Nonaqueous electrolyte secondary battery

Inventors: Masanori Maekawa (Tokushima, JP); Yasunobu Iwami (Tokushima, JP); Akira Kinoshita (Tokushima, JP)
Assignee: SANYO Electric Co., Ltd.
H01M4/623H01M4/62H01M4/625H01M10/0525Y02E60/122Y02T10/7011
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,640,798
App. No.
14/434,317
Granted
May 2, 2017
Kind
B2
Abstract

A nonaqueous electrolyte secondary battery according to one aspect of the present invention contains a dispersant in a positive electrode mixture layer. The content of a positive electrode active material in the positive electrode mixture layer is 97% by mass or more, and the content ratio of a conductive agent to a binder in the positive electrode mixture layer is 1.00-1.67. The binder is composed of a polyvinylidene fluoride which has a carboxyl group or a carboxyl group derivative as a terminal functional group.

Claims (8)

1. A nonaqueous electrolyte secondary battery comprising:

a positive electrode plate having a positive electrode mixture layer formed thereon, the positive electrode mixture layer containing a positive electrode active material which stores and releases a lithium ion, a conductive agent, a binder, and a dispersant,

a negative electrode plate having a negative electrode mixture layer formed thereon, the negative electrode mixture layer containing a negative electrode active material which stores and releases a lithium ion,

a nonaqueous electrolyte solution, and

a separator;

the dispersant being selected from the group consisting of methyl cellulose, hydroxyethyl methyl cellulose, hydroxypropyl methyl cellulose, and polyvinyl propanol, a content of the positive electrode active material in the positive electrode mixture layer being from 97% by mass or more to 98.25% by mass;

a content ratio of the conductive agent to the binder in the positive electrode mixture layer being 1.00-1.67; and

the binder being composed of a polyvinylidene fluoride having, as a terminal functional group, one selected from the group consisting of a carboxyl group and a carboxyl group derivative.

Assignments (2)
NUNC PRO TUNC ASSIGNMENT Recorded Aug 29, 2023
From: SANYO ELECTRIC CO., LTD.
To: PANASONIC ENERGY CO., LTD
Reel/Frame 064745/0391 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 24, 2015
From: MAEKAWA, MASANORI; IWAMI, YASUNOBU; KINOSHITA, AKIRA
To: SANYO ELECTRIC CO., LTD.
Reel/Frame 035485/0423 →
Priority Claims (1)
JP 2012-239290 · Oct 30, 2012 · national
Continuity (1)
Related Publication 20150270553A1 · Sep 24, 2015