Method for producing seamless metal pipe

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,232,418
App. No.
15/125,699
Granted
Mar 19, 2019
Kind
B2
Abstract

A solid billet is piercing-rolled using a 4 roll-type inclined rolling mill including larger-diameter cone-type main rolls arranged horizontally or vertically to face each other across a pass line and smaller-diameter auxiliary rolls arranged vertically or horizontally to face each other similarly across the pass line between the facing main rolls, while maintaining a feed angle β and cross angle γ of the main rolls and a feed angle β′ and cross angle γ′ of the auxiliary rolls to be within the ranges: 5°≤“β, β′”≤25°; 3°≤“γ, γ′”≤35°; and 10°≤“β+γ, β′+γ′”≤55°.

Claims (16)

1. A method for producing a seamless metal pipe, the method comprising:

piercing-rolling a solid billet using a 4 roll inclined rolling mill that includes a pair of cone-shaped main rolls having roll shafts supported at opposing ends thereof and arranged horizontally or vertically to face each other across a pass line and a pair of cone-shaped auxiliary rolls having roll shafts supported at opposing ends thereof and arranged vertically or horizontally to face each other similarly across the pass line between the facing main rolls, wherein the diameter of the main rolls is larger than the diameter of the auxiliary rolls; and

maintaining a feed angle β of the cone-shaped main rolls, a cross angle γ of the main rolls, a feed angle β′ of the auxiliary rolls, and a cross angle γ′ of the auxiliary rolls to be within following ranges:

5°≤β, β′≤25°;

3°≤γ, γ′≤35°;

and

10°≤β+γ, β′+γ′≤55°.

2. The method for producing a seamless metal pipe according to claim 1 , wherein the step of piercing-rolling the solid billet is expanding-piercing-rolling the solid billet so that a diameter d 0 of the solid billet, a diameter d of a hollow piece after the expanding-piercing-rolling, and a wall thickness t of the hollow piece together satisfy a following relationship:

1.5≤−Ψ r /Ψ θ ≤4.5

where Ψ r =ln(2t/d 0 )Ψ θ =ln {2(d−t)/d 0 }.

3. The method for producing a seamless metal pipe according to claim 2 , wherein the piercing-rolling is performed so that an inlet diameter D 1 , an outlet diameter D 2 , and a roll cross angle γ of the cone-shaped main rolls and also an inlet diameter D 1 ′, an outlet diameter D 2 ′, and a roll cross angle γ′ of the cone-shaped auxiliary rolls satisfy relationships with the diameter d 0 of the solid billet and the diameter d of the hollow piece after the piercing as follows:

( d/d 0 )/( D 2 /D 1 )<0.75+0.025γ;

and

( d/d 0 )/( D 2 ′/D 1 ′)<0.75+0.025γ′.

4. The method for producing a seamless metal pipe according to claim 2 , wherein the solid billet is piercing-rolled as the main rolls are being driven while the auxiliary rolls are left undriven.

5. The method for producing a seamless metal pipe according to claim 1 , wherein the solid billet is piercing-rolled as the main rolls are being driven while the auxiliary rolls are left undriven.

Assignments (2)
CHANGE OF NAME Recorded May 14, 2019
From: NIPPON STEEL & SUMITOMO METAL CORPORATION
To: NIPPON STEEL CORPORATION
Reel/Frame 049257/0828 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 13, 2016
From: HAYASHI, CHIHIRO
To: NIPPON STEEL & SUMITOMO METAL CORPORATION
Reel/Frame 039717/0731 →