IP Library Granted Patent US 10,216,089
Granted Patent B2
US 10,216,089 · App. 15/352,666 · Granted Feb 26, 2019

Methods of forming flexographic printing members

Inventors: Richard R. Ollmann, Jr. (Woodbury, MN); Elsie Anderson Fohrenkamm (St. Paul, MN); Fredrick Charles Mellema (Oakdale, MN)
Assignee: EASTMAN KODAK COMPANY
G03F7/32G03F7/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,216,089
App. No.
15/352,666
Granted
Feb 26, 2019
Kind
B2
Abstract

Flexographic printing members are prepared by developing an exposed flexographic printing member precursor with an aqueous flexographic developer. The aqueous flexographic developer comprises: a) a fatty acid composition consisting of one or more saturated or unsaturated fatty acids or alkali metal salts thereof, each saturated or unsaturated fatty acid or alkali metal salt thereof independently having 12 to 20 carbon atoms, the fatty acid composition being present in an amount of 0.25-2.0 weight %, and at least 85 weight % of the fatty acid composition is composed of one or more C 18 mono- or poly-unsaturated fatty acids or alkali metal salts thereof; b) an aminopolycarboxylic acid or alkali metal salt thereof in an amount of 0.05-0.30 weight %; c) a buffer compound in an amount of 05-0.60 weight %; and d) water. Such aqueous flexographic developers can also be provided in concentrated form and appropriately diluted before or during use.

Claims (57)

1. A method for providing a flexographic printing member, comprising:

developing an imagewise exposed flexographic printing member precursor with an aqueous flexographic developer to provide a relief image in a flexographic printing plate,

wherein the aqueous flexographic developer comprises:

a) a fatty acid composition consisting of one or more saturated or unsaturated fatty acids or alkali metal salts thereof, each saturated or unsaturated fatty acid or alkali metal salt thereof independently having 12 to 20 carbon atoms, the fatty acid composition being present in an amount of at least 0.25 weight % and up to and including 2.0 weight %,

wherein at least 85 weight % of the fatty acid composition is composed of one or more C 18 mono- or poly-unsaturated fatty acids or alkali metal salts thereof;

b) one or more aminopolycarboxylic acids or alkali metal salts thereof in an amount of at least 0.05 weight % and up to and including 0.30 weight %;

c) a buffer compound in an amount of at least 0.05 weight % and up to and including 0.60 weight %; and

d) water in an amount of at least 97 weight % and up to and including 99.5 weight %;

all amounts being based on the total weight of the aqueous flexographic developer; and

replenishing the aqueous flexographic developer with a replenisher developer composition having the same or a greater concentration of one or more of components a) through c).

2. The method of claim 1 , wherein the aqueous flexographic developer has a pH of at least 9.5 and up to and including 11.5.

3. The method of claim 1 , wherein the fatty acid composition consists essentially of oleic acid or an alkali metal salt thereof in an amount of at least 85 weight % and up to and including 100 weight %, based on the total weight of the fatty acid composition.

4. The method of claim 1 , wherein the buffer compound is a carbonate.

5. The method of claim 1 , wherein the fatty acid composition is present in an amount equal to or less than 1.25 weight % based on the total weight of the aqueous flexographic developer.

6. The method of claim 1 , wherein the aqueous flexographic developer comprises ethylenediamine tetracarboxylic acid or an alkali metal salt thereof in an amount of at least 0.05 weight % and up to and including 0.30 weight %, based on the total weight of the aqueous flexographic developer.

7. The method of claim 1 , wherein the aqueous flexographic developer further comprises at least 0.05 weight % and up to and including 0.30 weight % of a glycol and poly-glycol mono-ether co-solvent having a molecular weight of less than 150, the amount being based on the total weight of the aqueous flexographic developer.

8. The method of claim 7 , wherein:

a) the fatty acid composition consists essentially of oleic acid or an alkali metal salt thereof in an amount of at least 90 weight % and up to and including 100 weight % of the fatty acid composition, and the fatty acid composition is present in an amount of at least 0.50 weight % and up to and including 1.25 weight %;

b) ethylenediamine tetracarboxylic acid or an alkali metal salt thereof is present as the one or more aminopolycarboxylic acids or alkali metal salts thereof in an amount of at least 0.05 weight % and up to and including 0.25 weight %; and

c) a carbonate is present as the buffer compound in an amount of at least 0.20 weight % and up to and including 0.60 weight %;

all amounts being based on the total weight of the aqueous flexographic developer.

9. A method for providing a flexographic printing member, comprising:

providing a flexographic developer concentrate;

forming an aqueous flexographic developer either by dissolving the flexographic developer concentrate, if in solid form, in water, or by diluting the flexographic developer concentrate, if in liquid form, by mixing 1 part of the aqueous flexographic developer concentrate with at least 2 parts and up to and including 99.8 parts of water; and

developing an imagewise exposed flexographic printing member precursor with the aqueous flexographic developer, to provide a relief image in a flexographic printing member,

wherein the flexographic developer concentrate comprises:

a) a fatty acid composition consisting of one or more saturated or unsaturated fatty acids or alkali metal salts thereof, each saturated or unsaturated fatty acid or alkali metal salt thereof independently having 12 to 20 carbon atoms, the fatty acid composition being present in an amount of at least 10 weight % and up to and including 60 weight %;

wherein at least 85 weight % of the fatty acid composition is composed of one or more C 18 mono- or poly-unsaturated fatty acids or alkali metal salts thereof;

b) one or more aminopolycarboxylic acids or alkali metal salts thereof in an amount of at least 1.5 weight % and up to and including 15 weight %;

c) a buffer compound in an amount of at least 3.5 weight % and up to and including 25 weight %; and

d) water in an amount of up to and including 85 weight %, based on the total weight of the flexographic developer concentrate,

all amounts being based on the total weight of the flexographic developer concentrate.

10. The method of claim 9 , wherein the fatty acid composition consists essentially of oleic acid or an alkali metal salt thereof in an amount of at least 85 weight % and up to and including 100 weight %, based on the total weight of the fatty acid composition.

11. The method of claim 9 , wherein the buffer compound is a carbonate.

12. The method of claim 9 , wherein the fatty acid composition is present in an amount equal to or less than 25 weight %, based on the total weight of the flexographic developer concentrate.

13. The method of claim 9 , wherein the flexographic developer concentrate comprises ethylenediamine tetracarboxylic acid or an alkali metal salt thereof in an amount of at least 1.5 weight % and up to and including 10 weight %, based on the total weight of the flexographic developer concentrate.

14. The method of claim 9 , wherein the flexographic developer concentrate further comprises at least 1.5 weight % and up to and including 15 weight % of a glycol and poly-glycol mono-ether co-solvent having a molecular weight of less than 150, the amount being based on the total weight of the flexographic developer concentrate.

15. The method of claim 14 , wherein:

a) the fatty acid composition consists essentially of oleic acid or an alkali metal salt thereof in an amount of at least 90 weight % and up to and including 100 weight % of the fatty acid composition, and the fatty acid composition is present in an amount of equal to or less than 25 weight %;

b) ethylenediamine tetracarboxylic acid or an alkali metal salt thereof is present as the one or more aminopolycarboxylic acids or alkali metal salts thereof in an amount of at least 1.5 weight % and up to and including 10 weight %; and

c) a carbonate is present as the buffer compound in an amount of at least 4 weight % and up to and including 8 weight %;

all amounts being based on the total weight of the flexographic developer concentrate.

16. The method of claim 9 , further comprising:

replenishing the flexographic developer concentrate with a replenisher developer concentrate having the same or a greater concentration of one or more of components a) through c).

17. A method for providing a flexographic printing member, comprising:

imagewise exposing a flexographic printing member precursor to provide a latent relief image in an imagewise exposed flexographic printing member precursor,

providing a flexographic developer concentrate,

forming an aqueous flexographic developer either by dissolving the flexographic developer concentrate, if in solid form, in water, or by diluting the flexographic developer concentrate, if in liquid form, by mixing 1 part of the flexographic developer concentrate with at least 2 parts and up to and including 99.8 parts of water; and

developing the imagewise exposed flexographic printing member precursor with the aqueous flexographic developer, to provide a relief image in a flexographic printing member,

wherein the flexographic developer concentrate comprises:

a) a fatty acid composition consisting of one or more saturated or unsaturated fatty acids or alkali metal salts thereof, each saturated or unsaturated fatty acid or alkali metal salt thereof independently having 12 to 20 carbon atoms, the fatty acid composition being present in an amount of at least 10 weight % and up to and including 60 weight %;

wherein at least 85 weight % and up to and including 95 weight % of the fatty acid composition is composed of one or more C 18 mono- or poly-unsaturated fatty acids or alkali metal salts thereof;

b) one or more aminopolycarboxylic acids or alkali metal salts thereof in an amount of at least 1.5 weight % and up to and including 15 weight %; and

c) a buffer compound in an amount of at least 3.5 weight % and up to and including 25 weight %;

all amounts being based on the total weight of the flexographic developer concentrate.

18. The method of claim 17 , wherein the flexographic developer concentrate is provided in liquid form, and further comprises:

d) water in an amount of up to and including 85 weight %, based on the total weight of the flexographic developer concentrate.

Assignments (6)
RELEASE OF SECURITY INTEREST Recorded May 1, 2019
From: JPMORGAN CHASE BANK N.A.
To: EASTMAN KODAK COMPANY
Reel/Frame 049056/0265 →
RELEASE OF SECURITY INTEREST Recorded May 1, 2019
From: BANK OF AMERICA N.A., AS AGENT
To: EASTMAN KODAK COMPANY
Reel/Frame 049056/0377 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 11, 2019
From: EASTMAN KODAK COMPANY
To: MIRACLON CORPORATION
Reel/Frame 048857/0633 →
SECURITY INTEREST Recorded Mar 23, 2017
From: EASTMAN KODAK COMPANY; FAR EAST DEVELOPMENT LTD; FPC INC; KODAK (NEAR EAST), INC.; KODAK AMERICAS, LTD.; KODAK REALTY, INC.; LASER-PACIFIC MEDIA CORPORATION; QUALEX INC.; KODAK PHILIPPINES, LTD.; NPEC INC.
To: JPMORGAN CHASE BANK, N.A.
Reel/Frame 041695/0364 →
SECURITY INTEREST Recorded Mar 23, 2017
From: EASTMAN KODAK COMPANY; FAR EAST DEVELOPMENT LTD.; FPC INC.; KODAK (NEAR EAST), INC.; KODAK AMERICAS, LTD.; KODAK REALTY, INC.; LASER-PACIFIC MEDIA CORPORATION; QUALEX INC.; KODAK PHILIPPINES, LTD.; NPEC INC.
To: BANK OF AMERICA, N.A.
Reel/Frame 041696/0145 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 16, 2016
From: OLLMANN, RICHARD R., JR.; FOHRENKAMM, ELSIE ANDERSON; MELLEMA, FREDRICK CHARLES
To: EASTMAN KODAK COMPANY
Reel/Frame 040337/0456 →
Continuity (1)
Related Publication 20180136562A1 · May 17, 2018