Crosslinked speek cation exchange membrane having improved chemical stability by radiation and method of preparing the same
Provided is a method of preparing a crosslinked sulfonated poly(ether ether ketone) (SPEEK) cation exchange membrane including: preparing a crosslinker mixture of a first crosslinker containing two or more vinyl oxy groups and a second crosslinker containing three or more vinyl groups; preparing a mother liquor containing the crosslinker mixture, a SPEEK polymer substituted with sodium, and a solvent; and casting the mother liquor and then irradiating radiation thereon.
1. A method of preparing a crosslinked sulfonated poly(ether ether ketone) (SPEEK) cation exchange membrane, the method comprising:
preparing a crosslinker mixture, wherein the crosslinker mixture comprises:
a first crosslinker represented by Chemical Formula 1, wherein the first crosslinker is present in an amount of 60 to 95 wt % of a total amount of the crosslinker mixture; and
a second crosslinker, wherein the second crosslinker comprises at least one of triallyl isocyanurate or pentaerythritol triallyl ether, and is present in an amount of 5 to 40 wt % of the total amount of the crosslinker mixture;
preparing a mother liquor containing the crosslinker mixture, a SPEEK polymer substituted with sodium, and a solvent;
casting the mother liquor; and
irradiating the mother liquor with a radioactive ray,
wherein A is at least one selected from the group consisting of
and each of m and n is independently an integer of 1 to 5, and
wherein each of R 1 to R 10 is independently at least one selected from the group consisting of hydrogen, and a C 1 ˜C 6 alkyl.
2. The method of claim 1 , wherein the mother liquor contains 0.1 to 20 wt % of the crosslinker mixture, 1 to 30 wt % of the SPEEK polymer substituted with sodium, and 65 to 95 wt % of the solvent.
3. The method of claim 1 , wherein the first crosslinker contains any one or at least two selected from 1,4-butanediol divinyl ether, 1,6-hexanediol divinyl ether, di(ethylene glycol) divinyl ether, tri(ethylene glycol) divinyl ether, tetra(ethylene glycol) divinyl ether, and 1,4-cyclohexanedimethanol divinyl ether.
4. The method of claim 1 , wherein the solvent is any one or a mixture of at least two selected from a group consisting of N,N-dimethylacetamide, N-methyl-2-pyrrolidone, dimethylsulfoxide, tetrahydrofuran, dimethylformamide, toluene, cyclohexane, benzene, chlorobenzene, diphenyl ether, and 1,3,5-trimethylbenzene.
5. The method of claim 1 , wherein the radioactive ray is any one selected from a group consisting of gamma ray, UV ray, and electron ray.
6. The method of claim 5 , wherein the radioactive ray is the electron ray.
7. The method of claim 1 , wherein the radioactive ray is irradiated at a dose rate of 0.1 to 10 kGy/min and an irradiation dose of 50 to 600 kGy.
8. The method of claim 1 , wherein the radioactive ray is irradiated at a dose rate of 1 to 7 kGy/min and an irradiation dose of 200 to 400 kGy.
9. A crosslinked sulfonated poly(ether ether ketone) (SPEEK) cation exchange membrane prepared by the method of claim 1 .
10. A fuel cell membrane comprising the crosslinked SPEEK cation exchange membrane of claim 9 .
11. A water treatment membrane comprising the crosslinked SPEEK cation exchange membrane of claim 9 .