IP Library Granted Patent US 9,928,946
Granted Patent B2
US 9,928,946 · App. 14/425,075 · Granted Mar 27, 2018

Method for manufacturing a power cable and cable manufactured by means of such a method

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,928,946
App. No.
14/425,075
Granted
Mar 27, 2018
Kind
B2
Abstract

The invention relates to a method for manufacturing a cable, including, from the inside to the outside, a central electrical conductor ( 1 ), a first semiconductor screen ( 2 ), an intermediate electric insulator ( 3 ), a second semiconductor screen ( 4 ), a metal screen ( 5 ) and an outer sheath ( 6 ), the method comprising a step of extruding a composition comprising at least one polyolefin for forming at least one layer constituting the first semiconductor screen, the intermediate electric insulator or second semiconductor screen and a step of cross-linking said layer. According to the invention, the method comprises the step of injecting, into the composition, a liquid solution containing at least one peroxide and at least one so-called cross-linking coagent, during the manufacture of said layer. The invention likewise relates to a cable manufactured by means of such a method.

Claims (27)

1. A process for the manufacture of a cable for the transportation of electrical energy comprising at least, from the inside toward the outside, a central electrical conductor ( 1 ), a first semiconducting shield ( 2 ), an intermediate electrical insulator ( 3 ), a second semiconducting shield ( 4 ), a metal shield ( 5 ) and an external sheath ( 6 ), the process comprising a stage of extrusion of a composition comprising at least one polyolefin, in order to form at least one layer making up the first semiconducting shield, the intermediate electrical insulator or the second semiconducting shield, and a stage of crosslinking said layer, the process being characterized in that it comprises a stage of injecting, into the composition, a liquid solution which comprises at least one peroxide and at least one compound referred to as cocrosslinking agent during the manufacture of said layer, each different ingredients of the liquid solution being liquid and miscible with the other ingredients of the liquid solution or being solid and soluble with the other ingredients of the liquid solution,

wherein a polyethylene is chosen as polyolefin for the composition forming the layer and in addition the liquid solution is chosen so that the composition comprises between 0.01% and 1.2% by weight of peroxide, with respect to the polyethylene, and between 0.3% and 4% by weight of the cocrosslinking agent, with respect to the polyethylene, and

wherein the composition comprises a lower percentage by weight of peroxide, with respect to the polyolefin, than the percentage by weight of the cocrosslinking agent, with respect to the polyolefin.

2. The process as claimed in claim 1 , in which the liquid solution is chosen so that the composition comprises between 0.01% and 1% by weight of peroxide, with respect to the polyethylene.

3. The process as claimed in claim 1 , in which, for the manufacture of the layer forming the intermediate electrical insulator, the stage of injecting the liquid solution into the composition is carried out during the extrusion stage.

4. The process as claimed in claim 1 , in which, for the manufacture of the layer forming one of the two semiconducting shields, the stage of injecting the liquid solution into the composition is carried out before the extrusion stage.

5. The process as claimed in claim 1 , in which the cocrosslinking agent is a type-II cocrosslinking agent.

6. The process as claimed in claim 1 , in which the at least one peroxide is a nonaromatic peroxide.

7. The process as claimed in claim 1 , in which the at least one peroxide is an aromatic peroxide.

8. The process as claimed in claim 1 , comprising the stage of mixing at least one liquid antioxidant compound with a liquid peroxide, as the at least one peroxide, and a solid type-II cocrosslinking agent, as the cocrosslinking agent, in order to obtain the liquid solution.

9. The process as claimed in claim 1 , in which the polyolefin is a linear low density polyethylene.

10. The process as claimed in claim 1 , in which the liquid solution and/or the composition additionally comprises at least one “anti-scorching” compound.

11. The process as claimed in claim 1 , comprising the stages of:

Coextruding the intermediate electrical insulator, the first semiconducting shield and the second semiconducting shield in order to form a complex;

Crosslinking said complex;

Directly arranging the metal shield and the external sheath around the crosslinked complex without carrying out a degassing stage.

12. A cable for the transportation of electrical energy, comprising at least, from the inside toward the outside, a central electrical conductor, a first semiconducting shield, an intermediate electrical insulator, a second semiconducting shield, a metal shield and an external sheath, characterized in that the material of the intermediate electrical insulator and/or of the first semiconducting shield and/or of the second semiconducting shield comprises at least one polyolefin into which has been injected a liquid solution comprising at least one peroxide and at least one compound referred to as cocrosslinking agent, wherein each ingredient of the liquid solution is a liquid that is miscible with the other ingredients of the liquid solution or is a solid that is soluble with the other ingredients of the liquid solution,

wherein a polyethylene is chosen as polyolefin for the composition forming the layer and in addition the liquid solution is chosen so that the composition comprises between 0.01% and 1.2% by weight of peroxide, with respect to the polyethylene, and between 0.3% and 4% by weight of the cocrosslinking agent with respect to the polyethylene, and

wherein the composition comprises a lower percentage by weight of peroxide, with respect to the polyolefin, than the percentage by weight of the cocrosslinking agent with respect to the polyolefin.

13. The cable as claimed in claim 12 , arranged for the transportation of medium-voltage electrical energy.

14. The cable as claimed in claim 12 , arranged for the transportation of high-voltage electrical energy.

15. A process for the manufacture of a cable for the transportation of electrical energy comprising at least, from the inside toward the outside, a central electrical conductor ( 1 ), a first semiconducting shield ( 2 ), an intermediate electrical insulator ( 3 ), a second semiconducting shield ( 4 ), a metal shield ( 5 ) and an external sheath ( 6 ), the process comprising a stage of extrusion of a composition comprising at least one polyolefin, in order to form at least one layer making up the first semiconducting shield, the intermediate electrical insulator or the second semiconducting shield, and a stage of crosslinking said layer, the process being characterized in that it comprises a stage of injecting, into the composition, a liquid solution which comprises at least one peroxide and at least one compound referred to as cocrosslinking agent during the manufacture of said layer, wherein each ingredient of the liquid solution is a liquid that is miscible with the other ingredients of the liquid solution or is a solid that is soluble with the other ingredients of the liquid solution,

wherein the process further comprising the stages of:

coextruding the intermediate electrical insulator, the first semiconducting shield and the second semiconducting shield in order to form a complex;

crosslinking said complex;

directly arranging the metal shield and the external sheath around the crosslinked complex without carrying out a degassing stage,

wherein a polyethylene is chosen as polyolefin for the composition forming the layer and in addition the liquid solution is chosen so that the composition comprises between 0.01% and 1.2% by weight of peroxide, with respect to the polyethylene, and between 0.3% and 4% by weight of the cocrosslinking agent with respect to the polyethylene, and wherein the composition comprises a lower percentage by weight of peroxide, with respect to the polyolefin, than the percentage by weight of the cocrosslinking agent with respect to the polyolefin.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Jun 6, 2018
From: JPMORGAN CHASE BANK, N.A.
To: GENERAL CABLE TECHNOLOGIES CORPORATION; GENERAL CABLE INDUSTRIES, INC.
Reel/Frame 046307/0316 →
SECURITY INTEREST Recorded May 23, 2017
From: GENERAL CABLE TECHNOLOGIES CORPORATION; GENERAL CABLE INDUSTRIES, INC.
To: JPMORGAN CHASE BANK, N.A.
Reel/Frame 042554/0286 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 31, 2015
From: GARD, JEAN-CHRISTOPHE; DENIZET, ISABELLE; MAMMERI, MOHAMMED; POISSON, BERNARD; LESAGE, FREDDY; MAGNOL, JONATHAN
To: SILEC CABLE
Reel/Frame 037393/0004 →