Method and arrangement for vortex reduction in a metal making process

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,360,255
App. No.
14/192,345
Granted
Jun 7, 2016
Kind
B2
Abstract

A method for reducing vortex formation in molten metal when bottom tapping the molten metal from a metallurgical vessel in a metal making process. The method includes the steps of tapping the molten metal via a tapping hole in the metallurgical vessel, and providing a flow of the molten metal in the metallurgical vessel while tapping via a time-varying electromagnetic field applied to the metallurgical vessel, the flow of the molten metal being such that it constantly moves vortices in the molten metal away from a tapping hole region during the tapping to thereby prevent accumulation of the vortices for vortex formation over the tapping hole. It is also presented an arrangement for carrying out the method.

Claims (19)

1. A method for reducing vortex formation in molten metal when bottom tapping the molten metal from a metallurgical vessel in a metal making process, wherein the method comprises:

tapping the molten metal via a tapping hole in the metallurgical vessel, and

providing a flow of the molten metal in the metallurgical vessel while tapping by means of a time-varying electromagnetic field applied to the metallurgical vessel and provided by an electromagnetic stirrer,

wherein the time-varying electromagnetic field provides a forced convection of the molten metal in the metallurgical vessel, and

wherein the flow of the molten metal is such that the flow constantly moves vortices in the molten metal away from a tapping hole region of the metallurgical vessel and towards a wall of the metallurgical vessel to thereby prevent accumulation of the vortices and vortex formation over the tapping hole.

2. The method as claimed in claim 1 , wherein the flow of the molten metal is in a direction transverse to a central axis of the tapping hole.

3. The method as claimed in claim 1 , wherein the molten metal flows towards a first inner wall portion of the metallurgical vessel at the bottom of the metallurgical vessel and towards a second inner wall portion opposite the first inner wall portion at the surface of the molten metal.

4. The method as claimed in claim 1 , wherein the time-varying electromagnetic field has such strength that a flow rate of the molten metal is in the range 0.1-1 m/s.

5. The method as claimed in claim 4 , wherein the flow rate is in the range 0.1-0.6 m/s.

6. An arrangement for a metal making process, the arrangement comprising:

a metallurgical vessel for accommodating molten metal, the metallurgical vessel having a tapping hole for bottom tapping the molten metal from the metallurgical vessel, and

an electromagnetic stirrer arranged to generate a time-varying electromagnetic field in molten metal arranged in the metallurgical vessel,

wherein the electromagnetic stirrer comprises a coil arrangement, a frequency converter for operating the coil arrangement and a control unit for controlling the frequency converter such that the electromagnetic stirrer generates a time-varying electromagnetic field which is applied to the metallurgical vessel and which generates a time-varying electromagnetic field in the molten metal during tapping of the molten metal from the metallurgical vessel to thereby generate a flow of the molten metal in the metallurgical vessel, and

wherein the time-varying electromagnetic field is such that it provides a forced convection of the molten metal in the metallurgical vessel such that the flow constantly moves vortices away from a tapping hole region and towards a wall of the metallurgical vessel during the tapping to thereby prevent accumulation of the vortices for vortex formation over the tapping hole.

7. The arrangement as claimed in claim 6 , wherein the metallurgical vessel is an electric arc furnace.

8. The arrangement as claimed in claim 6 , wherein the time-varying electromagnetic field is configured to generate a flow of the molten metal which is transverse to a central axis of the tapping hole.

9. The arrangement as claimed in claim 6 , wherein the time-varying electromagnetic field is configured to generate a flow of the molten metal towards a first inner wall portion of the metallurgical vessel at the bottom of the metallurgical vessel and towards a second inner wall portion opposite the first inner wall portion at the surface of the molten metal.

10. The arrangement as claimed in claim 6 , wherein the electromagnetic field is configured to generate a flow rate of the molten metal is-in the range 0.1-1 m/s.

11. The arrangement as claimed in claim 10 , wherein the flow rate is in the range 0.1-0.6 m/s.

Assignments (2)
MERGER Recorded Dec 26, 2019
From: ABB RESEARCH LTD.
To: ABB SCHWEIZ AG
Reel/Frame 051419/0309 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 2, 2014
From: ERIKSSON, JAN-ERIK; KROON, TORD; RAHMANI, MOHAMED ALI; WIDLUND, OLA; ZHANG, XIAOJING; CARLSSON, CHRISTER; YANG, HONGLIANG
To: ABB RESEARCH LTD.
Reel/Frame 033007/0072 →