IP Library Granted Patent US 9,004,284
Granted Patent B2
US 9,004,284 · App. 13/841,191 · Granted Apr 14, 2015

Mineral slurry drying method and system

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,004,284
App. No.
13/841,191
Granted
Apr 14, 2015
Kind
B2
Abstract

The present invention provides methods and systems for reducing moisture in mineral slurries, particularly mineral slurries containing minerals of small particle diameter, using a granular drying material. The invention also relates to novel mineral products and intermediates useful in connection with the process. The method and system reduced moisture by contacting the mineral slurry with the granular drying material. The granular drying material is selected to be readily separated from the dried minerals using a size separation technique such as a sieve screen. The granular drying material is the regenerated, preferably using a process involving heat exchange and cross-flow air. The granular drying material is preferably capable of regeneration and recycling in a continuous process with minimal attrition.

Claims (29)

1. A method for reducing mineral slurry moisture comprising:

(a) contacting a first volume of mineral slurry with a second volume of granular drying media;

(b) reducing the moisture content of the mineral slurry by transferring moisture from minerals in the mineral slurry to the granular drying media; and

(c) separating the granular drying media from the minerals by difference in particle size, wherein the mineral slurry comprises a mineral that does not decompose at thermal drying temperatures,

wherein the process is continuous and at least a portion of the second volume of granular drying media is subjected to a step (d) of regenerating the granular drying media after step (c).

2. The method of claim 1 , wherein the first volume of mineral slurry has greater than 10% of particles of a diameter less than the average diameter of the granular drying media.

3. The method of claim 1 , wherein the first volume of mineral slurry has greater than 10% of particles smaller than 28 mesh.

4. The method of claim 1 , wherein the first volume of mineral slurry has greater than 50% of particles smaller than 28 mesh.

5. The method of claim 1 , wherein the first volume of mineral slurry has greater than 80% of particles smaller than 28 mesh.

6. The method of claim 1 , wherein the moisture content of the first volume of mineral slurry is greater than 20% by weight, and the moisture content of the mineral slurry is less than 10% by weight after step (c).

7. The method of claim 1 , wherein the granular drying media is spherical has a mean particle diameter ranging from approximately 2.0 mm to approximately 4.7 mm.

8. The method of claim 1 , wherein the granular drying media is spherical has a mean particle diameter of approximately 3.2 mm.

9. The method of claim 1 , wherein the granular drying media has a crush strength that exceeds 25 lbs.

10. The method of claim 1 , wherein the granular drying media has a surface area of greater than or equal to 340 m 2 /g.

11. The method of claim 1 , wherein the mineral is a metallic ore.

12. The method of claim 1 , wherein the mineral slurry comprises iron ore, salt, bauxite, phosphates, gypsum, alumina, maganese, aluminum, potash, chromium, kaolin, magnetite, feldspar, copper, bentonite, zinc, barytes, titanium, fluorspar, borates, lead, sulphur, perlite, diatomite, graphite, asbestos, nickel, zirconium, or zinc.

13. The method of claim 1 , wherein the first volume of mineral slurry has been subjected to a size separation step prior to step (a).

14. The method of claim 1 , wherein the first volume of mineral slurry has been subjected to a moisture reduction step prior to step (a).

15. The method of claim 1 , wherein the second volume of granular drying media comprises a molecular sieve, a hydratable polymer, a desiccant or a mixture thereof.

16. The method of claim 1 , wherein the second volume of granular drying media comprises activated alumina.

17. The method of claim 1 , wherein step (c) is conducted using a sieve screen.

18. A method for reducing mineral slurry moisture comprising:

(a) contacting a first volume of mineral slurry with a second volume of granular drying media:

(b) reducing the moisture content of the mineral slurry by transferring moisture from minerals in the mineral slurry to the granular drying media; and

(c) separating the granular drying media from the minerals by difference in particle size, wherein the mineral slurry comprises a mineral that does not decompose at thermal drying temperatures, further comprising a step (d) of regenerating the granular drying media after step (c), wherein the step (d) of regenerating the granular drying media utilizes a combination of heat exchange and cross-flow air.

19. The method of claim 18 , wherein the second volume of granular drying media comprises activated alumina.

20. The method of claim 18 , wherein the mineral slurry comprises iron ore, salt, bauxite, phosphates, gypsum, alumina, maganese, aluminum, potash, chromium, kaolin, magnetite, feldspar, copper, bentonite, zinc, barytes, titanium, fluorspar, borates, lead, sulphur, perlite, diatomite, graphite, asbestos, nickel, zirconium, or zinc.

21. The method of claim 18 , wherein the second volume of granular drying media comprises a molecular sieve, a hydratable polymer, a desiccant or a mixture thereof.

22. The method of claim 18 , wherein the method is continuous.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 8, 2015
From: BLAND, RICHARD W.; MCDANIEL, BRUCE
To: VITRINITE SERVICES, LLC
Reel/Frame 036506/0857 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 5, 2015
From: BLAND, RICHARD W.; MCDANIEL, BRUCE
To: VITRINITE SERVICES, LLC
Reel/Frame 034632/0090 →