IP Library Granted Patent US 11,078,409
Granted Patent B2
US 11,078,409 · App. 14/278,124 · Granted Aug 3, 2021

Electrically conductive proppant coating and related methods

Inventor: Joe D. Allison (Bartlesville, OK)
Assignee: CONOCOPHILLIPS COMPANY
C09K8/805E21B43/267E21B47/125
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,078,409
App. No.
14/278,124
Granted
Aug 3, 2021
Kind
B2
Abstract

An electrically conductive proppant coating and a method for applying the coating to the proppant, whereby the coated electrically conductive proppant can determine formation characteristics, such as dimensions, orientation, and conductivity.

Claims (26)

1. A method for determining geometry of a fracture in a subterranean formation, the method comprising:

a. injecting a coated proppant into the fracture to cause the fracture to function as an emitting antenna while opening the fracture or holding the fracture open, the coated proppant including a proppant suspended in an electrically-conductive coating, the electrically-conductive coating (i) deposited on a proppant surface of the proppant, (ii) stabilized with an oxidizing agent, and (iii) including a mixture of carbon residue forming material and a solvent, the coated proppant carbonized and graphitized, the carbon residue forming material being petroleum pitch, the solvent being toluene, xylene, quinoline, tetrahydrofuran, tetralin, or naphthalene;

b. sending, via electrical connections, a time-varying electrical signal into the fracture to charge the coated proppant, the time-varying electrical signal generated at a top surface above the fracture;

c. detecting, via a plurality of surface antennas at the top surface, the time-varying electrical signal, the plurality of surface antennas spaced from each other over an area above the fracture; and

d. determining the geometry of the fracture based on the time-varying electrical signal detected by the plurality of surface antennas.

2. The method according to claim 1 , wherein the solvent is toluene.

3. The method according to claim 1 , wherein the solvent is xylene.

4. The method according to claim 1 , wherein the electrically-conductive coating is graphitized immediately after being carbonized.

5. The method according to claim 1 , wherein the electrical connections extend from the surface of the fracture to a well casing.

6. The method according to claim 1 , wherein the electrical connections extend to a mud pit.

7. The method according to claim 1 , wherein the time-varying electrical signal is generated via a reversing DC current.

8. The method according to claim 1 , wherein the time-varying electrical signal is generated via an AC current.

9. The method according to claim 1 , wherein the detecting the time-varying electrical signal includes recording the time-varying electrical signal.

10. The method according to claim 1 , wherein the plurality of surface antennas are spaced from each other over different parts of the fracture.

11. The method according to claim 1 , wherein the oxidizing agent is a gaseous oxidizing agent.

12. The method according to claim 11 , wherein the gaseous oxidizing agent is selected from a group consisting of oxygen, sulfur fumes, gaseous oxides, nitrogen oxide gas, ambient air, halogens or combinations thereof.

13. A method for determining geometry of a fracture in a subterranean formation, the method comprising:

a. injecting a coated proppant into the fracture, the coated proppant including a proppant suspended in an electrically-conductive coating material deposited on a surface of the proppant and stabilized with an oxidizing agent, the coated proppant carbonized and graphitized;

b. sending a time-varying electrical signal into the fracture to charge the coated proppant;

c. detecting, via a plurality of surface antennas, the time-varying electrical signal, the plurality of surface antennas spaced from each other over an area above the fracture; and

d. determining the geometry of the fracture based on the time-varying electrical signal detected by the plurality of surface antennas.

14. The method according to claim 13 , wherein the coating material includes a mixture of carbon residue forming material and a solvent or combination of solvents.

15. The method according to claim 14 , wherein the carbon residue forming material is petroleum pitch.

16. The method according to claim 14 , wherein the solvent or combination of solvents is selected from a group consisting of toluene, xylene, quinoline, tetrahydrofuran, tetralin, naphthalene or combinations thereof.

17. The method according to claim 13 , wherein the coated proppant is injected into the fracture during creation of the fracture.

18. The method according to claim 13 , wherein the plurality of surface antennas are spaced from each other over different parts of the fracture.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 3, 2021
From: ALLISON, JOE D.
To: CONOCOPHILLIPS COMPANY
Reel/Frame 055476/0348 →
Continuity (2)
Provisional Application 61824811 · May 17, 2013
Related Publication 20140338898A1 · Nov 20, 2014
Cited By (9)
US 12,365,828 US 12,466,992 US 12,521,764 US 12,540,273 US 12,637,611 US 12,649,875 US 12,650,066 US 12,662,624 US 12,674,380