IP Library Granted Patent US 9,623,601
Granted Patent B2
US 9,623,601 · App. 14/507,767 · Granted Apr 18, 2017

Method and apparatus for forming blow molded vessels

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,623,601
App. No.
14/507,767
Granted
Apr 18, 2017
Kind
B2
Abstract

Methods and apparatus for molding a vessel, such as a bottle, with a high quality sealing surface are described herein. In one embodiment, a stepped blow pin can be used to form the sealing surface of a bottle. A stepped blow pin can include a body with a distal end and a proximal end. The blow pin can include a first region that includes a first diameter and a first engagement surface. The blow pin can further include a second region that includes a second diameter. The second region can be positioned between the first region and the distal end. A transition section can be positioned between the first region and second region. The blow pin can also include a top surface position at the proximal end, and a bottom surface positioned at the distal end.

Claims (34)

1. A method of forming a vessel with a high quality sealing surface using a blow molding process, the method including:

providing a mold that comprises:

a first mold body comprising:

a first cavity;

a first molding surface; and

a first neck forming region; and

a second mold body comprising:

a second cavity;

a second molding surface; and

a second neck forming region;

providing a plastic material;

providing a pin that comprises:

a body with a distal end and a proximal end;

a channel passing through the pin from the distal end to the proximal end;

a first region with a first diameter, the first region including a first engagement surface;

a second region with a second diameter that is greater than the first diameter of the first region, where the second region is positioned between the first region and the distal end;

a first transition positioned between the first region and second region;

a top surface position at the proximal end; and

a bottom surface at the distal end;

positioning the plastic material within the mold;

inserting the pin into the plastic material, where the first engagement surface is positioned proximate to the first neck forming region and second neck forming region;

engaging the plastic material with the first molding surface and second molding surface;

cooling the mold to solidify the plastic material; and

remove the solidified plastic material from the mold.

2. The method of claim 1 , where the pin is a blow pin and the blow molding process is an extrusion blow molding process.

3. The method of claim 1 , where the pin is a core pin and the blow molding process includes an injection process.

4. The method of claim 1 wherein a portion of the first region with a first diameter is used to form a bottle sealing surface portion of an inner surface of the bottle neck that will engage with a cap sealing surface to seal the bottle assembly.

5. The method of claim 1 further comprising a second transition portion positioned between the second region and the distal end and a third transition portion between a lower region and the bottom surface of the blow pin.

6. The method of claim 5 wherein the first, the second and the third transition portion has a beveled or chamfered or sloped or slanted configuration.

7. The method of claim 1 wherein the difference in the diameters of the first region and the second region is between about 0.001 inches and about 0.030 inches.

8. The method of claim 1 wherein the difference in the diameters of the first region and the second region is between about 0.003 inches and 0.010 inches.

9. The method of claim 1 wherein the diameter of the first region of the blow pin that forms the bottle sealing surface is about 0.586 inches.

10. The method of claim 1 wherein the diameter of the second region of the blow pin that forms the bottle sealing surface is about 0.594 inches.

11. The method of claim 1 wherein the greater diameter of the second region relative to the first region creates a pinch point that blocks the flow of pressurized air between the blow pin and a parison during the blow molding.

Assignments (4)
PATENT SECURITY AGREEMENT Recorded Sep 21, 2021
From: HEARTLAND CONSUMER PRODUCTS LLC
To: CITY NATIONAL BANK, AS ADMINISTRATIVE AGENT
Reel/Frame 057554/0697 →
RELEASE OF SECURITY INTEREST Recorded May 3, 2021
From: COOPERATIEVE RABOBANK U.A.
To: HEARTLAND CONSUMER PRODUCTS LLC; TC HEARTLAND LLC
Reel/Frame 056113/0471 →
SECURITY INTEREST Recorded Dec 7, 2018
From: HEARTLAND CONSUMER PRODUCTS LLC; TC HEARTLAND LLC
To: COOPERATIEVE RABOBANK U.A., NEW YORK BRANCH, AS ADMINISTRATIVE AGENT
Reel/Frame 047712/0601 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 11, 2016
From: GELOV, TEODOR H.
To: HEARTLAND CONSUMER PRODUCTS, LLC
Reel/Frame 039409/0866 →