IP Library Granted Patent US 9,796,140
Granted Patent B2
US 9,796,140 · App. 14/748,135 · Granted Oct 24, 2017

Automated systems for composite part fabrication

Inventor: James Sherwood Page (Oakland, CA)
Assignee: Autodesk, Inc.
B29C67/0085B29C67/0055B29C67/0059B29C67/0081B29C70/06B29C70/30B33Y10/00B33Y30/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,796,140
App. No.
14/748,135
Granted
Oct 24, 2017
Kind
B2
Abstract

A method includes: providing a matrix material and a fiber material separate from the matrix material to a fused deposition modelling (FDM) three dimensional (3D) printer; and delivering the matrix material and the fiber material to a printing location of the FDM 3D printer while maintaining separation of the fiber material from the matrix material up to the printing location of the FDM 3D printer, wherein the delivering includes melting the matrix material and embedding the fiber material within the matrix material. Further, a system includes: a build platform; and two or more tools associated with the build platform; wherein the two or more tools are configured and arranged with respect to the build platform to add matrix material and fiber material in non-planar layers to build the object.

Claims (42)

1. A method comprising:

providing a matrix material and a fiber material separate from the matrix material to a fused deposition modelling (FDM) three dimensional (3D) printer; and

delivering the matrix material and the fiber material to a printing location of the FDM 3D printer while maintaining separation of the fiber material from the matrix material up to the printing location of the FDM 3D printer, wherein the delivering comprises melting the matrix material and embedding the fiber material within the matrix material; and

wherein the matrix material comprises a first polymer, the fiber material comprises a second polymer, and both the first polymer and the second polymer are formed from a same monomer, but the first polymer has a lower melting temperature than the second polymer.

2. The method of claim 1 , wherein the providing comprises feeding the first polymer and the second polymer together, the first polymer forming a hollow tube that surrounds but is separate from the second polymer, and the delivering comprises feeding the first and second polymers through a heated nozzle at a temperature that melts the first polymer but not the second polymer, the first polymer having a lower glass transition temperature than a glass transition temperature of the second polymer.

3. The method of claim 1 , wherein the delivering comprises:

delivering the matrix material with a first tool comprising a heated nozzle; and

delivering the fiber material with a second tool, separate from the first tool.

4. The method of claim 3 , wherein the second tool comprising a spool and a heated roller, and delivering the fiber material comprises:

re-melting previously delivered matrix material using the heated roller, and

pressing the fiber material into the re-melted matrix material using the heated roller.

5. The method of claim 1 , wherein the delivering comprises delivering the matrix material and the fiber material with a single tool.

6. The method of claim 1 , wherein the delivering comprises:

delivering a first layer of the matrix material;

delivering a layer of the fiber material over the first layer of the matrix material;

delivering a second layer of the matrix material over the layer of fiber material; and

compacting and bonding the first and second layers of matrix material and the layer of fiber material together using an iron tool.

7. A method comprising:

providing a matrix material and a fiber material separate from the matrix material to a fused deposition modelling (FDM) three dimensional (3D) printer; and

delivering the matrix material and the fiber material to a printing location of the FDM 3D printer while maintaining separation of the fiber material from the matrix material up to the printing location of the FDM 3D printer, wherein the delivering comprises melting the matrix material and embedding the fiber material within the matrix material;

wherein the delivering comprises delivering the matrix material and the fiber material with a single tool; and

wherein the single tool comprises a heated nozzle and a roller on a swivel system, and the delivering comprises:

delivering the matrix material with the heated nozzle; and

delivering the fiber with the roller on the swivel system.

8. The method of claim 7 , wherein the matrix material comprises a first polymer, the fiber material comprises a second polymer, and both the first polymer and the second polymer are formed from a same monomer, but the first polymer has a lower melting temperature than the second polymer.

9. A method comprising:

providing a matrix material and a fiber material separate from the matrix material to a fused deposition modelling (FDM) three dimensional (3D) printer; and

delivering the matrix material and the fiber material to a printing location of the FDM 3D printer while maintaining separation of the fiber material from the matrix material up to the printing location of the FDM 3D printer, wherein the delivering comprises melting the matrix material and embedding the fiber material within the matrix material; and

wherein the delivering comprises depositing one or more first material segments with at least one first locking portion and one or more second material segments with at least one second locking portion with the at least one second locking portion having a shape that is defined by a shape of the at least one first locking portion, whereby the at least one second locking portion forms an interlock with the at least one first locking portion, and wherein the first and second material segments each comprise a continuous material, and the interlocked first and second material segments form an object having comparable resistance to delamination or breakage in all directions.

10. The method of claim 9 , wherein the one or more first material segments form a first layer, the one or more second material segments form a second layer, and each of the first and second layers are non-planar.

11. The method of claim 10 , wherein each of the first and second layers are formed from the matrix material comprising a first polymer and the fiber material comprising a second polymer, and both the first polymer and the second polymer are formed from a same monomer, but the first polymer has a lower melting temperature than the second polymer.

12. The method of claim 11 , wherein the providing comprises feeding the first polymer and the second polymer together, the first polymer forming a hollow tube that surrounds but is separate from the second polymer, and the delivering comprises feeding the first and second polymers through a heated nozzle at a temperature that melts the first polymer but not the second polymer, the first polymer having a lower glass transition temperature than a glass transition temperature of the second polymer.

13. The method of claim 9 , wherein the delivering comprises:

delivering the matrix material with a first tool comprising a heated nozzle; and

delivering the fiber material with a second tool, separate from the first tool.

14. The method of claim 13 , wherein the second tool comprising a spool and a heated roller, and delivering the fiber material comprises:

re-melting previously delivered matrix material using the heated roller, and

pressing the fiber material into the re-melted matrix material using the heated roller.

15. The method of claim 9 , wherein the delivering comprises delivering the matrix material and the fiber material with a single tool.

16. The method of claim 15 , wherein the single tool comprises a heated nozzle and a roller on a swivel system, and the delivering comprises:

delivering the matrix material with the heated nozzle; and

delivering the fiber with the roller on the swivel system.

Assignments (3)
CHANGE OF ADDRESS FOR ASSIGNEE Recorded Aug 19, 2022
From: AUTODESK, INC.
To: AUTODESK, INC.
Reel/Frame 061572/0061 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 2, 2015
From: PAGE, JAMES SHERWOOD
To: TOPOLABS TECHNOLOGY, LLC
Reel/Frame 036234/0045 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 2, 2015
From: TOPOLABS TECHNOLOGY, LLC
To: AUTODESK, INC.
Reel/Frame 036234/0053 →
Continuity (4)
Continuation In Part 14745285 · Jun 19, 2015
Provisional Application 62016011 · Jun 23, 2014
Provisional Application 62014453 · Jun 19, 2014
Related Publication 20150367576A1 · Dec 24, 2015