IP Library Granted Patent US 10,122,011
Granted Patent B2
US 10,122,011 · App. 14/485,976 · Granted Nov 6, 2018

Multi layered electrode and method of manufacturing the same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,122,011
App. No.
14/485,976
Granted
Nov 6, 2018
Kind
B2
Abstract

Disclosed are an electrode for secondary batteries including an electrode mixture coated on one surface or opposite surface of an electrode current collector, and a method of manufacturing the same. The electrode mixture includes an electrode mixture layer A, which is a portion close to a current collector, and an electrode mixture layer, which is a portion distant from a current collector. The electrode mixture layer A includes a mixture of two active materials, average diameters of which are different, and the electrode mixture layer B includes active materials, average diameters of which are the same.

Claims (24)

1. A lithium secondary battery comprising a cathode and an anode as electrodes, wherein each of the electrodes comprises an electrode mixture layer A close to the electrode current collector and an electrode mixture layer B distant from the electrode current collector, wherein the electrode mixture layer A comprises a mixture of two active materials having different average diameters and the electrode mixture layer B comprises active materials having the same average diameters,

wherein a ratio of the electrode mixture layer A to the electrode mixture layer B is 1:9 to 3:7, based on a total thickness of the electrode mixture layers,

wherein a thickness of the electrode mixture layer A is 5 to 35 μm,

wherein the cathode comprises a spinel-structure lithium nickel manganese composite oxide (LNMO) represented by Formula 2 below as cathode active materials,

wherein the anode comprises a lithium titanium oxide (LTO) represented by Formula 4 below as anode active materials:

Li x Ni y Mn 2−y O 4   (2)

wherein 0.9≤x≤1.2, and 0.4≤y≤0.5

Li a Ti b O 4   (4)

wherein 0.5≤a≤3 and 1≤b≤2.5.

2. The lithium secondary battery according to claim 1 , wherein the active materials of the electrode mixture layer A comprise a mixture of an active material having an average diameter of 1 to 10 μm and an active material having an average diameter of 3 to 30 μm.

3. The lithium secondary battery according to claim 1 , wherein the active materials of the electrode mixture layer B comprise active materials having an average diameter of 3 to 30 μm.

4. The lithium secondary battery according to claim 1 , wherein electrode density of the electrode mixture layer A is higher than electrode density of the electrode mixture layer B.

5. The lithium secondary battery according to claim 1 , wherein the lithium nickel manganese composite oxide of Formula 2 is LiNi 0.5 Mn 1.5 O 4 or LiNi 0.4 Mn 1.6 O 4 .

6. The lithium secondary battery according to claim 1 , wherein the lithium titanium oxide of Formula 4 is Li 1.33 Ti 1.67 O 4 or LiTi 2 O 4 .

7. The lithium secondary battery according to claim 1 as a unit battery.

8. A battery pack comprising the battery module according to claim 7 .

9. A device comprising the battery pack according to claim 8 .

10. The device according to claim 9 , wherein the device is an electric vehicle, a hybrid electric vehicle, a plug-in hybrid electric vehicle, or a system for storing power.

11. A method of manufacturing the lithium secondary battery of claim 1 ,

the method comprising:

(i) first coating an electrode mixture including a mixture of two active materials, average diameters of which are different, on the electrode current collector; and

(ii) second coating an electrode mixture including active materials, average diameters of which are the same, on the first coated electrode.

12. The method of manufacturing the lithium secondary battery of claim 11 further comprising a drying process after the first coating.

13. The method of manufacturing the lithium secondary battery of claim 11 further comprising drying and pressing processes after the second coating.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2021
From: LG CHEM, LTD.
To: LG ENERGY SOLUTION, LTD.
Reel/Frame 058295/0068 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 22, 2015
From: LEE, ILJOON; LEE, JAE HYUN; KIM, JIHYUN
To: LG CHEM, LTD.
Reel/Frame 036154/0165 →