IP Library Granted Patent US 9,109,117
Granted Patent B2
US 9,109,117 · App. 13/629,213 · Granted Aug 18, 2015

Process for making composite polymer

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,109,117
App. No.
13/629,213
Granted
Aug 18, 2015
Kind
B2
Abstract

In the process of forming a wood pulp fiber and thermoplastic polymer composition the step of adding mineral oil to the composition during mixing.

Claims (20)

1. A method of making a composition, comprising:

providing chemical wood pulp fibers in the form of particles, thermoplastic polymer, and mineral oil to a first mixing device,

wherein for every 100 weight percent of material provided to the first mixing device, the pulp fibers are 65 to 90 weight percent of the material and the mineral oil is 0.1 to 5 weight percent of the material,

mixing the fiber, the polymer and the mineral oil in the first mixing device to form a fiber/polymer blend in which the substantially individual chemical wood pulp fibers are dispersed within the polymer,

further mixing the fiber/polymer blend in a second mixing device, wherein the second mixing device uses split flow to disperse the fibers in the polymer, and

thereafter forming the fiber/polymer blend into pellets.

2. The method of claim 1 wherein the chemical wood pulp fibers are bleached chemical wood pulp fibers.

3. The method of claim 1 wherein the thermoplastic polymer is selected from the group consisting of a biopolymer, polylactic acid, cellulose acetate, cellulose propionate, cellulose butyrate, a polycarbonate, polyethylene terephthalate, a polyolefin, polyethylene, high density polyethylene, low density polyethylene, linear low density polyethylene, polypropylene, polystyrene, a polystyrene copolymer, an acrylonitrile-butadiene-styrene copolymer, a styrene block copolymer, polyvinyl chloride, and a recycled plastic.

4. The method of claim 1 wherein one or more of the first and the second mixing device has two intermeshing rotors.

5. The method of claim 1 wherein mineral oil is also added to the composition in the second mixing device.

6. A method of making a composition, comprising:

providing thermoplastic polymer, mineral oil, and particles consisting of chemical wood pulp fibers to a mixing device,

wherein for every 100 weight percent of material provided to the mixing device, the pulp fibers are 80 to 90 weight percent of the material and the mineral oil is 0.1 to 5 weight percent of the material,

mixing the particles, the polymer, and the mineral oil in the mixing device to form a fiber/polymer blend in which the pulp fibers are dispersed within the polymer, and

thereafter forming the fiber/polymer blend into pellets.

7. The method of claim 6 ,

wherein the mixing device is a first mixing device, and

wherein the method further includes, subsequent to mixing, further mixing the fiber/polymer blend in a second mixing device, wherein the second mixing device uses split flow to disperse the fibers in the polymer.

8. The method of claim 1 , wherein for every 100 weight percent of material provided to the mixing device, the pulp fibers are 75 to 90 weight percent of the material.

9. The method of claim 8 , wherein for every 100 weight percent of material provided to the mixing device, the pulp fibers are 80 to 90 weight percent of the material.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 14, 2025
From: INTERNATIONAL PAPER COMPANY
To: GCF US HOLDINGS LLC
Reel/Frame 073563/0717 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 5, 2019
From: WEYERHAEUSER NR COMPANY
To: INTERNATIONAL PAPER COMPANY
Reel/Frame 049964/0838 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 9, 2015
From: INTERFACIAL SOLUTIONS IP, LLC
To: WEYERHAEUSER NR COMPANY
Reel/Frame 035808/0994 →