Anti-corrosion anti-reflection glass and related methods
View Patent ↗Certain example embodiments relate to methods of making anti-corrosion anti-reflection (ACAR) films, and/or associated coated articles. The methods may involve forming the reaction product of a hydrolysis and/or a condensation reaction of at least one hybrid alkoxide selected from the group consisting of Si(OR) 4 —Al(s-OBu) 3 , Si(OR) 4 —B(OBu) 3 and Si(OR) 4 and Zr(OBu) 4 , where R is a CH 2 CH 3 group, s-OBu is sec-butoxide and OBu is n-butoxide. The solution optionally may be blended and/or mixed with silicon nanoparticles and/or siloxanes. A Tqe % gain of about 3.2% and/or refractive index of 1.5 or less is/are possible in certain example embodiments.
1. A method of making a coated article comprising an anti-reflection coating supported by a glass substrate, the method comprising:
depositing, directly or indirectly, on the glass substrate at least a portion of a solution comprising at least one hybrid alkoxide comprising Si(OR) 4 and Zr(OBu) 4 , where R is a CH 2 CH 3 group, and OBu is n-butoxide, respectively;
wherein the solution comprises a weight ratio of ZrO 2 to SiO 2 of greater than 1.0; and
curing the deposited solution and/or allowing the deposited solution to cure, in making the anti-reflection coating.
2. The method according to claim 1 , wherein the solution comprises a silicon nanoparticle and siloxanes.
3. The method according to claim 1 , wherein the solution comprises tetraethyl orthosilicates.
4. The method according to claim 1 , wherein the anti-reflection coating has a refractive index less than 1.5.