Method of using laser shock impacts to produce raised elements on a wall surface capable of being swept by a fluid in order to control the intensity of turbulence in a transition zone

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,607,456
App. No.
13/570,475
Granted
Dec 17, 2013
Kind
B1
Abstract

A method for producing, on the surface of a wall capable of being swept by a fluid, raised elements forming disruptions of the boundary layer is disclosed. The method includes applying laser shocks to the surface so as to create peaks on the edge of the impact zones such that the peaks form the disruptive raised elements.

Claims (15)

1. A method for producing, on a wall surface capable of being swept by a fluid, disruptive raised elements in a boundary layer, comprising:

identifying a desired transition zone on the wall surface between a laminar boundary layer and a turbulent boundary layer;

applying laser shocks to the transition zone on said surface so as to create peaks on a border of impact zones of said laser shocks; and

varying heights of the peaks by applying at least some of the laser shocks such that the laser shocks overlap,

wherein said overlap of the laser shocks results in a squashed peak on the border of the impact zones,

wherein the height of the squashed peak is a function of an amount of the overlap between the laser shocks such that the height of the squashed peak decreases as the amount of the overlap between laser shocks increases,

wherein the wall is of a turbomachine blade,

wherein the peaks constitute said disruptive raised elements,

wherein intensity of turbulence in the transition zone is controlled based on at least one of shape of the impacts, height of the peaks, or distance between laser shocks,

wherein the squashed peaks are applied in zones in which a slight roughness and laminar flow are desired; and

wherein said impact zones present a round or elliptical shape.

2. The method as claimed in claim 1 , wherein laser shocks are produced arranged so that the impacts produced are partially overlapping one another.

3. The method as claimed in claim 1 , wherein energy applied to the laser shocks is varied according to the impact zone, so as to obtain disruptive raised elements of different heights.

4. The method as claimed in claim 1 , wherein the wall is of a compressor blade of a gas turbine engine.

5. The method as claimed in claim 1 , wherein the laser shocks are applied on a suction side of the blade.

Assignments (2)
CORRECTIVE ASSIGNMENT TO CORRECT THE COVER SHEET TO REMOVE APPLICATION NOS. 10250419, 10786507, 10786409, 12416418, 12531115, 12996294, 12094637 12416422 PREVIOUSLY RECORDED ON REEL 046479 FRAME 0807. ASSIGNOR(S) HEREBY CONFIRMS THE CHANGE OF NAME. Recorded Aug 24, 2018
From: SNECMA
To: SAFRAN AIRCRAFT ENGINES
Reel/Frame 046939/0336 →
CHANGE OF NAME Recorded May 23, 2018
From: SNECMA
To: SAFRAN AIRCRAFT ENGINES
Reel/Frame 046479/0807 →