IP Library Granted Patent US 10,394,171
Granted Patent B2
US 10,394,171 · App. 15/383,460 · Granted Aug 27, 2019

Method of manufacturing heat-fixing rubber roller and heat-fixing rubber roller

Inventors: Kazuhisa Ishikawa (Tokyo, JP); Shiro Katsuki (Tokyo, JP); Narutoshi Kusaka (Tokyo, JP); Shinji Yamazaki (Tokyo, JP); Yoshimi Matsuzawa (Tokyo, JP)
Assignee: SWCC SHOWA CABLE SYSTEMS CO., LTD.
G03G15/206B29C35/02B29C67/202G03G15/2057B29K2009/06B29K2105/041B29K2105/045B29K2105/24B29K2209/06B29K2409/06B29K2609/06B29K2705/00B29K2809/06B29L2009/00B29L2031/767C08L83/04
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,394,171
App. No.
15/383,460
Granted
Aug 27, 2019
Kind
B2
Abstract

A method of manufacturing a heat-fixing rubber roller includes: forming a rubber layer of a silicone rubber composition on an outer periphery of a metal core shaft, the composition containing water-soluble sugar powder and methylene glycol; vulcanizing the rubber layer; and eluting the sugar powder and the triethylene glycol from the vulcanized rubber layer to form a foam rubber layer.

Claims (11)

1. A method of manufacturing a heat-fixing rubber roller, the method comprising:

forming a rubber layer of a silicone rubber composition on an outer periphery of a metal core shaft, the composition containing water-soluble sugar powder and triethylene glycol;

vulcanizing the rubber layer; and

eluting the sugar powder and the triethylene glycol from the vulcanized rubber layer to form a foam rubber layer.

2. The method of manufacturing the heat-fixing rubber roller according to claim 1 , wherein the foam rubber layer has an open cell ratio of 90% or more.

3. The method of manufacturing the heat-fixing rubber roller according to claim 1 , wherein the sugar powder has a particle size of 1 to 1000 μm.

4. The method of manufacturing the heat-fixing rubber roller according to claim 3 , wherein the sugar powder has a particle size of 10 to 400 μm.

5. The method of manufacturing the heat-fixing rubber roller according to claim 1 , wherein the silicone rubber composition contains 100 parts by mass of the silicone rubber, 50 to 200 parts by mass of the sugar powder, and 1 to 50 parts by mass of the triethylene glycol.

6. The method of manufacturing the heat-fixing rubber roller according to claim 1 , wherein the sugar powder is at least one selected from a group consisting of glucose, lactose, sucrose, trehalose, fructose, sugar, granulated sugar, and powdered sugar.

7. The method of manufacturing the heat-fixing rubber roller according to claim 1 , wherein the silicone rubber is addition-reaction liquid silicone rubber.

8. A heat-fixing rubber roller manufactured by the method of manufacturing the heat-fixing rubber roller according to claim 1 .

Assignments (4)
MERGER Recorded Feb 29, 2024
From: SWCC SHOWA CABLE SYSTEMS CO., LTD
To: SWCC CORPORATION
Reel/Frame 066740/0471 →
CORRECTIVE ASSIGNMENT TO CORRECT THE ASSIGNEE NAME PREVIOUSLY RECORDED ON REEL 041262 FRAME 0672. ASSIGNOR(S) HEREBY CONFIRMS THE ASSIGNMENT. Recorded May 1, 2018
From: ISHIKAWA, KASUHISA; KATSUKI, SHIRO; KUSAKA, NARUTOSHI; YAMAZAKI, SHINJI; MATSUZAWA, YOSHIMI
To: SWCC SHOWA DEVICE TECHNOLOGY CO., LTD
Reel/Frame 046050/0699 →
MERGER Recorded Oct 18, 2017
From: SWCC SHOWA DEVICE TECHNOLOGY CO., LTD.
To: SWCC SHOWA CABLE SYSTEMS CO., LTD.
Reel/Frame 044225/0299 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 15, 2017
From: ISHIKAWA, KAZUHISA; KATSUKI, SHIRO; KUSAKA, NARUTOSHI; YAMAZAKI, SHINJI; MATSUZAWA, YOSHIMI
To: SWCC SHOW DEVICE TECHNOLOGY CO., LTD.
Reel/Frame 041262/0672 →
Priority Claims (1)
JP 2014-127689 · Jun 20, 2014 · national
Continuity (2)
Continuation PCTJP2015003034 · Jun 17, 2015
Related Publication 20170097594A1 · Apr 6, 2017