IP Library Granted Patent US 9,991,519
Granted Patent B2
US 9,991,519 · App. 14/917,807 · Granted Jun 5, 2018

Electrolytic aluminum foil, production method therefor, current collector for electrical storage device, electrode for electrical storage device, and electrical storage device

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,991,519
App. No.
14/917,807
Granted
Jun 5, 2018
Kind
B2
Abstract

An object of the present invention is to provide an electrolytic aluminum foil having no significant difference in properties between one surface and the other surface thereof, and also a method for producing the same. Another object is to provide a current collector for an electrical storage device using the electrolytic aluminum foil, an electrode for an electrical storage device, and an electrical storage device. An electrolytic aluminum foil of the present invention as a means for achieving the object is characterized in that both surfaces of the foil have L* values of 86.00 or more in the L*a*b* color space (SCI method). The electrolytic aluminum foil of the present invention can be produced, for example, employing a method for producing an electrolytic aluminum foil, which comprises applying a current between a cathode drum partially immersed in a plating solution and an anode plate immersed in the plating solution to form an aluminum film on the surface of the cathode drum, and then separating, from the cathode drum, the aluminum film raised from the liquid surface by rotating the cathode drum, and in which the dew point of a treatment atmosphere at the time of the separation of the aluminum film from the cathode drum to give an electrolytic aluminum foil is controlled to be −50.0° C. or less.

Claims (9)

1. An electrolytic aluminum foil, characterized in that both surfaces of the foil have L* values of 86.00 or more in the L*a*b* color space (SCI method), and

characterized in that the difference in L* value between the surfaces is 9.00 or less.

2. The electrolytic aluminum foil according to claim 1 , characterized in that the electrolytic aluminum foil is produced by separating an aluminum film formed on the surface of a cathode drum by electrolysis in a plating solution from the cathode drum.

3. The electrolytic aluminum foil according to claim 2 , characterized in that the surface of the foil on the side that has been in contact with the plating solution has an a* value of 1.00 or less and a b* value of 5.00 or less in the L*a*b* color space (SCI method).

4. The electrolytic aluminum foil according to claim 2 , characterized in that the surface of the foil on the side that has been in contact with the cathode drum has a surface roughness Ra of 0.50 μm or more and an L* value of 87.00 to 90.00 in the L*a*b* color space (SCI method).

5. The electrolytic aluminum foil according to claim 2 , characterized in that the surface of the foil on the side that has been in contact with the cathode drum has an a* value of 1.00 or less and a b* value of 5.00 or less in the L*a*b* color space (SCI method).

6. A current collector for an electrical storage device, characterized by comprising the electrolytic aluminum foil according to claim 1 .

7. An electrode for an electrical storage device, characterized by comprising an electrode active material supported on the electrolytic aluminum foil according to claim 1 .

8. An electrical storage device, characterized by being configured using the electrode for an electrical storage device according to claim 7 .

Assignments (2)
CHANGE OF NAME Recorded Dec 27, 2023
From: HITACHI METALS, LTD.
To: PROTERIAL, LTD.
Reel/Frame 066130/0563 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 16, 2016
From: OKAMOTO, ATSUSHI; MATSUDA, JUNICHI
To: HITACHI METALS, LTD.
Reel/Frame 037993/0563 →