by the following structural formula (1)

CH 2 ═CH—C p H 2p O—(C 2 H 4 O) p1 (C 3 H 6 O) p2 R  (1)

wherein p is a number in the range from 1 to 10, p1 and p2 are numbers in the range from 0 to 30, (p1+p2) is a number in the range from 4 to 50, and R is the hydrogen atom or a C 1-10 alkyl group,

and component (b) in step [A] is an organohydrogenpolysiloxane given by the following structural formula (2)

wherein R 2 is a substituted or unsubstituted monovalent hydrocarbyl group, R is the hydrogen atom or a group selected from R 2 , m is a number in the range from 0 to 1000, and n is a number in the range from 0 to 200, wherein when n =0, at least one of R is the hydrogen atom.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 17, 2019
From: DOW CORNING TORAY CO., LTD.
To: DOW TORAY CO., LTD.
Reel/Frame 051322/0925 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 24, 2012
From: SOUDA, TATSUO; TAMURA, SEIKI
To: DOW CORNING TORAY CO., LTD.
Reel/Frame 028841/0829 →