Method for preparing a polymer conjugate
View Patent ↗Provided herein is a straightforward and efficient method for covalently attaching a polyethylene glycol polymer to a taxane. The method involves, among other things, a step of reacting a taxane with a polyethylene glycol polymer comprising a functional group reactive with a functional group within said taxane in the presence of a coupling reagent and DPTS. The result of the reacting step is the formation of a polyethylene glycol-taxane conjugate.
1. A method for covalently attaching a polyethylene glycol polymer to an active agent, said method comprising the step of:
reacting a small molecule active agent having a molecular weight of less than about 800 Daltons and having a single hydroxyl group with a linear polyethylene glycol having a single functional group reactive with a hydroxyl group in the presence of a coupling reagent and 4-(dimethylamino)-pyridinium-p-toluenesulfonate (DPTS), under conditions effective to promote reaction between the single hydroxyl group of the small molecule active agent and the single functional group of the linear polyethylene glycol to thereby form a polyethylene glycol-small molecule active agent conjugate.
2. The method of claim 1 , wherein said coupling reagent is a carbodiimide.
3. The method of claim 2 , wherein said coupling reagent is selected from the group consisting of dicyclohexylcarbodiimide (DCC), N,N′-diisopropylcarbodiimide (DIC), 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide hydrochloride (EDAC), 1-(3-dimethylaminopropyl)-3-ethylcarbodiimide (EDC), N-tert-butyl-N′-methylcarbodiimide (TBMC), and N-tert-butyl-N′-ethylcarbodiimide (TBEC).
4. The method of claim 1 , wherein said coupling reagent is N,N′-diisopropylcarbodiimide.
5. The method of claim 1 , wherein said reacting step is carried out in an organic solvent selected from the group consisting of dichloromethane, chloroform, acetonitrile and tetrahydrofuran.
6. The method of claim 5 , wherein said reacting step is carried out at a temperature ranging from 0° C. to 100° C.
7. The method of claim 6 , wherein said reacting step is carried out at room temperature.
8. The method of claim 1 , wherein the amount of DPTS in said reacting step ranges from about 0.05 to 0.75 equivalents relative to said single hydroxyl group within said small molecule active agent.
9. The method of claim 8 , wherein the amount of DPTS in said reacting step ranges from about 0.10 to 0.60 equivalents relative to said single hydroxyl group within said small molecule active agent.
10. The method of claim 1 , wherein the amount of said coupling reagent ranges from about 1.25 to 5 equivalents relative to said single hydroxyl group within said small molecule active agent.
11. The method of claim 1 , wherein the single functional group of the linear polyethylene glycol is carboxyl.
12. The method of claim 1 , wherein said reaction results in formation of an ester bond.