IP Library Granted Patent US 9,738,819
Granted Patent B2
US 9,738,819 · App. 14/563,193 · Granted Aug 22, 2017

Pressure-sensitive adhesive composition

Inventors: Han Na Chi (Daejeon, KR); No Ma Kim (Daejeon, KR); Jeong Ae Yoon (Daejeon, KR); Sung Soo Yoon (Daejeon, KR); Min Ki Lee (Daejeon, KR)
Assignee: LG Chem, Ltd.
C09J153/00C08F293/005C08K5/105C09J11/06C09J133/066G02B1/04G02B5/305C09J2201/606G02B5/3033G02F2202/28Y10T428/2848Y10T428/2891
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,738,819
App. No.
14/563,193
Granted
Aug 22, 2017
Kind
B2
Abstract

Provided are a pressure-sensitive adhesive composition, an optical member, a polarizing plate and a display device. The pressure-sensitive adhesive composition having physical properties required for an optical member using a particular block copolymer and an antioxidant or a photostabilizer, which forms a fine phase change region in a crosslinking structure, and particularly having excellent bending preventability and storage stability may be provided. Such a pressure-sensitive adhesive composition may be used for optical uses, for example, to laminate various optical members, or apply an optical member to a display device.

Claims (27)

1. A pressure-sensitive adhesive polarizing plate, comprising:

a polarizer; and

a pressure-sensitive adhesive layer formed on one or both surfaces of the polarizer, and including a pressure-sensitive adhesive composition which is crosslinked, wherein the pressure-sensitive adhesive composition prior to crosslinking comprises:

a block copolymer, which is a diblock copolymer including a first block having a glass transition temperature of 70 to 95° C. and a second block having a glass transition temperature of −55 to −45° C. and a crosslinkable functional group; and

an antioxidant,

wherein the first block has a polymerization unit of an alkyl methacrylate, and the second block has a polymerization unit of an alkyl acrylate and a crosslinkable monomer,

wherein the block copolymer includes 100 to 1,500 parts by weight of the second block with respect to 100 parts by weight of the first block, and

wherein the antioxidant is at least one selected from the group consisting of a phenol-based antioxidant and a thioether-based antioxidant,

wherein the antioxidant is included at 0.01 to 3 parts by weight with respect to 100 parts by weight of the block copolymer, and

wherein a viscosity change of the pressure-sensitive adhesive composition prior to crosslinking after being maintained at 60° C. for 30 days is 5% or less.

2. The pressure-sensitive adhesive polarizing plate of claim 1 , wherein a difference in glass transition temperature between the first and second blocks of the block copolymer is 80 to 150° C.

3. The pressure-sensitive adhesive polarizing plate of claim 1 , wherein the first block has a number average molecular weight of 3,000 to 200,000.

4. The pressure-sensitive adhesive polarizing plate of claim 1 , wherein the block copolymer has a number average molecular weight of 50,000 to 300,000.

5. The pressure-sensitive adhesive polarizing plate of claim 1 , wherein the block copolymer has a polydispersity index (Mw/Mn) of 1.0 to 3.0.

6. The pressure-sensitive adhesive polarizing plate of claim 1 , further comprising a multifunctional crosslinking agent.

7. A pressure-sensitive adhesive optical laminate, comprising:

an optical film; and

a pressure-sensitive adhesive layer formed on one or both surfaces of the optical film and including a pressure-sensitive adhesive composition, which is crosslinked, wherein the pressure-sensitive adhesive composition prior to crosslinking comprises:

a block copolymer, which is a diblock copolymer including a first block having a glass transition temperature of 70 to 95° C. and a second block having a glass transition temperature of −55 to −45° C. and a crosslinkable functional group; and

an antioxidant,

wherein the first block has a polymerization unit of an alkyl methacrylate, and the second block has a polymerization unit of an alkyl acrylate and a crosslinkable monomer,

wherein the block copolymer includes 100 to 1,500 parts by weight of the second block with respect to 100 parts by weight of the first block, and

wherein the antioxidant is at least one selected from the group consisting of a phenol-based antioxidant and a thioether-based antioxidant,

wherein the antioxidant is included at 0.01 to 3 parts by weight with respect to 100 parts by weight of the block copolymer, and

wherein a viscosity change of the pressure-sensitive adhesive composition prior to crosslinking after being maintained at 60° C. for 30 days is 5% or less.

8. A display device comprising the pressure-sensitive adhesive optical laminate of claim 7 .

9. A display device comprising the pressure-sensitive adhesive polarizing plate of claim 1 .

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 26, 2025
From: LG CHEM LTD.
To: SHANJIN OPTOELECTRONICS (SUZHOU) CO., LTD.
Reel/Frame 070629/0281 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 9, 2014
From: CHI, HAN NA; KIM, NO MA; YOON, JEONG AE; YOON, SUNG SOO; LEE, MIN KI
To: LG CHEM, LTD.
Reel/Frame 034439/0232 →
Priority Claims (1)
KR 10-2013-0070539 · Jun 19, 2013 · national
Continuity (2)
Continuation PCTKR2014005447 · Jun 19, 2014
Related Publication 20150086781A1 · Mar 26, 2015