Method for determining sulfur content in fibers

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,086,382
App. No.
14/371,794
Granted
Jul 21, 2015
Kind
B2
Abstract

The invention concerns methods for measuring sulfur content in a fiber or polymer resin sample comprising: a) contacting the sample with a solution comprising sodium hydroxide to convert sulfur to sodium sulfate, b) combusting the sample of step a) in a furnace to remove essentially all organic materials to produce a residue; c) dissolving the residue in concentrated nitric acid; and d) determining the sulfur content of the sample using ICP Emission Spectrometry.

Claims (8)

1. A method of measuring sulfur content in a fiber or polymer resin sample comprising the following steps, in order:

a) contacting said sample with a solution comprising sodium hydroxide to convert said sulfur to sodium sulfate,

b) combusting the sample of step a) in a furnace to remove essentially all organic materials to produce a residue;

c) dissolving said residue of step b) in concentrated nitric acid; and

d) determining the sulfur content of the residue in concentrated nitric acid of step c) using Inductively Coupled Plasma (ICP) Emission Spectrometry to excite atoms and ions in the sample to emit electromagnetic radiation, and then comparing the intensity of emission using a sulfur emission line to that of samples of known concentration.

2. The method of claim 1 , where said solution comprising sodium hydroxide is an aqueous solution having a sodium hydroxide content in the range of from 0.01 to 1 N.

3. The method of claim 1 , wherein prior to step b), the fiber or polymer resin sample of step a) is heated to remove at least a portion residual liquid from said sample.

4. The method of claim 1 , wherein said fiber or polymer resin sample is soluble in concentrated sulfuric acid.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 25, 2019
From: E. I. DU PONT DE NEMOURS AND COMPANY
To: DUPONT SAFETY & CONSTRUCTION, INC.
Reel/Frame 049585/0450 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 5, 2015
From: TSCHRITTER, JONATHAN SAMUEL
To: E. I. DU PONT DE NEMOURS AND COMPANY
Reel/Frame 034633/0506 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 22, 2014
From: TSCHRITTER, JONATHAN SAMUEL
To: E. I. DUPONT DE NEMOURS AND COMPANY
Reel/Frame 033364/0293 →