IP Library Granted Patent US 9,533,370
Granted Patent B2
US 9,533,370 · App. 15/036,967 · Granted Jan 3, 2017

Method for laser marking an anodized metal surface with a desired colour

Inventors: Horia Sorin Andrei (Berlin, DE); Paul Martin Harrison (Salisbury, GB)
Assignee: SPI Lasers UK Limited
B23K26/0063B23K26/0006B23K26/0622B23K26/0643B23K26/0648B23K26/082B41J3/413B41M5/262
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,533,370
App. No.
15/036,967
Granted
Jan 3, 2017
Kind
B2
Abstract

A method for laser marking an anodized metal surface ( 5 ) with a desired color, which method comprises: providing a laser ( 1 ) for emitting a laser beam ( 4 ) comprising laser pulses having a pulse energy, a pulse width, and a pulse repetition frequency; providing a scanner ( 2 ) comprising a first mirror ( 6 ) for scanning the laser beam in a first direction ( 8 ), and a second mirror ( 7 ) for scanning the laser beam in a second direction ( 9 ); providing a lens ( 3 ) for focussing the laser beam from the laser ( 2 ) onto the anodized metal surface ( 5 ) to form a spot ( 31 ) having a spot diameter and a pulse fluence; providing a controller ( 11 ) for controlling the scanner ( 2 ) with a control signal ( 12 ); marking a plurality of lines ( 15 ) separated by a hatch distance ( 19 ) on the anodized metal surface to form a desired mark ( 16 ) by scanning the scanner ( 2 ) while pulsing the laser ( 1 ); selecting a scan speed ( 16 ), the pulse repetition frequency, and the spot diameter such that the separation ( 18 ) between consecutive spots ( 31 ) during each scan of the scanner ( 2 ) is at least one quarter of the spot diameter; the method being characterized by: overwriting each line ( 15 ) more than once; the color being given by the spot to spot separation ( 18 ), hatch distance ( 19 ), the pulse fluence, the pulse width, and the number of times each line is written; and selecting the spot to spot separation ( 18 ), the hatch distance ( 19 ), the pulse fluence, the pulse width, and the number of times each line is written to form the desired color.

Claims (30)

1. A method for laser marking an anodized metal surface with a desired colour, which method comprises:

providing a laser for emitting a laser beam comprising laser pulses having a pulse energy, a pulse width, and a pulse repetition frequency;

providing a seamier comprising a first mirror for scanning the laser beam in a first direction, and a second mirror for scanning the laser beam in a second direction;

providing a lens for focussing the laser beam from the laser onto the anodized metal surface to form a spot having a spot diameter and a pulse fluence;

providing a controller for controlling the scanner with a control signal;

marking a plurality of lines separated by a hatch distance on the anodized metal surface to form a desired mark by scanning the scanner while pulsing the laser; and

selecting a scan speed, the pulse repetition frequency, and the spot diameter such that the separation between consecutive spots during each scan of the scanner is at least one quarter of the spot diameter;

the method being characterized by

overwriting each line more than once;

the colour being given by the spot to spot separation, the hatch distance, the pulse fluence, the pulse width, and the number of times each line is written; and

selecting the spot to spot separation, the hatch distance, the pulse fluence, the pulse width, and the number of times each line is written to form the desired colour.

2. A method according to claim 1 wherein the second mirror is characterised by a digital resolution, and the hatch distance corresponds to an integral multiple of the digital resolution.

3. A method according to claim 1 wherein the metal is a precipitation hardened aluminium alloy.

4. A method according to claim 1 wherein the metal has been glass bead blasted.

5. A method according to claim 1 wherein the metal has been hard anodized.

6. A method according to claim 1 wherein the anodization has a thickness between 5 μm and 25 μm.

7. A method according to claim 6 wherein the anodization has a thickness between 5 μm and 15 μm.

8. A method according to claim 1 wherein the anodization is clear.

9. A method according to claim 1 wherein the anodization is coloured.

10. A method according to claim 1 wherein the colour is gray or black with an L value no greater than 40.

11. A method according to claim 10 wherein the L value is no greater than 30.

12. A method according to claim 1 wherein the laser is a pulsed laser providing a laser beam having a pulse width greater than one hundred picoseconds.

13. A method according to claim 12 wherein the pulse width is greater than 1 nanosecond.

14. A method according to claim 1 wherein the scanner is accelerated prior to pulsing the laser.

15. A method according to claim 1 wherein the anodized metal surface is orientated to minimize the overall time taken to form the mark.

16. A method according to claim 1 wherein the scanning speed is at least 5 m/s.

17. A method according to claim 1 wherein the pulse repetition frequency is at least 500 kHz.

18. A method according to claim 1 wherein the scanning speed is at least 9 m/s, and the pulse repetition frequency is at least 900 kHz.

19. A method according to claim 1 wherein each line is overwritten at least 5 times.

20. A method according to claim 1 wherein the spot to spot separation is at least half the spot diameter.

Assignments (1)
CHANGE OF NAME Recorded Dec 1, 2024
From: SPI LASERS UK LIMITED
To: TRUMPF LASER UK LIMITED
Reel/Frame 069442/0478 →
Priority Claims (1)
GB 1321322.8 · Dec 3, 2013 · national
Continuity (1)
Related Publication 20160256955A1 · Sep 8, 2016