IP Library Granted Patent US 9,896,915
Granted Patent B2
US 9,896,915 · App. 15/137,892 · Granted Feb 20, 2018

Outer tube for a perforating gun

Inventors: Jozef Balun (Paderborn, DE); Waldemar Engel (Paderborn, DE)
Assignee: Benteler Steel/Tube GmbH
E21B43/116F42D1/00
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,896,915
App. No.
15/137,892
Granted
Feb 20, 2018
Kind
B2
Abstract

An outer tube for a perforating gun is provided that includes an inner wall and an outer wall and also a wall thickness (D) and a length (L), wherein the outer tube has a hardness over its entire longitudinal extent along the length (L) and its transverse extent along the wall thickness (D), wherein the hardness of the outer tube is reduced, in at least one region, to an extent (T) measured from the outer wall to the inner wall, wherein, in this region, the outer tube has a reduced hardness (HV) on its outer wall, said reduced hardness being reduced in this region by at least 5% in relation to the hardness (H) of the inner wall.

Claims (30)

1. An outer tube for a perforating gun, comprising:

an inner wall and an outer wall and also a wall thickness and a length,

a reduced hardness in at least one region of the outer wall, said reduced hardness extending into the wall thickness by an extent measured from the outer wall to the inner wall, said reduced hardness is at least 5% less than a hardness of the inner wall, and

wherein the at least one region having the reduced hardness is established by a deep decarburization such that the hardness across the wall thickness in the at least one region having reduced hardness decreases continuously from the inner wall to the outer wall.

2. The outer tube as claimed in claim 1 , comprising a metal.

3. The outer tube as claimed in claim 2 , comprising at least one of a steel and a steel alloy.

4. The outer tube as claimed in claim 1 , wherein the extent measured from the outer wall to the inner wall is at least 200 μm and at most 50% of the wall thickness.

5. The outer tube as claimed in claim 4 , wherein the reduced hardness of the outer wall is at least 10% less than the hardness of the inner wall.

6. The outer tube as claimed in claim 4 , further comprising a 0.2% offset yield strength R p,0.2 of at least 700 MPa.

7. The outer tube as claimed in claim 4 , wherein the at least one region having the reduced hardness is only local and is enclosed all the way around a circumference thereof by regions of the outer wall with a hardness greater than the reduced hardness.

8. The outer tube as claimed in claim 4 , further comprising:

a multiplicity of depressions which extend radially from the outer wall in a direction of the inner wall.

9. The outer tube as claimed in claim 1 , wherein the reduced hardness of the outer wall is at least 10% less than the hardness of the inner wall.

10. The outer tube as claimed in claim 9 , further comprising a 0.2% offset yield strength R p,0.2 of at least 700 MPa.

11. The outer tube as claimed in claim 9 , wherein the at least one region having the reduced hardness is only local and is enclosed all the way around a circumference thereof by regions of the outer wall with a hardness greater than the reduced hardness.

12. The outer tube as claimed in claim 9 , further comprising:

a multiplicity of depressions which extend radially from the outer wall in a direction of the inner wall.

13. The outer tube as claimed in claim 1 , further comprising a 0.2% offset yield strength R p,0.2 of at least 700 MPa.

14. The outer tube as claimed in claim 13 , wherein the at least one region having the reduced hardness is only local and is enclosed all the way around a circumference thereof by regions of the outer wall with a hardness greater than the reduced hardness.

15. The outer tube as claimed in claim 1 , wherein the at least one region having the reduced hardness is only local and is enclosed all the way around a circumference thereof by regions of the outer wall with a hardness greater than the reduced hardness.

16. The outer tube as claimed in claim 1 , further comprising:

a multiplicity of depressions which extend radially from the outer wall in a direction of the inner wall.

17. The outer tube as claimed in claim 16 , wherein the at least one region having the reduced hardness is arranged outside the depressions.

18. The outer tube as claimed in claim 16 , wherein the reduced hardness of a region is offset from a depression in a circumferential direction about a longitudinal axis of the outer wall.

19. The outer tube as claimed in claim 18 , wherein the offset is between 60° and 120° about the longitudinal axis of the outer wall.

20. A perforating gun having an outer tube as claimed in claim 1 serving as a tubular housing, comprising:

an inner part, which is arranged in the outer tube; and

holders carrying explosive charges.

21. The outer tube as claimed in claim 1 , further comprising:

a non-reduced hardness in at least one region of the outer wall, said non-reduced hardness extending through the entire wall thickness such that said non-reduced hardness is substantially the same as the hardness of the inner wall.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 7, 2016
From: BALUN, JOZEF; ENGEL, WALDEMAR
To: BENTELER STEEL/TUBE GMBH
Reel/Frame 038828/0173 →
Continuity (1)
Related Publication 20170306728A1 · Oct 26, 2017