Method of inhibiting surface gelation of an uncured gelcoat composition
View Patent ↗A method to prevent gelation of an uncured gelcoat composition during storage is described. The method includes applying a gelation inhibitor to the surface of a gelcoat composition in the container to prevent premature gelation. The gelation inhibitor additionally prevents the formation of a crust on the inner surface of storage container lids.
1. A method to inhibit surface gelation of an uncured gelcoat composition, comprising:
providing a storage container;
filling the storage container with the gelcoat composition; and
applying a gelation inhibitor to an upper surface of the gelcoat composition as a float having thickness of about 0.05 to 0.5 inches.
2. The method of claim 1 , wherein the gelation inhibitor is a solvent selected from the group consisting of hydrocarbons, ketones, alcohols and glycols.
3. The method of claim 1 , wherein the gelation inhibitor is a ketone.
4. The method of claim 3 , wherein the gelation inhibitor is acetone.
5. The method of claim 1 , wherein the gelation inhibitor is applied at a concentration of from about 0.25 wt % to about 0.75 wt % based on total weight of the gelcoat composition.
6. The method of claim 1 , wherein inhibiting surface gelation extends shelf-life of the gelcoat composition by at least 30 days at 70° F.
7. The method of claim 1 , wherein inhibiting surface gelation extends shelf-life of the gelcoat composition by at least 30 days at temperatures above 70° F.
8. The method of claim 7 , wherein elevated temperature comprises temperature of about 80° F. up to about 140° F.
9. The method of claim 1 , wherein applying the gelation inhibitor comprises pouring a fixed volume of the gelation inhibitor on top of the gelcoat composition.
10. The method of claim 1 , wherein the gelcoat composition
comprises about 25 wt % to about 94 wt % unsaturated polyester resin;
about 0.05 wt % to about 3 wt % promoter to initiate and facilitate cure of the gelcoat composition; and
about 5 wt % to about 50 wt % reactive diluent.
11. The method of claim 10 , wherein the reactive diluent comprises one or more monomers selected from the group consisting of styrenes, acrylates, methacrylates, phthalates, cyanurates, vinyl ethers, alcohols, polyols, esters of unsaturated monofunctional alcohols with C 1 -C 18 carboxylic acids, and mixtures thereof.
12. The method of claim 10 , wherein the reactive diluent comprises one or more monomers selected from the group consisting of styrene, methyl methacrylate, vinyl toluene, p-tert-butyl-styrene, p-methyl styrene, 2-hydroxyethyl methacrylate, ethylene dimethacrylate, and mixtures thereof.
13. The method of claim 10 , wherein the promoter comprises one or more compounds selected from the group consisting of metal compounds, amines, Lewis acids, quarternary ammonium salts, sulfur compounds, dimethyl acetoacetamide, ethyl acetoacetate, methyl acetoacetate, and mixtures thereof.
14. A method of inhibiting crust formation on at least an inner surface of a lid of a gelcoat storage container, comprising:
providing a storage container;
filling the storage container with the gelcoat composition; and
applying a gelation inhibitor to an upper surface of the gelcoat composition as a float having thickness of about 0.05 to 0.5 inches.