IP Library Granted Patent US 8,497,005
Granted Patent B1
US 8,497,005 · App. 13/534,058 · Granted Jul 30, 2013

Highly abrasion-resistant grafted polyolefin pipe

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,497,005
App. No.
13/534,058
Granted
Jul 30, 2013
Kind
B1
Abstract

A pipe or tube article comprising an innermost comprising a grafted polyolefin composition made from a grafted polyolefin composition is disclosed which can provide long lifetime, highly abrasion-resistant pipes for mining and other transportation uses. Methods for preparing the article and transporting abrasive materials through the article are also described.

Claims (10)

1. A method comprising producing or obtaining an abrasive particulate stream or abrasive slurry stream; flowing the abrasive particulate stream or abrasive slurry stream into one end of a metal pipe; receiving the abrasive particulate stream or abrasive slurry stream out of the other end of the metal pipe wherein

the metal of the metal pipe is made of steel, aluminum, or copper, or alloys of two or more thereof;

the metal pipe comprises an inner layer, which is a film or sheet;

the inner layer comprises or is produced from a grafted polyolefin;

the film or sheet has a thickness of about 0.001 to about 102 mm and comprises the grafted polyolefin;

the grafted polyolefin is produced by grafting a parent polyolefin with an α,β-ethylenically unsaturated carboxylic acid or anhydride;

the parent polyolefin comprises repeat units derived from ethylene and a C 3-20 α-olefin, has a density of about 0.9 g/cc (ASTM D-792) or less; and

the parent polyolefin has a Shore A hardness of about 96 or less (ASTM D2240, ISO 868).

2. The method of claim 1 wherein the parent polyolefin has a density of about 0.84 to about 0.88.

3. The method of claim 2 wherein the grafted polyolefin has a Shore A hardness of about 80 or less.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 22, 2019
From: E.I. DU PONT DE NEMOURS AND COMPANY
To: PERFORMANCE MATERIALS NA, INC.
Reel/Frame 050237/0001 →