Bioactive bone graft substitute
View Patent ↗The invention relates to biocompatible bone graft materials for repairing bone defects and the application of such bone grafts. The devices of the invention comprise resorbable calcium phosphate, resorbable collagen and bioactive glasses.
1. A kit for the preparation of a bone graft comprising:
(a) a bone graft material comprising a blend of resorbable collagen and resorbable calcium phosphate; and
(b) a separate container that contains bioactive glass therein.
2. The kit of claim 1 , wherein the bioactive glass comprises combeite glass-ceramic, 45S5 glass, 45S5 glass-ceramic, 58S5 glass, S53P4 glass, apatite-wollastonite glass, or apatite-wollastonite glass-ceramic.
3. The kit of claim 1 , wherein the bioactive glass has a particle size of less than 150 μm.
4. The kit of claim 1 , wherein the bioactive glass is provided in a unit dose amount.
5. The kit of claim 1 , wherein the bioactive glass is combeite.
6. The kit of claim 1 , wherein the calcium phosphate is beta-TCP.
7. The kit of claim 1 , wherein the bone graft material has micro-, meso-, and macroporosity.
8. The kit of claim 1 , wherein the bone graft material is flexible, moldable, or flowable upon wetting.
9. The kit of claim 1 , wherein the blend is homogeneous.
10. The kit of claim 1 , wherein the bone graft comprises up to about 20% by weight of collagen.
11. The kit of claim 1 , wherein the bone graft comprises up to about 15% by weight of collagen.
12. The kit of claim 1 , wherein the bone graft comprises up to about 10% by weight of collagen.
13. The kit of claim 1 , wherein the bioactive glass is present in an amount such that when the bioactive glass is blended with the bone graft material to form the bone graft, the bone graft comprises up to about 40% by weight of bioactive glass.
14. The kit of claim 1 , wherein the bioactive glass is present in an amount such that when the bioactive glass is blended with the bone graft material to form the bone graft, the bone graft comprises up to about 20% by weight of bioactive glass.
15. The kit of claim 1 , wherein the bioactive glass is present in an amount such that when the bioactive glass is blended with the bone graft to form the bone graft, the bone graft comprises up to about 15% by weight of bioactive glass.
16. A method for restoring or repairing bone in a mammal comprising:
providing a biocompatible bone graft material of claim 1 ;
incorporating resorbable bioactive glass into the bone graft material to form a bone graft comprising calcium phosphate, collagen, and bioactive glass; and
placing the bone graft into a bony space.
17. The method of claim 16 , wherein the bioactive glass comprises combeite glass-ceramic, 45S5 glass, 45S5 glass-ceramic, 58S5 glass, S53P4 glass, apatite-wollastonite glass, or apatite-wollastonite glass-ceramic.
18. The method of claim 16 , further comprising wetting the bone graft material with a biologically compatible fluid prior to placing the bone graft into the bony space.
19. The method of claim 18 , wherein the biologically compatible fluid is bone marrow aspirate.
20. The method of claim 16 , wherein the bone graft material has micro-, meso-, and macroporosity.