Systems and methods of protecting electrolysis cell sidewalls

Inventors: Xinghua Liu (Murrysville, PA); Douglas A. Weirauch, Jr. (State College, PA); Frankie E. Phelps (Apollo, PA); Joseph M. Dynys (New Kensington, PA); Jonell Kerkhoff (Murrysville, PA); Robert A. DiMilia (Greensburg, PA)
Assignee: Alcoa USA Corp.
C25C3/08C25C3/085C25C3/14C25C3/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,771,659
App. No.
14/206,300
Granted
Sep 26, 2017
Kind
B2
Abstract

A system is provided including an electrolysis cell configured to retain a molten electrolyte bath, the bath including at least one bath component, the electrolysis cell including: a bottom, and a sidewall consisting essentially of the at least one bath component; and a feeder system, configured to provide a feed material including the least one bath component to the molten electrolyte bath such that the at least one bath component is within 2% of saturation, wherein, via the feed material, the sidewall is stable in the molten electrolyte bath.

Claims (60)

1. An electrolysis cell, comprising:

an anode;

a cathode in spaced relation from the anode;

a molten electrolyte bath in liquid communication with the anode and the cathode, wherein the molten electrolyte bath comprises a bath chemistry including at least one bath component;

a cell body having: a bottom and at least one sidewall surrounding the bottom, wherein the cell body is configured to retain the molten electrolyte bath, wherein the sidewall consists essentially of the at least one bath component, the sidewall further comprising:

a first sidewall portion, configured to fit onto a thermal insulation package of the sidewall and retain the electrolyte; and

a second sidewall portion configured to extend up from the bottom of the cell body,

wherein the second sidewall portion is longitudinally spaced from the first sidewall portion, such that the first sidewall portion, the second sidewall portion, and a base between the first portion and the second portion define a trough;

wherein the trough is configured to receive a protecting deposit and retain the protecting deposit separately from the cell bottom;

wherein the protecting deposit is configured to dissolve from the trough into the molten electrolyte bath such that the molten electrolyte bath comprises a level of the at least one bath component which is sufficient to maintain the first sidewall portion and second sidewall portion in the molten electrolyte bath.

2. The electrolysis cell of claim 1 , wherein the bath component comprises an average bath content of: within 1% of saturation.

3. The electrolysis cell of claim 1 , wherein the saturation of the bath component is: at least 95% of saturation.

4. The electrolysis cell of claim 1 , wherein the bath component comprises a bath content saturation percentage measured at a location adjacent to the sidewall.

5. The electrolysis cell of claim 4 , wherein the location adjacent to the sidewall further comprises: not greater than 6″ from the sidewall.

6. An electrolysis cell, comprising:

an anode;

a cathode in spaced relation from the anode;

a molten electrolyte bath in liquid communication with the anode and the cathode, wherein the molten electrolyte bath comprises a bath chemistry including at least one bath component;

a cell body having: a bottom and at least one sidewall surrounding the bottom, wherein the cell body is configured to retain the molten electrolyte bath, wherein the sidewall consists essentially of the at least one bath component, the sidewall further comprising:

a first sidewall portion, configured to fit onto a thermal insulation package of the sidewall and retain the electrolyte; and

a second sidewall portion configured to extend up from the bottom of the cell body, wherein the second sidewall portion is longitudinally spaced from the first sidewall portion, such that the first sidewall portion, the second sidewall portion, and a base between the first portion and the second portion define a trough; wherein the trough is configured to receive a protecting deposit and retain the protecting deposit separate from the cell bottom;

wherein the protecting deposit is configured to dissolve from the trough into the molten electrolyte bath such that the molten electrolyte bath comprises a level of the at least one bath component which is sufficient to maintain the first sidewall portion and second sidewall portion in the molten electrolyte bath; and

a directing member, wherein the directing member is positioned between the first sidewall portion and the second sidewall portion, further wherein the directing member is laterally spaced above the trough, such that the directing member is configured to direct the protecting deposit into the trough.

7. The electrolysis cell of claim 6 , wherein the bath component comprises an average bath content of: within 1% of saturation.

8. The electrolysis cell of claim 6 , wherein the saturation of the bath component is: at least 95% of saturation.

9. The electrolysis cell of claim 6 , wherein the bath component comprises a bath content saturation percentage measured at a location adjacent to the sidewall.

10. The electrolysis cell of claim 9 , wherein the location adjacent to the sidewall further comprises: not greater than 6″ from the sidewall.

11. An assembly, comprising:

an electrolysis sidewall having a first portion and a second portion,

wherein the second portion is configured to align with the first sidewall portion with respect to a thermal insulation package,

further wherein the second sidewall portion is configured to extend from the sidewall in a stepped configuration,

wherein the second sidewall portion comprises an upper surface and a side surface which define the stepped portion.

12. The assembly of claim 11 , wherein the upper surface is configured to provide a planar surface.

13. The assembly of claim 11 , wherein the upper surface is configured to provide a sloped surface, wherein the sloped surface comprises a slope towards the first sidewall portion to provide, via cooperation between the first sidewall portion and the upper surface of the second sidewall portion, a recessed area.

14. The assembly of claim 13 , wherein the recessed area is configured to retain a protecting deposit therein.

15. The assembly of claim 14 , wherein the protecting deposit comprises the at least one bath component.

16. The assembly of claim 11 , wherein a base comprises an at least one bath component.

17. The assembly of claim 16 , wherein the bath component comprises an average bath content of: within 1% of saturation.

18. The assembly of claim 16 , wherein the saturation of the bath component is: at least 95% of saturation.

19. The assembly of claim 16 , wherein the bath component comprises a bath content saturation percentage measured at a location adjacent to the sidewall.

20. The assembly of claim 19 , wherein the location adjacent to the sidewall further comprises: not greater than 6″ from the sidewall.

21. The assembly of claim 11 , wherein a protecting deposit extends from a trough and up to at least an upper surface of an electrolyte bath.

22. The assembly of claim 11 , comprising:

a directing member, wherein the directing member is positioned between the first sidewall portion and the second sidewall portion,

further wherein the directing member is positioned above a base of a trough, further wherein the directing member is configured to direct a protecting deposit into the trough.

23. The assembly of claim 22 , wherein the directing member is constructed of a material which is present in a bath chemistry, such that via the bath chemistry, the directing member is maintained in the molten salt electrolyte.

24. The assembly of claim 11 , wherein a base of a trough is defined by a feed block, wherein the feed block is constructed of a material selected from components in a bath chemistry, wherein via the bath chemistry, the feed block is maintained in the molten salt bath.

25. The assembly of claim 11 , further comprising a feeder configured to provide a protecting deposit in a trough.

26. A method, comprising:

passing current between an anode and a cathode through a molten electrolyte bath of an electrolytic cell,

feeding a feed material into the electrolytic cell to supply the molten electrolyte bath with at least one bath component,

wherein feeding is at a rate sufficient to maintain a bath content of the at least one bath component to within 95% of saturation and not greater than 100% of saturation; and

via the feeding step, maintaining a sidewall of the electrolytic cell constructed of a material including the at least one bath component.

27. The method of claim 26 , comprising:

concomitant to the first step, maintaining the bath at a temperature not exceeding 960° C., such that the sidewalls of the cells are substantially free of a frozen ledge.

28. The method of claim 26 , comprising: consuming a protecting deposit to supply metal ions to the electrolyte bath.

29. The method of claim 26 , comprising: producing a metal product from the at least one bath component.

30. The method of claim 26 , wherein the bath component comprises an average bath content of: within 1% of saturation.

31. The method of claim 26 , wherein the bath component comprises a bath content saturation percentage measured at a location adjacent to the sidewall.

32. The method of claim 31 , wherein the location adjacent to the sidewall further comprises: not greater than 6″ from the sidewall.

Assignments (5)
RELEASE OF SECURITY INTEREST Recorded Sep 28, 2022
From: JPMORGAN CHASE BANK, N.A.
To: ALCOA USA CORP.
Reel/Frame 061558/0257 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 18, 2019
From: ALCOA USA CORP.
To: ELYSIS LIMITED PARTNERSHIP
Reel/Frame 048624/0566 →
SECURITY INTEREST Recorded Jan 27, 2017
From: ALCOA USA CORP.
To: JPMORGAN CHASE BANK, N.A., AS ADMINISTRATIVE AGENT
Reel/Frame 041521/0521 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 3, 2016
From: ALCOA INC.
To: ALCOA USA CORP.
Reel/Frame 040556/0141 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 15, 2014
From: LIU, XINGHUA; WEIRAUCH, DOUGLAS A., JR.; PHELPS, FRANKIE E.; DYNYS, JOSEPH M.; KERKHOFF, JONELL; DIMILIA, ROBERT A.
To: ALCOA INC.
Reel/Frame 034507/0715 →
Continuity (2)
Provisional Application 61780493 · Mar 13, 2013
Related Publication 20140262807A1 · Sep 18, 2014