IP Library Granted Patent US 9,356,312
Granted Patent B2
US 9,356,312 · App. 13/864,564 · Granted May 31, 2016

Method for preparing secondary battery and the secondary battery prepared by using the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,356,312
App. No.
13/864,564
Granted
May 31, 2016
Kind
B2
Abstract

Disclosed is a method for producing a secondary battery in which an electrode assembly comprising a cathode, an anode and a separator interposed between the cathode and the anode is accommodated in a battery case, the method comprising inserting the electrode assembly into the battery case, injecting an electrolyte into the battery case accommodating the electrode assembly to obtain a secondary battery, storing the secondary battery at a SOC of 1 to 20 for 3 hours to 10 days, removing gas present in the secondary battery, and sealing the battery case, wherein the anode comprises lithium titanium oxide (LTO) represented by the following Formula 1 as an anode active material: Li a Ti b O 4−c A c   (1) wherein a, b and c are determined according to an oxidation number of M′ within ranges of 0.5≦a≦3, 1≦b≦2.5, and 0≦c<0.2; and A is at least one monovalent or bivalent anion. Disclosed is also a secondary battery produced by the method.

Claims (30)

1. A method for producing a secondary battery in which an electrode assembly comprising a cathode, an anode and a separator interposed between the cathode and the anode is accommodated in a battery case, the method comprising:

inserting the electrode assembly into the battery case;

injecting an electrolyte into the battery case accommodating the electrode assembly to obtain a secondary battery;

storing the secondary battery at a SOC of 1 to 20% for 3 hours to 10 days;

removing gas present in the secondary battery; and

sealing the battery case,

wherein the anode comprises lithium titanium oxide (LTO) represented by the following Formula 1 as an anode active material:

Li a Ti b O 4−c A c   (1)

wherein a, b and c are determined according to an oxidation number within ranges of 0.5≦a≦3, 1≦b≦2.5, and 0≦c<0.2; and

A is at least one monovalent or bivalent anion.

2. The method according to claim 1 , wherein the storing is carried out at 40° C. to 70° C.

3. The method according to claim 1 , wherein the lithium titanium oxide of Formula 1 is Li 1.33 Ti 1.67 O 4 or LiTi 2 O 4 .

4. A secondary battery produced by the method according to claim 1 .

5. The secondary battery according to claim 4 , wherein the secondary battery is accommodated in a rectangular, cylindrical or pouch battery case.

6. The secondary battery according to claim 5 , wherein the pouch battery case comprises a laminate sheet including a resin layer and a metal layer.

7. The secondary battery according to claim 6 , wherein the laminate sheet has a laminate structure including an outer resin layer, an air and moisture-blocking metal layer, and a heat-fusing inner resin layer.

8. The secondary battery according to claim 4 , wherein the secondary battery comprises lithium manganese composite oxide with a spinel structure represented by the following Formula 2 as a cathode active material:

Li x M′ y Mn 2−y O 4−z A z   (2)

wherein 0.9≦x≦1.2, 0<y<2, and 0≦z<0.2;

M′ is at least one element selected from the group consisting of Al, Mg, Ni, Co, Fe, Cr, V, Ti, Cu, B, Ca, Zn, Zr, Nb, Mo, Sr, Sb, W, Ti and Bi; and

A is at least one monovalent or bivalent anion.

9. The secondary battery according to claim 8 , wherein the lithium manganese composite oxide of Formula 2 is lithium nickel manganese oxide represented by the following Formula 3:

Li x Ni y Mn 2−y O 4   (3)

wherein 0.9≦x≦1.2, and 0.4≦y≦0.5.

10. The secondary battery according to claim 9 , wherein the lithium nickel manganese oxide of Formula 3 is LiNi 0.5 Mn 1.5 O 4 or LiNi 0.4 Mn 1.6 O 4 .

11. The secondary battery according to claim 10 , wherein the secondary battery is a lithium secondary battery.

12. A battery module comprising the secondary battery according to claim 4 as a unit battery.

13. A battery pack comprising the battery module according to claim 12 .

14. A device comprising the battery pack according to claim 13 .

15. The device according to claim 14 , wherein the device is an electric vehicle, a hybrid electric vehicle, a plug-in hybrid electric vehicle or a power storage system.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2021
From: LG CHEM, LTD.
To: LG ENERGY SOLUTION, LTD.
Reel/Frame 058295/0068 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 18, 2014
From: LEE, YOUNKYOUNG; KIM, JIHYUN; LEE, SEONGMIN
To: LG CHEM, LTD.
Reel/Frame 033765/0420 →