IP Library Granted Patent US 9,337,488
Granted Patent B2
US 9,337,488 · App. 14/460,087 · Granted May 10, 2016

Method of manufacturing a multicomponent system lithium phosphate compound particle having an olivine structure

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,337,488
App. No.
14/460,087
Granted
May 10, 2016
Kind
B2
Abstract

A method of manufacturing a multicomponent lithium phosphate compound particle with an olivine structure of formula Li y M1 1-Z M2 Z PO 4 , M1 is Fe, Mn or Co; Y satisfies 0.9≦Y≦1.2; M2 is Mn, Co, Mg, Ti or Al; and Z satisfies 0<Z≦0.1, in which the M2 concentration is continuously lowered from a surface of the particle to a core portion of the particle. The method includes mixing a lithium M1 phosphate compound with an olivine structure of formula Li X M1PO 4 , M1 is Fe, Mn or Co, and X satisfies 0.9≦X≦1.2, and a precursor of a lithium M2 phosphate compound with an olivine structure of formula Li X M2PO 4 , M2 is Mn, Co, Mg, Ti or Al, and X satisfies 0.9≦X≦1.2, to form a mixture; and subjecting the mixture to heating in an inert atmosphere or a vacuum.

Claims (8)

1. A method of manufacturing a multicomponent system lithium phosphate compound particle having an olivine structure and represented by a formula of Li y M1 1-Z M2 Z PO 4 in which M1 is one metal element selected from the group consisting of Fe, Mn and Co; Y is a number satisfying a formula of 0.9≦Y≦1.2; M2 is at least one metal element selected from the group consisting of Mn, Co, Mg, Ti and Al; and Z is an number satisfying a formula of 0<Z≦0.1, in which a concentration of the metal element M2 contained in a surface of the particle is higher than the concentration of the metal element M2 contained in a core portion of the particle, and the concentration of the metal element M2 is continuously lowered from the surface of particle to the core portion of the particle; the method comprising:

mixing a lithium M1 phosphate compound having an olivine structure and represented by a formula of Li X M1PO 4 in which M1 is one metal element selected from the group consisting of Fe, Mn and Co, and X is an number satisfying a formula of 0.9≦X≦1.2, and a precursor of a lithium M2 phosphate compound having an olivine structure and represented by a formula of Li X M2PO 4 in which M2 is at least one metal element selected from the group consisting of Mn, Co, Mg, Ti and Al, and X is an number satisfying a formula of 0.9≦X≦1.2 to form a mixture; and

subjecting the mixture to a heat treatment in an inert atmosphere or in a vacuum.

2. The method according to claim 1 , wherein the precursor of the lithium M2 phosphate compound is a mixture of lithium phosphate and M2 phosphate, the mixture being satisfied stoichiometry of lithium M2 phosphate.

3. A method of manufacturing a composite particle of carbon and a multicomponent system lithium phosphate compound having an olivine structure and represented by a formula of Li y M1 1-Z M2 Z PO 4 in which M1 is one metal element selected from the group consisting of Fe, Mn and Co; Y is a number satisfying a formula of 0.9≦Y≦1.2; M2 is at least one metal element selected from the group consisting of Mn, Co, Mg, Ti and Al; and Z is an number satisfying a formula of 0<Z≦0.1, in which a concentration of the metal element M2 contained in a surface of the particle is higher than the concentration of the metal element M2 contained in core portion of the particle, and the concentration of the metal element M2 is continuously lowered from the surface of particle to the core portion of the particle; the method comprising:

mixing a lithium M1 phosphate compound having an olivine structure and represented by a formula of Li x M1PO 4 in which M1 is one metal element selected from the group consisting of Fe, Mn and Co and X is an number satisfying a formula of 0.9≦X≦1.2, a precursor of a lithium M2 phosphate compound having an olivine structure and represented by a formula of Li X M2PO 4 in which M2 is at least one metal element selected from the group consisting of Mn, Co, Mg, Ti and Al and X is an number satisfying a formula of 0.9≦X≦1.2, and carbon or a carbon source to form a mixture; and

subjecting the mixture to a heat treatment in an inert atmosphere or in a vacuum.

4. The method according to claim 3 , wherein the precursor of the lithium M2 phosphate compound is a mixture of lithium phosphate and M2 phosphate, the mixture being satisfied stoichiometry of lithium M2 phosphate.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 1, 2022
From: SUMITOMO OSAKA CEMENT CO., LTD.
To: SUMITOMO METAL MINING CO., LTD.
Reel/Frame 060069/0546 →
CHANGE OF NAME Recorded Feb 12, 2021
From: TOKYO METROPOLITAN UNIVERSITY
To: TOKYO METROPOLITAN PUBLIC UNIVERSITY CORPORATION
Reel/Frame 055291/0517 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 14, 2014
From: ABE, HIDETOSHI; SUZUKI, TOMONORI; EGURO, TAKASHI; KANAMURA, KIYOSHI; SAITO, MITSUMASA
To: THE FURUKAWA BATTERY CO., LTD.; TOKYO METROPOLITAN UNIVERSITY; SUMITOMO OSAKA CEMENT CO., LTD.
Reel/Frame 033540/0172 →