IP Library Granted Patent US 9,574,251
Granted Patent B2
US 9,574,251 · App. 14/405,908 · Granted Feb 21, 2017

Method of producing sintered ore

Inventors: Yuji Iwami (Tokyo, JP); Tetsuya Yamamoto (Tokyo, JP); Koichi Nushiro (Tokyo, JP); Yohei Takigawa (Tokyo, JP)
Assignee: JFE Steel Corporation
C22B1/20C22B1/205
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,574,251
App. No.
14/405,908
Granted
Feb 21, 2017
Kind
B2
Abstract

A method of producing a sintered ore includes charging a sintering raw material containing a powder ore and a carbonaceous material onto a circulatory moving pallet to form a charged layer, igniting the carbonaceous material on a surface of the charged layer, introducing air above the charged layer containing a gaseous fuel diluted to not more than a lower limit of combustion concentration with wind boxes arranged below the pallet into the charged layer by suction, and combusting the gaseous fuel and the carbonaceous material in the charged layer, wherein more than 50% of a total supply of the gaseous fuel is supplied in a front ½ portion of a region supplying the gaseous fuel.

Claims (8)

1. A method of producing a sintered ore comprising:

charging a sintering raw material containing a powder ore and a carbonaceous material onto a circulatory moving pallet to form a charged layer,

igniting the carbonaceous material on a surface of the charged layer,

introducing air above the charged layer containing a gaseous fuel diluted to not more than a lower limit of combustion concentration with wind boxes arranged below the pallet into the charged layer by suction, and

combusting the gaseous fuel and the carbonaceous material in the charged layer, wherein the region supplying the gaseous fuel is a region wherein a high-temperature keeping time kept at not lower than 1200° C. but not higher than 1380° C. is less than 150 seconds when the area is sintered by combustion heat of only the carbonaceous material, and wherein more than 50% of a total supply of the gaseous fuel is supplied in a front ⅓ portion of a region supplying the gaseous fuel.

2. The method according to claim 1 , wherein the region supplying the gaseous fuel is not more than 40% of a machine length ranging from an ignition furnace to an ore removing portion.

3. The method according to claim 2 , wherein the concentration of the gaseous fuel contained in air introduced in the charged layer is not more than the lower limit of combustion concentration.

4. The method according to claim 1 , wherein the concentration of the gaseous fuel contained in air introduced in the charged layer is not more than the lower limit of combustion concentration.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 5, 2014
From: IWAMI, YUJI; YAMAMOTO, TETSUYA; NUSHIRO, KOICHI; TAKIGAWA, YOHEI