Radiant barrier
View Patent ↗A radiant barrier has a layer of a flexible polymer, such as TPO, and a layer of metallic aluminum bonded thereto. A reinforcement layer, such as a fiberglass scrim, and a layer of adhesive, such as EVA, may be used to strengthen the barrier and prevent de-lamination. LDPE may be incorporated into the TPO to increase strength. The barrier may also be a moisture barrier. The layers may be laminated by a heated roll set and the aluminum applied by vapor deposition.
1. A radiant barrier, consisting essentially of:
a laminate of a plurality of layers, including
a first layer of a flexible thermoplastic polyolefin (TPO) 50 to 70 microns thick;
a second layer of metallic aluminum 1 to 50 microns thick bonded to the first layer.
2. The radiant barrier of claim 1 , further comprising
a reinforcement layer disposed between the first layer and the second layer.
3. The radiant barrier of claim 2 , wherein the reinforcement layer includes fiberglass.
4. The radiant barrier of claim 3 , wherein the reinforcement layer further includes fibers made from at least one polymer.
5. The radiant barrier of claim 2 wherein the reinforcement layer contains fibers of at least two of fiberglass, polyester, polypropylene and Kevlar.
6. The radiant barrier of claim 2 , wherein the reinforcement layer is 75 to 100 microns thick.
7. The radiant barrier of claim 2 , further comprising a layer of ethyl vinyl acetate (EVA) interposed between at least two of the first layer, the second layer and the reinforcement layer.
8. The radiant barrier of claim 7 , further comprising a layer of low density polyethylene (LDPE) interposed between at least two of the first layer, the second layer, the reinforcement layer and the EVA layer.
9. The radiant barrier of claim 8 , wherein the layer of TPO and the layer of LDPE are mixed to form an intermixed layer.
10. The radiant barrier of claim 1 , wherein the radiant barrier has an emissivity in the range of 0.01 to 0.09, a reflectivity of at least 80 at wavelengths of light in the range of 250 nm to 2500 um at an incidence angle of 20 degrees.
11. The radiant barrier of claim 1 , further comprising a layer of adhesive interposed between the first and second layers to promote adhesion there between.
12. The radiant barrier of claim 1 , wherein the radiant barrier is also a moisture barrier.
13. The radiant barrier of claim 1 wherein the aluminum layer has a matte surface and a reflective surface and the reflective surface is positioned in the laminate to face a source of radiation when the radiant barrier is installed on a structure.
14. A radiant barrier, comprising:
a laminate having
a first layer of a mixture of thermoplastic polyolefin (TPO) and low density polyethylene (LDPE);
a second layer of metallic aluminum bonded to the first layer, wherein the volume of low density polyethylene (LDPE) intermixed with the TPO is present in a percentage amount in the range of 10% to 25% by volume relative to the volume of TPO.
15. The radiant barrier of claim 14 , wherein the second layer is applied to the first layer by vapor deposition.
16. The radiant barrier of claim 14 , wherein the first layer is mixed by converging a layer of TPO and a layer of LDPE under heat and pressure.
17. The radiant barrier of claim 16 , wherein the first layer and second layer are bonded by heat and pressure.