Shape-correcting and rolling method and shape-correcting device for high-strength steel

Inventors: Gil-Ho Song (Gwangyang-si, KR); Jae-Woong Byun (Gwangyang-si, KR); Nam-Il Jo (Gwangyang-si, KR); Sang-Kug Je (Gwangyang-si, KR); Jae-Wook Bae (Gwangyang-si, KR)
Assignee: POSCO
B21B1/26B21B1/22B21B15/005B21B27/06C21D8/0242B21B2001/228B21B2027/086B21C47/02B21C47/16B21D1/02C21D8/0226
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,086,418
App. No.
14/647,439
Granted
Oct 2, 2018
Kind
B2
Abstract

There are provided a shape-correcting and rolling method and a shape-correcting device for effectively correcting the shape of high-strength steel. The shape-correcting and rolling method includes: transferring a hot-rolled coil to a pay-off reel after cooling the hot-rolled coil or directly through a hot rolling to skin pass mill direct transfer process; unwinding the coil from the pay-off reel; correcting a shape of a strip unwound from the coil by using a heat pipe roller; and rewinding the strip as a coil.

Claims (47)

1. A shape-correcting and rolling method for high-strength steel, comprising:

performing a hot rolling to skin pass mill direct transfer process by transferring a hot-rolled coil to a pay-off reel;

unwinding a strip from the coil of the pay-off reel;

correcting a shape of the strip by using at least a pair of heat pipe rollers; and

rewinding the strip as a coil,

wherein each of the heat pipe rollers comprises

a plurality of first heat pipes extending in a length direction of the heat pipe roller from an end to a center region of the heat pipe roller and

a plurality of second heat pipes extending from an opposite end to the center region,

the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the heat pipe roller, and

the plurality of first and the plurality of second heat pipes overlap each other only in the center region in the length direction of the heat pipe roller.

2. The shape-correcting and rolling method of claim 1 , wherein prior to the correcting of the shape of the strip, the method further comprises rolling the strip at a reduction ratio of 20% to 30%.

3. The shape-correcting and rolling method of claim 2 , wherein prior to the rolling of the strip, the method further comprises removing scale from surfaces of the strip by shot blasting.

4. The shape-correcting and rolling method of claim 1 , wherein in the correcting of the shape of the strip, the strip has a temperature equal to or higher than 150° C., but lower than a phase transformation temperature.

5. The shape-correcting and rolling method of claim 4 , further comprising warm-rolling the strip.

6. The shape-correcting and rolling method of claim 1 , wherein a heat insulating process is performed on the coil during the unwinding of the coil, so as to prevent cooling of the coil.

7. The shape-correcting and rolling method of claim 1 , wherein prior to the correcting of the shape of the strip, the method further comprises heating the strip so that the strip has a uniform temperature.

8. A shape-correcting and rolling method for high-strength steel, comprising:

performing a first transfer process by transferring a hot-rolled coil to a temperature adjusting unit;

cooling the coil while monitoring a temperature of the coil;

performing a second transfer process by transferring the coil cooled to a temperature of 150° C. or higher to a pay-off reel;

unwinding a strip from the coil of the pay-off reel;

correcting a shape of the strip by using a pair of heat rollers; and

rewinding the strip as a coil,

wherein each of the heat pipe rollers comprises

a plurality of first heat pipes extending in a length direction of the heat pipe roller from an end to a center region of the heat pipe roller and

a plurality of second heat pipes extending from an opposite end to the center region,

the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the heat pipe roller, and

the plurality of first and the plurality of second heat pipes overlap each other only in the center region in the length direction of the heat pipe roller.

9. The shape-correcting and rolling method of claim 2 , wherein the cooling of the coil comprises:

measuring the temperature of the coil; and

comparing the measured temperature of the coil with a predetermined temperature range so as to determine whether the measured temperature of the coil is within the predetermined temperature range.

10. The shape-correcting and rolling method of claim 9 , wherein the cooling of the coil is performed by placing the coil on a skid in a yard, and

a thermocouple disposed in the skid indirectly measures the temperature of the coil by measuring a temperature of the skid heated by the coil placed on the skid.

11. A shape-correcting device for high-strength steel, the shape-correcting device comprising:

a pay-off reel from which a coil is unwound;

a skin pass mill correcting a strip unwound from the coil of the pay-off reel; and

a coiler rewinding the strip after the strip passes through the skin pass mill,

wherein the skin pass mill comprises a work roll that is a heat pipe roller in which heat pipes are installed,

wherein the heat pipes comprise

a plurality of first heat pipes extending in a length direction of the work roll from an end to a center region of the work roll and

a plurality of second heat pipes extending from an opposite end to the center region,

the plurality of first and the plurality of second heat pipes are alternately arranged in a circumferential direction of the work roll, and

one of the plurality of the first heat pipes and one of the plurality of the second heat pipes overlap each other only in the center region in the length direction of the work roll.

12. The shape-correcting device of claim 11 , wherein the heat pipes are uniformly arranged in the circumferential direction of the work roll at a predetermined insertion depth.

13. The shape-correcting device of claim 11 , wherein a heating device is disposed between the pay-off reel and the skin pass mill so as to heat the strip to a temperature equal to or higher than 150° C. but lower than a phase transformation temperature.

14. The shape-correcting device of claim 11 , further comprising a shot blaster configured to shoot steel balls having a micrometer (μm) size toward the strip and a rolling mill disposed behind the shot blaster to roll the strip, wherein the shot blaster and the rolling mill are disposed between the pay-off reel and the skin pass mill.

15. The shape-correcting device of claim 11 , further comprising at least one additional pay-off reel and a heat insulation cover, wherein when one of the pay-off reels is operated, the heat insulation cover covers the remaining pay-off reel that is not operated and a coil disposed on the remaining pay-off reel.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 26, 2022
From: POSCO HOLDINGS INC.
To: POSCO CO., LTD
Reel/Frame 061777/0974 →
CHANGE OF NAME Recorded Sep 28, 2022
From: POSCO
To: POSCO HOLDINGS INC.
Reel/Frame 061562/0012 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 26, 2015
From: SONG, GIL-HO; BYUN, JAE-WOONG; JO, NAM-IL; JE, SANG-KUG; BAE, JAE-WOOK
To: POSCO
Reel/Frame 035715/0311 →
Priority Claims (1)
KR 10-2012-0150135 · Dec 21, 2012 · national
Continuity (1)
Related Publication 20150306645A1 · Oct 29, 2015