IP Library Granted Patent US 9,708,701
Granted Patent B2
US 9,708,701 · App. 13/577,924 · Granted Jul 18, 2017

Device for obtaining ceramic fibers coated by a liquid process with a thick metal sheath

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,708,701
App. No.
13/577,924
Granted
Jul 18, 2017
Kind
B2
Abstract

A device for metal coating of fibers, for example ceramic fibers, by a liquid process, the device including a crucible containing a liquid metal bath through which a fiber is drawn to be coated with the metal, and a cooling system positioned downstream from the metal bath to solidify the metal sheath created around the fiber by capillarity. The cooling system includes at least one nozzle for ejecting a compressed gas towards the coated fiber, and the system is sized such as to solidify the metal on the periphery of the coated fiber over a length of no more than 200 mm.

Claims (17)

1. A device for metal coating of fibers by liquid means, comprising:

a crucible containing a liquid metal bath through which a fiber is drawn to be coated with the metal;

a cooling system positioned downstream from the liquid metal bath to solidify a metal sheath created around the fiber by capillarity,

wherein the cooling system comprises at least one tube comprising an oblique lateral face oriented toward the fiber, on the downstream side of said tube relative to the motion of the fiber, and a nozzle provided in said face which is oriented toward the fiber, for ejecting a compressed gas shaped to eject the gas in a direction making an angle of less than 30° with a travel direction of the coated fiber and positioned at a distance of less than 5 mm from the liquid metal bath, and

wherein the system is sized to solidify the metal on the periphery of the coated fiber over a length of no more than 200 mm.

2. The device as claimed in claim 1 , wherein the cooling system comprises two series of tubes each bearing at least one nozzle, the tubes being placed face to face, on either side of the coated fiber as the coated fiber emerges from the liquid metal.

3. The device as claimed in claim 2 , wherein the at least one nozzle has a shape of a slit made in the tube extending perpendicular to the travel direction of the coated fiber.

4. The device as claimed in claim 1 , further comprising a mobile roller configured to shift the fiber so that the fiber passes through the liquid metal bath or not,

wherein the cooling system is positioned along the coated fiber, between the liquid metal bath and the mobile roller.

5. The device as claimed in claim 4 , wherein the cooling system comprises two series of tubes each bearing at least one nozzle for ejecting a compressed gas, the series being positioned on either side of the coated fiber as the coated fiber emerges from the liquid metal bath, along two planes parallel to one another and parallel to the coated fiber, so that the coated fiber can move between these planes, under action of the mobile roller to enter into or emerge from the liquid metal bath.

6. The device as claimed in claim 1 , wherein the travel direction of the fiber is a vertical direction.

7. The device as claimed in claim 1 , wherein each tube has a substantially hexagonal shape in cross section and bear six lateral faces.

8. A device for metal coating of fibers by liquid means, comprising:

a crucible containing a liquid metal bath through which a fiber is drawn to be coated with the metal;

a cooling system positioned downstream from the liquid metal bath to solidify a metal sheath created around the fiber by capillarity,

wherein the cooling system comprises at least one tube having a substantially hexagonal shape in cross section, and at least one nozzle oriented toward the fiber and provided on an oblique lateral side of said hexagonal tube at a downstream side of said tube relative to the motion of the fiber, for ejecting a compressed gas shaped to eject the gas in a direction making an angle of less than 30° with a travel direction of the coated fiber and positioned at a distance of less than 5 mm from the liquid metal bath, and

wherein the system is sized to solidify the metal on the periphery of the coated fiber over a length of no more than 200 mm.

Assignments (3)
CORRECTIVE ASSIGNMENT TO CORRECT THE COVER SHEET TO REMOVE APPLICATION NOS. 10250419, 10786507, 10786409, 12416418, 12531115, 12996294, 12094637 12416422 PREVIOUSLY RECORDED ON REEL 046479 FRAME 0807. ASSIGNOR(S) HEREBY CONFIRMS THE CHANGE OF NAME. Recorded Aug 24, 2018
From: SNECMA
To: SAFRAN AIRCRAFT ENGINES
Reel/Frame 046939/0336 →
CHANGE OF NAME Recorded May 23, 2018
From: SNECMA
To: SAFRAN AIRCRAFT ENGINES
Reel/Frame 046479/0807 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 13, 2012
From: FRANCHET, JEAN-MICHEL PATRICK MAURICE; KLEIN, GILLES CHARLES CASIMIR; SANCHEZ, GERALD
To: SNECMA
Reel/Frame 028774/0165 →