IP Library Patent Application 14157736
Patent Application
App. No. 14/157,736

EXTRUDED PET PARISON, CONTAINER, AND METHOD

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
14/157,736
Abstract

An extruded PET parison includes a first extruded polymer comprising PET, and a second extruded polymer comprising PET. In embodiments, the first extruded polymer and the second extruded polymer are co-extruded, and the first extruded polymer has an intrinsic viscosity that is higher that the intrinsic viscosity of the second extruded polymer. A monolayer embodiment is also disclosed. In embodiments, a monolayer extruded PET container is comprised of bottle grade PET resin that has been solid stated and may have an IV from about 0.96 to about 1.4.

Claims (21)

1 . An extruded PET parison comprising:

a first extruded polymer comprising PET; and

a second extruded polymer comprising PET;

wherein the first and second polymers are co-extruded, the first and second extruded polymers are in a solid state, and the first extruded polymer has an intrinsic viscosity that is higher that the intrinsic viscosity of the second extruded polymer.

2 . The parison of claim 1 , wherein the first extruded polymer has an intrinsic viscosity of at least 0.96.

3 . The parison of claim 1 , wherein the first extruded polymer has an intrinsic viscosity from about 1.0 to about 1.4.

4 . The parison of claim 1 , wherein the second extruded polymer has an intrinsic viscosity of less than 0.85.

5 . The parison of claim 1 , wherein the second extruded polymer has an intrinsic viscosity of about 0.80 to about 0.87.

6 . The parison of claim 1 , wherein the second extruded polymer comprises post-consumer recycled (PCR) PET or regrind PET.

7 . The parison of claim 1 , wherein the second extruded polymer includes a colorant.

8 . The parison of claim 1 , wherein the cross-sectional thickness of the first extruded polymer is at least about 0.20 of the total parison thickness.

9 . The parison of claim 1 , wherein the cross-sectional thickness of the second extruded polymer is less than about 0.80 of the total parison thickness.

10 . The parison of claim 1 , including one or more additional extruded polymer layers.

11 . The parison of claim 10 , wherein the one or more additional extruded polymer layers comprise recycled or reground material.

12 . A container formed from the parison of claim 1 .

13 . An extruded PET parison comprising:

an extruded monolayer polymer comprising PET;

wherein the extruded monolayer polymer is in a solid state, and the extruded monolayer polymer has an intrinsic viscosity from about 0.96 to about 1.4 and is devoid of chain extenders.

14 . The parison of claim 13 , wherein the intrinsic viscosity is about 1.1.

15 . A container formed from the parison of claim 13 .

16 . The container of claim 15 , wherein the container is substantially free of striations and haze.

Assignments (1)
SECURITY INTEREST Recorded Oct 12, 2017
From: PLASTIPAK PACKAGING, INC.
To: WELLS FARGO BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 044204/0547 →