Protection of the color of textile fibers by means of cationic polysacchrides

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,273,434
App. No.
15/227,124
Granted
Apr 30, 2019
Kind
B2
Abstract

The present invention relates to the use of a cationic polysaccharide in a detergent composition used for treating dyed textile fibers in an aqueous medium, in order to reduce the loss of color of the dyed fibers when treating same using said detergent composition.

Claims (5)

1. A method of reducing color loss from dyed cotton textile fibers after 3, 5 or 10 washing cycles, which fibers are based on cotton fibers dyed by pigments, comprising treating the textile fibers in an aqueous medium with a laundry product comprising 1% by weight of the laundry product of a cationic guar, wherein said cationic guar has an average molecular weight ranging from 300,000 to 500,000 g/mol and a degree of cationic substitution ranging from 0.08 to 0.11, and wherein the cationic guar comprises guar hydroxypropyltrimonium chloride.

2. The method of claim 1 , wherein the cationic guar has a degree of cationic substitution ranging from 0.09 to 0.11.

3. The method of claim 1 , wherein the concentration of the cationic guar in the aqueous medium ranges from 0.005 to 1 g/L.

4. The method of claim 1 , wherein the laundry product comprises a detergent composition adapted for machine washing, optionally comprising a washing additive.

5. A method of making a laundry product comprising adding a cationic guar to the laundry product, wherein the laundry product reduces color loss from a dyed cotton textile fiber when said dyed cotton textile fiber is treated with the laundry product in an aqueous medium after 3, 5 or 10 washing cycles and wherein the cationic guar is added to said laundry product in an amount of 1% by weight, relative to the weight of the laundry product, wherein said cationic guar has an average molecular weight ranging from 300,000 to 500,000 g/mol and a degree of cationic substitution ranging from 0.08 to 0.11, and wherein the cationic guar comprises guar hydroxypropyltrimonium chloride.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 26, 2024
From: RHODIA OPERATIONS
To: SPECIALTY OPERATIONS FRANCE
Reel/Frame 066374/0642 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 7, 2023
From: RHODIA OPERATIONS
To: SPECIALTY OPERATIONS FRANCE
Reel/Frame 065488/0365 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 26, 2016
From: LAMBERT, FLORENCE; ORIZET, CELINE
To: RHODIA OPERATIONS
Reel/Frame 039552/0390 →