IP Library Granted Patent US 9,647,211
Granted Patent B2
US 9,647,211 · App. 14/471,811 · Granted May 9, 2017

Method of manufacturing ink for forming functional layer and method of manufacturing organic EL element

Inventors: Shotaro Watanabe (Chino, JP); Yuta Okawa (Fujimi-machi, JP)
Assignee: SEIKO EPSON CORPORATION
H01L51/0007C09D11/30C09D11/50C09D11/52C09K11/06H01L51/5012H01L51/5056H01L51/5088
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,647,211
App. No.
14/471,811
Granted
May 9, 2017
Kind
B2
Abstract

A method of manufacturing an ink for forming a functional layer includes: dispersing a mixture in which a low molecular material and a high molecular material are mixed in a poor solvent; and dissolving the mixture by adding a good solvent to the poor solvent in which the mixture is dispersed, in which a volume ratio of the poor solvent is from 10% to 70% with respect to the total volume in which the good solvent is added to the poor solvent and the poor solvent and the good solvent can be mixed.

Claims (33)

1. A method of manufacturing an ink for forming a functional layer which is used when a functional layer having a luminescence function is formed, comprising:

dispersing a solid content of any of a first material having a molecular weight of 10,000 or less, a second material having a weight average molecular weight of 10,000 or more, or a mixture in which the first material and the second material are mixed, in a first solvent; and

dissolving the solid content by adding a second solvent to the first solvent in which the solid content is dispersed to form a mixture of the first solvent, the second solvent, and the solid content, the solid content having a higher solubility in the second solvent than in the first solvent;

wherein a volume ratio of the first solvent is from 10% to 70% with respect to a total volume of the mixture of the first solvent, the second solvent, and the solid content.

2. The method of manufacturing an ink for forming a functional layer according to claim 1 ,

wherein a boiling point of the first solvent is from 150° C. to 300° C. and a boiling point of the second solvent is from 250° C. to 300° C.

3. The method of manufacturing an ink for forming a functional layer according to claim 1 ,

wherein the first solvent is at least one of: a linear alkane-based solvent, an aliphatic alcohol-based solvent, an aliphatic ether-based solvent, and an aromatic hydrocarbon-based solvent, and

the second solvent is at least one of: 3-phenoxy toluene, 2-isopropyl naphthalene, dibenzyl ether, and isopropyl biphenyl.

4. The method of manufacturing an ink for forming a functional layer according to claim 1 ,

wherein the first solvent is at least one of: a linear alkane-based solvent and an aliphatic alcohol-based solvent, and

the second solvent is at least one of: 3-phenoxy toluene, 2-isopropyl naphthalene, dibenzyl ether, and isopropyl biphenyl.

5. The method of manufacturing an ink for forming a functional layer according to claim 1 ,

wherein the first solvent is at least one of: four kinds of linear alkane-based solvents (nonane, decane, undecane, and dodecane), five kinds of aliphatic alcohol-based solvents (hexanol, heptanol, octanol, nonyl alcohol, and decyl alcohol), fourteen kinds of aliphatic ether-based solvents (dipentyl ether, diethylene glycol dimethyl ether, diethylene glycol ethyl methyl ether, diethylene glycol isopropyl methyl ether, diethylene glycol diethyl ether, diethylene glycol butyl methyl ether, diethylene glycol dibutyl ether, dipropylene glycol dimethyl ether, dipropylene glycol methyl propyl ether, triethylene glycol dimethyl ether, triethylene glycol ethyl methyl ether, triethylene glycol butyl methyl ether, tripropylene glycol dimethyl ether, and tetraethylene glycol dimethyl ether), and eight kinds of aromatic hydrocarbon-based solvents (1,3-diisopropylbenzene, 1,4-diisopropylbenzene, triisopropylbenzene, pentylbenzene, hexylbenzene, heptylbenzene, octylbenzene, and nonylbenzene), and

the second solvent is at least one of: 3-phenoxy toluene, 2-isopropyl naphthalene, dibenzyl ether, and isopropyl biphenyl.

6. A method of manufacturing an organic EL element provided with a functional layer having a luminescence function between an anode and a cathode,

wherein the functional layer includes a hole injection layer, a hole transport layer, and a luminescence layer, laminated from the anode side in order, and

the method comprises forming at least one layer among the hole injection layer, the hole transport layer, and the luminescence layer using an ink for forming a functional layer manufactured using the method according to claim 1 .

7. A method of manufacturing an organic EL element provided with a functional layer having a luminescence function between an anode and a cathode,

wherein the functional layer includes a hole injection layer, a hole transport layer, and a luminescence layer, laminated from the anode side in order, and

the method comprises forming at least one layer among the hole injection layer, the hole transport layer, and the luminescence layer using an ink for forming a functional layer manufactured using the method according to claim 2 .

8. The method of manufacturing an organic EL element according to claim 6 ,

wherein, in the forming of the functional layer, the hole injection layer is formed using the ink for forming a functional layer.

9. The method of manufacturing an organic EL element according to claim 7 ,

wherein, in the forming of the functional layer, the hole injection layer is formed using the ink for forming a functional layer.

10. The method of manufacturing an organic EL element according to claim 6 ,

wherein, in the forming of the functional layer, the hole transport layer is formed using the ink for forming a functional layer.

11. The method of manufacturing an organic EL element according to claim 7 ,

wherein, in the forming of the functional layer, the hole transport layer is formed using the ink for forming a functional layer.

12. The method of manufacturing an organic EL element according to claim 6 ,

wherein, in the forming of the functional layer, the luminescence layer is formed using the ink for forming a functional layer.

13. The method of manufacturing an organic EL element according to claim 7 ,

wherein, in the forming of the functional layer, the luminescence layer is formed using the ink for forming a functional layer.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 2, 2026
From: SEIKO EPSON CORPORATION
To: SHIHENG CREATION LIMITED
Reel/Frame 074265/0049 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 28, 2014
From: WATANABE, SHOTARO; OKAWA, YUTA
To: SEIKO EPSON CORPORATION
Reel/Frame 033632/0453 →
Priority Claims (1)
JP 2013-181894 · Sep 3, 2013 · national
Continuity (1)
Related Publication 20150064828A1 · Mar 5, 2015