Neutral aqueous wax emulsions
Wax emulsions for the manufacture of wallboard include water; a lignosulfonic acid or a salt thereof; and at least one wax selected from the group consisting of slack wax, paraffin wax and montan wax. The emulsions may have a pH of between about 6.5 and 7.9. Such emulsions can provide enhanced moisture resistance to the wallboard.
1. A method for manufacturing wallboard, the method comprising:
providing a wax emulsion comprising water, a lignosulfonic acid or a salt thereof, a stabilizer consisting essentially of an ethylene-vinly alcohol-vinyl acetate terpolymer, and at least one wax selected from the group consisting of slack wax, and paraffin wax, the wax emulsion comprising a pH of between about 6.5 and 7.9;
providing an aqueous slurry of a gypsum slurry; and
mixing the wax emulsion and the gypsum slurry to form a mixture.
2. The method of claim 1 , further comprising applying the mixture to a first sheet of wallboard facer.
3. The method of claim 1 , further comprising disposing a second sheet of wallboard facer on top of the mixture, so that the first and second sheets are in opposed facing relationship and have a layer of the mixture therebetween.
4. The method of claim 1 , further comprising performing press-in-place molding to the mixture.
5. The method of claim 1 , wherein the wax emulsion does not comprise an added base.