IP Library Granted Patent US 10,128,529
Granted Patent B2
US 10,128,529 · App. 15/346,932 · Granted Nov 13, 2018

Lithium-ion secondary battery, fabricating method therof, and electronic device

Inventors: Ai Nakagawa (Kanagawa, JP); Teppei Oguni (Kanagawa, JP); Kai Kimura (Kanagawa, JP); Rika Yatabe (Kanagawa, JP)
Assignee: Semiconductor Energy Laboratory Co., Ltd.
H01M10/0525G01R31/36G01R31/44H01M4/133H01M4/136H01M4/366H01M4/587H01M4/5825H01M4/62H01M4/626H01M4/661H01M10/0422H01M10/058H01M10/0567H01M10/0568H01M10/0569H02J7/0014H01M10/0463H01M10/425H01M2010/4271H01M2220/30H01M2300/0025H01M2300/0037
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,128,529
App. No.
15/346,932
Granted
Nov 13, 2018
Kind
B2
Abstract

A lithium-ion secondary battery with a high capacity retention rate is provided. In addition, a fabricating method of a lithium-ion secondary battery with a high capacity retention rate is provided. The lithium-ion secondary battery includes a positive electrode, a negative electrode, and an electrolyte solution. The negative electrode includes a negative electrode active material layer. The electrolyte solution includes at least one of lithium bis(trifluoromethanesulfonyl)amide (LiTFSA) and lithium bis(fluorosulfonyl)amide (LiFSA). The electrolyte solution includes vinylene carbonate (VC). A coating film including lithium oxide is on a surface of the negative electrode active material layer. A fabricating method of a lithium-ion secondary battery includes a first step of enclosing a positive electrode, a negative electrode, and an electrolyte solution in an exterior body, and a second step of annealing the exterior body enclosing the positive electrode, the negative electrode, and the electrolyte solution for 24 hours or longer after the first step. The annealing in the second step is performed at a temperature higher than or equal to 80° C. and lower than or equal to 100° C.

Claims (64)

1. A lithium-ion secondary battery comprising:

a positive electrode;

a negative electrode; and

an electrolyte solution,

wherein the negative electrode comprises a negative electrode active material layer,

wherein the electrolyte solution comprises at least one of lithium bis(trifluoromethanesulfonyl)amide and lithium bis(fluorosulfonyl)amide and comprises vinylene carbonate,

wherein a coating film is on a surface of the negative electrode active material layer,

wherein the coating film comprises lithium oxide, lithium hydroxide, lithium carbonate, and lithium fluoride, and

wherein a proportion of lithium oxide in the coating film is greater than or equal to 4% and less than or equal to 20%.

2. The lithium-ion secondary battery according to claim 1 ,

wherein the negative electrode further comprises a negative electrode current collector,

wherein the negative electrode current collector comprises copper, and

wherein the negative electrode active material layer comprises graphite particles.

3. The lithium-ion secondary battery according to claim 1 ,

wherein the electrolyte solution further comprises ethylene carbonate and diethyl carbonate.

4. The lithium-ion secondary battery according to claim 1 ,

wherein a capacity retention rate of the lithium-ion secondary battery as a function of the square root of the number of cycles can be represented as a straight line having a slope less than or equal to −0.21, and

wherein the lithium-ion secondary battery has been submitted to an annealing performed at a temperature higher than or equal to 60° C.

5. An electronic device comprising:

the lithium-ion secondary battery according to claim 1 ;

a switch; and

a display portion.

6. A lithium-ion secondary battery comprising:

a positive electrode;

a negative electrode; and

an electrolyte solution,

wherein the positive electrode comprises a positive electrode current collector and a positive electrode active material layer,

wherein the positive electrode current collector comprises aluminum,

wherein the positive electrode active material layer comprises a graphene compound or lithium iron phosphate,

wherein the negative electrode comprises a negative electrode active material layer,

wherein the electrolyte solution comprises at least one of lithium bis(trifluoromethanesulfonyl)amide and lithium bis(fluorosulfonyl)amide and comprises vinylene carbonate,

wherein a coating film is on a surface of the negative electrode active material layer,

wherein the coating film comprises lithium oxide, lithium hydroxide, lithium carbonate, and lithium fluoride, and

wherein a proportion of lithium oxide in the coating film is greater than or equal to 4% and less than or equal to 20%.

7. The lithium-ion secondary battery according to claim 6 ,

wherein the negative electrode further comprises a negative electrode current collector,

wherein the negative electrode current collector comprises copper, and

wherein the negative electrode active material layer comprises graphite particles.

8. The lithium-ion secondary battery according to claim 6 ,

wherein the electrolyte solution further comprises ethylene carbonate and diethyl carbonate.

9. The lithium-ion secondary battery according to claim 6 ,

wherein a capacity retention rate of the lithium-ion secondary battery as a function of the square root of the number of cycles can be represented as a straight line having a slope less than or equal to −0.21, and

wherein the lithium-ion secondary battery has been submitted to an annealing performed at a temperature higher than or equal to 60° C.

10. An electronic device comprising:

the lithium-ion secondary battery according to claim 6 ;

a switch; and

a display portion.

11. A fabricating method of a lithium-ion secondary battery comprising:

a first step of enclosing a negative electrode comprising a negative electrode active material layer, a positive electrode, and an electrolyte solution in an exterior body; and

a second step of annealing the exterior body enclosing the positive electrode, the negative electrode, and the electrolyte solution for 24 hours or longer after the first step,

wherein the annealing in the second step is performed at a temperature higher than or equal to 80° C. and lower than or equal to 100° C.,

wherein the electrolyte solution comprises at least one of lithium bis(trifluoromethanesulfonyl)amide and lithium bis(fluorosulfonyl)amide and comprises vinylene carbonate,

wherein the positive electrode comprises a positive electrode current collector comprising aluminum,

wherein the positive electrode comprises a positive electrode active material layer comprising a graphene compound, and

wherein a coating film is on a surface of the negative electrode active material layer.

12. The fabricating method of a lithium-ion secondary battery, according to claim 11 ,

wherein the negative electrode comprises a negative electrode current collector comprising copper, and

wherein the negative electrode active material layer comprises graphite particles.

13. The fabricating method of a lithium-ion secondary battery, according to claim 11 ,

wherein the coating film changes in quality in the second step.

14. The fabricating method of a lithium-ion secondary battery, according to claim 11 , further comprising a third step of connecting the positive electrode and the negative electrode to a device and performing charging and discharging,

wherein the third step is performed between the first step and the second step, and

wherein the coating film is formed in the third step.

15. The fabricating method of a lithium-ion secondary battery, according to claim 11 , wherein the coating film comprises lithium oxide, lithium hydroxide, lithium carbonate, and lithium fluoride.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 9, 2016
From: NAKAGAWA, AI; OGUNI, TEPPEI; KIMURA, KAI; YATABE, RIKA
To: SEMICONDUCTOR ENERGY LABORATORY CO., LTD.
Reel/Frame 040270/0555 →
Priority Claims (1)
JP 2015-222748 · Nov 13, 2015 · national
Continuity (1)
Related Publication 20170141428A1 · May 18, 2017