IP Library Patent Application 14382725
Patent Application
App. No. 14/382,725

METHOD FOR MARKING COMPONENTS EMPLOYING OVERLAPPING AND SUBSEQUENTLY BARELY OVERLAPPING LASER PULSES

Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US None
App. No.
14/382,725
Abstract

A method for marking components ( 2 ) by a plurality of pulses ( 4 ) of a pulsed beam of a laser is disclosed. At first, a melted burr is formed when the marking ( 2 ) is being created. Subsequently, the melted burr is removed, whereby the pulsed laser beam is moved over the melted burr at a second speed. The sequential pulses ( 4 ) hardly overlap or not at all.

Claims (10)

1 - 7 . (canceled)

8 . A method for marking components by a plurality of pulses of a pulsed beam of a laser directed at a surface of the component, the method comprising the following steps:

forming a melted burr at side edges of the marking when the marking is being created whereby, during the creation of the marking, the pulsed laser beam is moved relative to the component at a first speed, so that the pulses overlap; and

removing the melted burr, the pulsed laser beam being moved over the melted burr at a second speed so that the sequential pulses do not overlap or overlap insubstantially.

9 . The method as recited in claim 8 wherein, after the removal, edge areas of the marking are subsequently melted, the laser beam is defocused and, at the same time, guided over the side edges of the marking at a third speed.

10 . The method as recited in claim 9 wherein the third speed amounts to 400 mm/sec at a pulse frequency of 200,000 Hz.

11 . The method as recited in claim 8 wherein the second speed is 2500 mm/sec at a pulse frequency of 50,000 Hz.

12 . The method as recited in claim 8 wherein the melted burr is formed by material of the component not evaporating completely when the marking was made.

13 . The method as recited in claim 8 wherein the component is a roller bearing that is provided with the marking.

14 . The method as recited in claim 8 wherein the melted burrs of the marking of the roller bearing are removed in such a way that the surface of the roller bearing can still function as a sealing surface.

Assignments (3)
CORRECTIVE ASSIGNMENT TO CORRECT THE PROPERTY NUMBERS PREVIOUSLY RECORDED ON REEL 037732 FRAME 0347. ASSIGNOR(S) HEREBY CONFIRMS THE APP. NO. 14/553248 SHOULD BE APP. NO. 14/553258. Recorded Oct 11, 2016
From: SCHAEFFLER TECHNOLOGIES GMBH & CO. KG
To: SCHAEFFLER TECHNOLOGIES AG & CO. KG
Reel/Frame 040404/0530 →
CHANGE OF NAME Recorded Feb 5, 2016
From: SCHAEFFLER TECHNOLOGIES GMBH & CO. KG
To: SCHAEFFLER TECHNOLOGIES AG & CO. KG
Reel/Frame 037732/0347 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 18, 2014
From: GIESE, MARIO
To: SCHAEFFLER TECHNOLOGIES GMBH & CO. KG
Reel/Frame 033770/0027 →