Bi-cell for secondary battery having improved stability and method of preparing the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,825,275
App. No.
14/467,542
Granted
Nov 21, 2017
Kind
B2
Abstract

Provided are a bi-cell for a secondary battery having improved stability which may reduce shrinkage of a separator, and a method of preparing the bi-cell. The bi-cell for a secondary battery having improved stability according to an exemplary embodiment of the present invention is characterized in that a cathode and an anode are alternatingly disposed in a state in which the cathode has one more layer than the anode or the anode has one more layer than the cathode, separators having a bigger size than the cathode and the anode and insulating the cathode and the anode are disposed between the cathode and the anode, and edges of an upper separator and edges of a lower separator, which face to each other having the cathode and the anode disposed therebetween, are attached to each other to form fused portions.

Claims (18)

1. A bi-cell for a secondary battery comprising:

a cathode and an anode are alternatingly disposed in a state in which the cathode has one more layer than the anode or the anode has one more layer than the cathode;

separators having a bigger size than the cathode and the anode and insulating the cathode and the anode are disposed between the cathode and the anode; and

edges of an upper separator and edges of a lower separator, which face to each other having the cathode or the anode disposed therebetween, are attached to each other to form fused portions contacting said cathode or anode disposed therebetween,

wherein binder layers are respectively formed on surfaces of the upper separator and the lower separator, and

the fused portions are formed by heating and pressing the edges of the upper separator and the edges of the lower separator while being in contact with each other.

2. The bi-cell for a secondary battery of claim 1 , wherein the fused portions are formed by applying a heat of 50° C. to 100° C. and a pressure of 10 gf/cm 2 to 20 gf/cm 2 to the edges of the upper separator and the edges of the lower separator.

3. The bi-cell for a secondary battery claim 2 , wherein the fused portions are formed by applying the heat and the pressure for 3 seconds to 5 seconds to the edges of the upper separator and the edges of the lower separator.

4. The bi-cell for a secondary battery of claim 1 , wherein the pressure applied to the edges of the upper separator and the edges of the lower separator to form the fused portions is lower than a pressure required to attach the cathode and the anode to the separators.

5. A method of preparing a bi-cell for a secondary battery, the method comprising:

alternatingly disposing a cathode and an anode to allow the cathode to have one more layer than the anode or the anode to have one more layer than the cathode, and disposing separators having a bigger size than the cathode and the anode between the cathode and the anode (S 10 ); and

forming fused portions by attaching edges of an upper separator and edges of a lower separator, which face to each other having the cathode or the anode disposed therebetween, to each other (S 20 ), the fused portions contacting said cathode or anode disposed therebetween,

wherein binder layers are respectively formed on surfaces of the upper separator and the lower separator, and

operation S 20 is performed by heating and pressing the edges of the upper separator and the edges of the lower separator while being in contact with each other.

6. The method of claim 5 , wherein operation S 20 is performed by applying a heat of 50° C. to 100° C. and a pressure of 10 gf/cm 2 to 20 gf/cm 2 to the edges of the upper separator and the edges of the lower separator.

7. The method of claim 6 , wherein operation S 20 is performed by applying the heat and the pressure for 3 seconds to 5 seconds to the edges of the upper separator and the edges of the lower separator.

8. The method of claim 5 , wherein the pressure applied to the edges of the upper separator and the edges of the lower separator to form the fused portions is lower than a pressure required to attach the cathode and the anode to the separators.

9. The method of claim 6 , wherein the pressure applied to the edges of the upper separator and the edges of the lower separator to form the fused portions is lower than a pressure required to attach the cathode and the anode to the separators.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2021
From: LG CHEM, LTD.
To: LG ENERGY SOLUTION, LTD.
Reel/Frame 058295/0068 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 9, 2014
From: KIM, JUNG HAN; KIM, MIN SU
To: LG CHEM, LTD.
Reel/Frame 033696/0289 →