Bedding product including composite layer and method of manufacture
A composite layer for use in a bedding product such as a mattress and a method of manufacture are disclosed. The composite layer generally includes an extruded three dimensional fibrous layer and a foam material, e.g., polyurethane, latex or the like, disposed within the fibrous layer and occupying at least a portion of the free volume in the layer. Also disclosed are processes for manufacturing a foam-fiber composite.
1. A single foam-fiber composite layer consisting of:
an extruded three dimensional polymer fiber portion having constant length, width and height dimensions, wherein the extruded three dimensional polymer fiber portion has a bottom surface, a top surface, and peripheral edges extending between the top and bottom surfaces, the extruded three dimensional polymer fiber portion consisting of randomly oriented polymer fibers bonded at coupling points between adjacent fibers and having a free volume per unit area of the layer; and
a foam portion disposed on and in a portion of the bottom surface and the peripheral edges of the extruded three dimensional polymer fiber portion, wherein the foam portion extends into at least 10 percent of the extruded three dimensional polymer fiber portion to provide the single roam-fiber composite layer with a foam-only portion, a roam and fiber portion, and a fiber-only portion, wherein a bottom surface and peripheral edges of the single foam-fiber composite layer consists of the foam-only portion.
2. The single foam-fiber composite layer of claim 1 , wherein the extruded three dimensional polymer fiber portion is selected from the group consisting of polyesters, polyethylene, polypropylene, nylon, elastomers, copolymers and its derivatives, including monofilament or bicomponent filaments having different melting points.
3. The single foam-fiber composite layer of claim 1 , wherein the foam portion comprises a polyurethane foam, a latex foam; a polystyrene foam, polyethylene foam, a polypropylene foam, a polyether-polyurethane foam.
4. The single foam-fiber composite layer of claim 1 , wherein the foam portion is a viscoelastic foam.
5. The single foam-fiber composite layer of claim 1 , wherein the foam portion has a lower curing temperature than a melting temperature and/or a softening temperature of the polymer fibers.
6. The single foam-fiber composite layer of claim 1 , wherein the extruded three dimensional polymer fiber portion comprises multiple zones of the polymer fibers having different densities and/or indentation force deflection values.
7. The single foam-fiber composite layer of claim 1 , wherein the height dimension of the three dimensional polymer fibers ranges from 1 to 6 inches.
8. The single foam-fiber composite layer of claim 1 , wherein the extruded three dimensional polymer fiber portion has a density ranging from 1.5 to 6 pounds per cubic foot.
9. The single foam-fiber composite layer of claim 1 , wherein the extruded three dimensional polymer fiber portion has an indentation force deflection ranging from 5 to 25 pounds-force.
10. The single foam-fiber composite layer of claim 1 , wherein the extruded three dimensional polymer fiber portion is a polymer selected from the group consisting of polyester, polyethylene and polypropylene, and the foam is a latex foam.
11. A mattress comprising:
at least one single foam-fiber composite layer consisting of an extruded three dimensional polymer fiber portion having constant length, width and height dimensions, wherein the extruded three dimensional polymer fiber portion has a bottom surface, a top surface, and peripheral edges extending between the top and bottom surfaces, the extruded three dimensional polymer fiber portion consisting of randomly oriented polymer fibers bonded at coupling points between adjacent fibers and having a free volume per unit area of the layer; and
a foam portion disposed on and in a portion of the bottom surface and the peripheral edges of the extruded three dimensional polymer fiber portion, wherein the foam portion extends into at least 10 percent of the extruded three dimensional polymer fiber portion to provide the foam-fiber composite layer with a foam-only portion, a foam and fiber portion, and a fiber-only portion, wherein a bottom surface and peripheral edges of the at least one single foam-fiber composite layer consists of the foam-only portion.
12. The mattress of claim 11 , wherein the extruded three dimensional polymer fiber portion is selected from the group consisting of polyesters, polyethylene, polypropylene, nylon, elastomers, copolymers and its derivatives, including monofilament or bicomponent filaments having different melting points.
13. The mattress of claim 11 , wherein the foam portion comprises a polyurethane foam, a latex foam; a polystyrene foam, polyethylene foam, a polypropylene foam, a polyether-polyurethane foam.
14. The mattress of claim 11 , wherein the foam portion is a viscoelastic foam.
15. The mattress of claim 11 , wherein the foam portion has a lower curing temperature than a melting temperature and/or a softening temperature of the polymer fibers.
16. The mattress of claim 11 , wherein the extruded three dimensional polymer fiber portion comprises multiple zones of the polymer fibers having different densities and/or indentation force deflection values.
17. The mattress of claim 11 , wherein the height dimension of the three dimensional polymer fibers ranges from 1 to 6 inches.
18. The mattress of claim 11 , wherein the extruded three dimensional polymer fiber portion has a density ranging from 1.5 to 6 pounds per cubic foot.
19. The mattress of claim 11 , wherein the extruded three dimensional polymer fiber portion has an indentation force deflection ranging from 5 to 25 pounds-force.
20. The mattress of claim 11 , wherein the extruded three dimensional polymer fiber portion is a polymer selected from the group consisting of polyester, polyethylene and polypropylene, and the foam is a latex foam.